Steam oxidation resistance of Ni-aluminide/Fe-aluminide duplex coatings formed on creep resistant ferritic steels by low temperature pack cementation process

被引:22
作者
Xiang, Z. D. [1 ]
Zeng, D. [1 ]
Zhu, C. Y. [1 ]
Rose, S. R. [2 ]
Datta, P. K. [2 ]
机构
[1] Wuhan Univ Sci & Technol, Sch Met & Mat, Wuhan 430081, Peoples R China
[2] Northumbria Univ, Sch Comp Engn & Informat Sci, Newcastle Upon Tyne NE1 8ST, Tyne & Wear, England
基金
中国国家自然科学基金;
关键词
Metal coatings; Intermetallics; Steel; Oxidation; High temperature corrosion; ALLOY-STEELS; HYBRID COATINGS; WATER-VAPOR; MICROSTRUCTURE; ALUMINISATION; RATES; AL;
D O I
10.1016/j.corsci.2010.09.064
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Steam oxidation resistance and thermal stability were studied at 650 C for a coating with an outer Ni2Al3 layer and an inner Fe2Al5 layer formed on P92 steel surface The parabolic rate law of oxidation was obeyed only in less than 2000 h with positive deviations occurring at longer oxidation times The outer layer of the coating was transformed to NiAl during oxidation but It remained stable once it was formed The mechanisms for the enhanced thermal stability were discussed and a simple approach to enhancing the lifetime of the coating was proposed (c) 2010 Elsevier Ltd All rights reserved
引用
收藏
页码:496 / 502
页数:7
相关论文
共 27 条
  • [1] Evolution of microstructure and deformation resistance in creep of tempered martensitic 9-12%Cr-2%W-5%Co steels
    Agamennone, R.
    Blum, W.
    Gupta, C.
    Chakravartty, J. K.
    [J]. ACTA MATERIALIA, 2006, 54 (11) : 3003 - 3014
  • [2] Long exposure steam oxidation testing and mechanical properties of slurry aluminide coatings for steam turbine components
    Agüero, A
    Muelas, R
    Pastor, A
    Osgerby, S
    [J]. SURFACE & COATINGS TECHNOLOGY, 2005, 200 (5-6) : 1219 - 1224
  • [3] Aguero A., 2008, Energy Materials, V3, P35, DOI 10.1179/174892407X248554
  • [4] Formation and oxidation performance of low-temperature pack aluminide coatings on ferritic-martensitic steels
    Bates, B. L.
    Wang, Y. Q.
    Zhang, Y.
    Pint, B. A.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2009, 204 (6-7) : 766 - 770
  • [5] Corrosion behavior of ferritic-martensitic steel T91 in supercritical water
    Chen, Yun
    Sridharan, Kumar
    Allen, Todd
    [J]. CORROSION SCIENCE, 2006, 48 (09) : 2843 - 2854
  • [6] ELDRIDGE J, 1964, T METALL SOC AIME, V230, P226
  • [7] Assessment of the Fe-Ni-Al system
    Eleno, Luiz
    Frisk, Karin
    Schneider, Andre
    [J]. INTERMETALLICS, 2006, 14 (10-11) : 1276 - 1290
  • [8] THERMODYNAMICS OF IRON-ALUMINUM ALLOYS AT 1573-K
    JACOBSON, NS
    MEHROTRA, GM
    [J]. METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1993, 24 (03): : 481 - 486
  • [9] History of power plants and progress in heat resistant steels
    Masuyama, F
    [J]. ISIJ INTERNATIONAL, 2001, 41 (06) : 612 - 625
  • [10] The theory of the formation of protective oxide films on metals, II.
    Mott, NF
    [J]. TRANSACTIONS OF THE FARADAY SOCIETY, 1940, 35 (03): : 0472 - 0482