Effect of static pre-loading on fracture toughness of Nicalon® fibre glass matrix composite

被引:3
|
作者
Dlouhy, I
Chlup, Z
Chawla, KK
Kulkarni, R
Koopman, M
Boccaccini, AR
机构
[1] ASCR, Inst Physt Mat, Brno 61662, Czech Republic
[2] Univ Alabama Birmingham, Dept Mat Sci & Engn, Birmingham, AL 35294 USA
[3] Univ London Imperial Coll Sci Technol & Med, Dept Mat, London SW7 2BP, England
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2004年 / 367卷 / 1-2期
关键词
Nicalon (R) fibre; glass matrix composite; fracture toughness; chevron-notch; static fatigue;
D O I
10.1016/j.msea.2003.09.058
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Static fatigue of commercially available unidirectional SiC-fibre reinforced glass matrix composite has been followed by measuring the fracture toughness of samples statically pre-loaded at different stresses and times. Pre-load levels were just below the loads corresponding to fracture strength, the (bending) pre-stress being on level 300, 310 and 315 MPa. Three hold times, 25, 50 and 75 h, were applied at each of the stresses. For fracture toughness (K-1c) determination, a chevron-notch (CN) three-point bend test was applied. The method has been found to be useful to accurately detect and quantify very subtle microdamage on fibre/matrix interfaces caused by static pre-stressing. Despite of the high scatter of the measured K-1c values, a decrease in fracture toughness with increasing pre-stress and hold time has been found. A parameter is proposed that may be used to quantify the cumulative and combined effect of pre-stress and hold time on fracture toughness of composites. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:17 / 23
页数:7
相关论文
共 50 条
  • [1] Effect of fibre content on the interlaminar fracture toughness of unidirectional glass-fibre/polyamide composite
    Chen, JH
    Schulz, E
    Bohse, J
    Hinrichsen, G
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1999, 30 (06) : 747 - 755
  • [2] The effect of matrix toughness and loading rate on the mode-II interlaminar fracture toughness of glass-fibre/vinyl-ester composites
    Compston, P
    Jar, PYB
    Burchill, PJ
    Takahashi, K
    COMPOSITES SCIENCE AND TECHNOLOGY, 2001, 61 (02) : 321 - 333
  • [3] Effect of pre-strain on fracture toughness of ductile structural steels under static and dynamic loading
    Qiu, H
    Enoki, M
    Hiraoka, K
    Kishi, T
    ENGINEERING FRACTURE MECHANICS, 2005, 72 (10) : 1624 - 1633
  • [4] Effect of loading velocity on fracture toughness of a SiCw/A6061 composite
    Wang, L
    Kobayashi, T
    MATERIALS TRANSACTIONS JIM, 1997, 38 (07): : 615 - 621
  • [5] The influence of fibre sizing on the strength and fracture toughness of glass fibre composites
    Feih, S
    Wei, J
    Kingshott, P
    Sorensen, BF
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2005, 36 (02) : 245 - 255
  • [6] EFFECT OF RIBBON ORIENTATION ON THE FRACTURE-TOUGHNESS OF A METALLIC-GLASS-RIBBON-REINFORCED GLASS-CERAMIC MATRIX COMPOSITE
    VAIDYA, RU
    SUBRAMANIAN, KN
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (10) : 2962 - 2964
  • [7] THE EFFECT OF MICROSTRUCTURE ON THE FRACTURE-TOUGHNESS OF A METAL-MATRIX COMPOSITE
    DOWNES, TJ
    KING, JE
    COMPOSITES, 1993, 24 (03): : 276 - 281
  • [8] The effect of matrix fracture toughness on the plastic deformation of the metallic glassy composite
    Chu, Zhenhua
    Yuan, Guangyin
    Kato, Hidemi
    Xie, Guoqiang
    Yan, Dianran
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 612 : 10 - 15
  • [9] Effect of displacement loading rates on mode-I fracture toughness of fiber glass-epoxy composite laminates
    Satyanarayana, Aala
    Gatti, Mahendra
    ENGINEERING FRACTURE MECHANICS, 2019, 218
  • [10] The fracture toughness of natural fibre- and glass fibre-reinforced SMC
    Patel, Harish K.
    Balasubramanian, Vimalan
    Peijs, Ton
    PLASTICS RUBBER AND COMPOSITES, 2017, 46 (08) : 355 - 364