In vitro degradation study of novel HEC/PVA/collagen nanofibrous scaffold for skin tissue engineering applications

被引:67
作者
Zulkifli, Farah Hanani [1 ]
Hussain, Fathima Shahitha Jahir [1 ]
Rasad, Mohammad Syaiful Bahari Abdull [2 ]
Yusoff, Mashitah Mohd [1 ]
机构
[1] Univ Malaysia Pahang, Fac Ind Sci & Technol, Kuantan 26300, Pahang, Malaysia
[2] Int Islamic Univ Malaysia, Kulliyyah Allied Hlth Sci, Kuantan 25200, Pahang, Malaysia
关键词
In vitro degradation; Hydroxyethyl cellulose; Collagen; Nanofibers scaffold; Tissue engineering; HYDROXYETHYL CELLULOSE; COLLAGEN; GLUTARALDEHYDE; SPECTROSCOPY; BEHAVIOR; IR;
D O I
10.1016/j.polymdegradstab.2014.10.017
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The aim of this study was focused on the degradation behavior of electrospun (hydroxyethyl cellulose/poly(vinyl) alcohol) HEC/PVA and HEC/PVA/collagen nanofibrous scaffolds, as a potential substrates for skin tissue engineering in two biologically related media: phosphate buffered solution (PBS) and Dulbecco's modified Eagle's medium (DMEM) for 12 weeks incubation period. The scaffolds were characterized at different degradation times by a series of analysis including pH changes of solutions, weight loss, swelling ratio, SEM, ATR-FTIR, DSC, TGA and mechanical properties. The results indicated that HEC/PVA/collagen scaffolds were exhibited slower degradation rate in both medium as compared to HEC/PVA blend nanofibers. All fibers displayed uneven and rough surfaces towards the final week of incubation in both PBS and DMEM solution. As degradation time increased, there were little changes in the chemical structure as determined by FTIR spectra while thermal studies revealed that the melting temperatures and crystallinity of scaffolds were slightly shifted to a lower value. Both HEC/PVA and HEC/PVA/collagen fibers showed significant decrease in Young's modulus and tensile stress over 12 weeks degradation. These results show that these nanofibrous scaffold demonstrate degradation behavior that meets the requirement as potential degradable biomaterials for dermal replacement. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:473 / 481
页数:9
相关论文
共 29 条
[1]   Preparation and Characterization of Hydrogel Based on Poly(vinyl alcohol) Cross-Linked by Different Cross-Linkers Used to Dry Organic Solvents [J].
AL-Sabagh, A. M. ;
Abdeen, Z. .
JOURNAL OF POLYMERS AND THE ENVIRONMENT, 2010, 18 (04) :576-583
[2]   Interpenetrating polymer network blend microspheres of chitosan and hydroxyethyl cellulose for controlled release of isoniazid [J].
Angadi, Sudha C. ;
Manjeshwar, Lata S. ;
Aminabhavi, Tejraj M. .
INTERNATIONAL JOURNAL OF BIOLOGICAL MACROMOLECULES, 2010, 47 (02) :171-179
[3]   Biodegradable polymer matrix nanocomposites for tissue engineering: A review [J].
Armentano, I. ;
Dottori, M. ;
Fortunati, E. ;
Mattioli, S. ;
Kenny, J. M. .
POLYMER DEGRADATION AND STABILITY, 2010, 95 (11) :2126-2146
[4]   Polyvinyl alcohol-collagen-hydroxyapatite biocomposite nanofibrous scaffold: Mimicking the key features of natural bone at the nanoscale level [J].
Asran, Ashraf Sh. ;
Henning, S. ;
Michler, Goerg H. .
POLYMER, 2010, 51 (04) :868-876
[5]  
Beyler C., THERMAL DECOMPOSITIO, P110
[6]  
Burgos N, 2013, CHARACTERIZATION AGE, P98
[7]   FT-IR study for hydroxyapatite/collagen nanocomposite cross-linked by glutaraldehyde [J].
Chang, MC ;
Tanaka, J .
BIOMATERIALS, 2002, 23 (24) :4811-4818
[8]  
Dong YX, 2010, DISTINCTIVE DEGRADAT, P283
[9]   Degradation of synthetic polymeric scaffolds for bone and cartilage tissue repairs [J].
Eglin, David ;
Mortisen, Derek ;
Alini, Mauro .
SOFT MATTER, 2009, 5 (05) :938-947
[10]   Free radical degradation of hydroxyethyl cellulose [J].
Erkselius, S ;
Karlsson, OJ .
CARBOHYDRATE POLYMERS, 2005, 62 (04) :344-356