Effect of grain size on the microstructure and mechanical properties of friction stir welded non-combustive magnesium alloys

被引:45
作者
Chen, Juan [1 ]
Fujii, Hidetoshi [1 ]
Sun, Yufeng [1 ]
Morisada, Yoshiaki [1 ]
Kondoh, Katsuyoshi [1 ]
Hashimoto, Kenji [2 ]
机构
[1] Osaka Univ, Joining & Welding Res Inst, Osaka 5670047, Japan
[2] Tokyu Car Cooperat, Kanazawa Ward, Yokohama, Kanagawa 2360043, Japan
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2012年 / 549卷
基金
日本科学技术振兴机构;
关键词
Friction stir welding; Magnesium alloys; Texture; Tension test; TEXTURE; FLOW; BEHAVIOR;
D O I
10.1016/j.msea.2012.04.030
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The novel fine-grained and coarse-grained non-combustive AMX602 (Mg-6% Al-0.5% Mn-2% Ca) magnesium plates with average grain sizes of 1.06 and 6.14 mu m respectively were subjected to the friction stir welding. The effect of the initial grain size on the microstructure and mechanical properties of the joints were studied. The results showed that the grains growth occurred in the stir zone of the fine-grained specimens after welding. However, grain refinement occurred in the coarse-grained counterpart. The texture evolution of the fine and coarse grained materials joints had similar trends but with different texture intensities. It is suggested that the initial grain size affects the texture intensity through the slip inhomogeneity caused by different amount of grain boundaries. The microhardness of the fine-grained material joints was lower than that of the base material, whereas it became higher in the coarse-grained specimens. The results of the tensile test indicated that the grain size and grain orientation of the joints had an effect on the mechanical properties and fracture locations of the joints. Although both the fine-grained and coarse-grained material joints had similar yield strengths, the fine-grained specimen had a higher ultimate tensile strength of 261.6 MPa and the coarse-grained specimen had a relatively lower one of 203.6 MPa. (c) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:176 / 184
页数:9
相关论文
共 28 条
[1]  
Arbegast WJ, 2003, HOT DEFORMATION OF ALUMINUM ALLOYS III, P313
[2]  
Bendzsak G.J., 2000, P 1 INT FRICT STIR W
[3]   Friction stir welding of AZ31 magnesium alloy rolled sheets: Influence of processing parameters [J].
Commin, L. ;
Dumont, M. ;
Masse, J. -E. ;
Barrallier, L. .
ACTA MATERIALIA, 2009, 57 (02) :326-334
[4]   Microstructure and mechanical properties of hot extruded Mg-Al-Mn-Ca alloy produced by rapid solidification powder metallurgy [J].
Elsayed, Ayman ;
Kondoh, Katsuyoshi ;
Imai, Hisashi ;
Umeda, Junko .
MATERIALS & DESIGN, 2010, 31 (05) :2444-2453
[5]   Principles of grain refinement and superplastic flow in magnesium alloys processed by ECAP [J].
Figueiredo, Roberto B. ;
Langdon, Terence G. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 501 (1-2) :105-114
[6]   Friction stir welding of ultrafine grained interstitial free steels [J].
Fuji, H ;
Ueji, R ;
Takada, Y ;
Kitahara, H ;
Tsuji, N ;
Nakata, K ;
Nogi, K .
MATERIALS TRANSACTIONS, 2006, 47 (01) :239-242
[7]   Correlation of plastic deformation and dynamic recrystallization in magnesium alloy Zk60 [J].
Galiyev, A ;
Kaibyshev, R ;
Gottstein, G .
ACTA MATERIALIA, 2001, 49 (07) :1199-1207
[8]  
Humphreys FJ, 2017, Recrystallization and Related Annealing Phenomena, Vthird
[9]   Texture development and its effect on mechanical properties of an AZ61 Mg alloy fabricated by equal channel angular pressing [J].
Kim, WJ ;
Hong, SI ;
Kim, YS ;
Min, SH ;
Jeong, HT ;
Lee, JD .
ACTA MATERIALIA, 2003, 51 (11) :3293-3307
[10]   Microstructures and mechanical responses of powder metallurgy non-combustive magnesium extruded alloy by rapid solidification process in mass production [J].
Kondoh, Katsuyoshi ;
Hamada, El-Sayed Ayman ;
Imai, Hisashi ;
Umeda, Junko ;
Jones, Tyrone .
MATERIALS & DESIGN, 2010, 31 (03) :1540-1546