Measurement of in-plane thermal conductivity of carbon paper diffusion media in the temperature range of-20 °C to+120 °C

被引:72
作者
Zamel, Nada [1 ]
Litovsky, Efim [2 ]
Shakhshir, Saher [1 ]
Li, Xianguo [1 ]
Kleiman, Jacob [2 ]
机构
[1] Univ Waterloo, Dept Mech & Mechatron Engn, Lab Fuel Cells & Green Energy RD&D 20 20, Waterloo, ON N2L 3G1, Canada
[2] Integr Testing Lab Inc, Markham, ON, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Thermal diffusivity; Thermal conductivity; Method of monotonous heating; PEM fuel cells; Cold start; COLD START; STANDARD POROSIMETRY; CONTACT RESISTANCE; FUEL; BEHAVIOR; LAYERS;
D O I
10.1016/j.apenergy.2011.02.037
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Carbon paper is commonly used as the gas diffusion layer (GDL) in polymer electrolyte membrane (PEM) fuel cells as it exhibits high chemical and mechanical durability. This diffusion medium is also anisotropic, which directly affects its transport properties and specifically the thermal conductivity. In this study, the in-plane thermal conductivity of the carbon paper GDL was determined using thermal diffusivity measurements for a temperature range from -20 to +120 degrees C and four Teflon loadings (0, 5, 20 and 50 wt.%). It is important to understand the effect of temperature on the thermal conductivity since PEM fuel cells are designed to operate under various temperatures depending on the application of use. Further, Teflon is used to change the hydrophobic properties of the carbon paper GDL with 20 wt.% as the most widely used percentage. In this study, the Teflon loadings were chosen to gain a comprehensive understanding of the thermal resistance due to Teflon. In this study, a quasi-steady method was used to measure the thermal properties of the carbon paper; hence, the phase transformation in the presence of PTFE was investigated. The thermal conductivity decreases with an increase in temperature for all samples. The addition of as little as 5 wt.% Teflon resulted in high thermal resistance decreasing the overall thermal conductivity of the sample. Further addition of Teflon did not have major effects on the thermal conductivity. For all treated samples, the thermal conductivity lies in the range of 10.1-14.7 W/mK. Finally, empirical relations for the thermal diffusivity and conductivity with temperature were deduced. (C) 2011 Elsevier Ltd. All rights reserved.
引用
收藏
页码:3042 / 3050
页数:9
相关论文
共 40 条
[1]  
[Anonymous], 1989, COMPENDUM THERMOPHYS
[2]  
[Anonymous], 1997, INTRO ERROR ANAL
[3]  
*ASTM, 2009, E2584 ASTM NIST
[4]  
Blumm J, 2010, CHARACTERIZATION PTF
[5]   Ex situ measurements of through-plane thermal conductivities in a polymer electrolyte fuel cell [J].
Burheim, O. ;
Vie, P. J. S. ;
Pharoah, J. G. ;
Kjelstrup, S. .
JOURNAL OF POWER SOURCES, 2010, 195 (01) :249-256
[6]   Wettability and capillary behavior of fibrous gas diffusion media for polymer electrolyte membrane fuel cells [J].
Gostick, Jeff T. ;
Ioannidis, Marios A. ;
Fowler, Michael W. ;
Pritzker, Mark D. .
JOURNAL OF POWER SOURCES, 2009, 194 (01) :433-444
[7]   Capillary pressure and hydrophilic porosity in gas diffusion layers for polymer electrolyte fuel cells [J].
Gostick, Jeffrey T. ;
Fowler, Michael W. ;
Ioannidis, Marios A. ;
Pritzker, Mark D. ;
Volfkovich, Y. M. ;
Sakars, A. .
JOURNAL OF POWER SOURCES, 2006, 156 (02) :375-387
[8]   Non-isothermal cold start of polymer electrolyte fuel cells [J].
Jiang, Fangming ;
Fang, Weifeng ;
Wang, Chao-Yang .
ELECTROCHIMICA ACTA, 2007, 53 (02) :610-621
[9]   Cold start analysis of polymer electrolyte membrane fuel cells [J].
Jiao, Kui ;
Li, Xianguo .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2010, 35 (10) :5077-5094
[10]   Three-dimensional multiphase modeling of cold start processes in polymer electrolyte membrane fuel cells [J].
Jiao, Kui ;
Li, Xianguo .
ELECTROCHIMICA ACTA, 2009, 54 (27) :6876-6891