Preparation of High-Strength Ti3AlC2 by Spark Plasma Sintering

被引:14
|
作者
Wang, Wenjuan [1 ,2 ]
Li, Cuiwei [1 ,2 ]
Zhai, Hongxiang [1 ,2 ]
Wang, Changan [2 ]
机构
[1] Beijing Jiaotong Univ, Inst Mat Sci & Engn, Sch Mech & Elect Control, Engn, Beijing 100044, Peoples R China
[2] Beijing Jiaotong Univ, Inst Mat Sci & Engn, Sch Mech & Elect Control Engn, Beijing 100044, Peoples R China
关键词
MECHANICAL-PROPERTIES; TI3SIC2; PHASES; DEPENDENCE; HARDNESS;
D O I
10.1111/ijac.12254
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Ti3AlC2 bulk materials with high mechanical properties have been fabricated by spark plasma sintering using Ti3AlC2 powders as starting material. Effects of sintering temperature on the microstructure and mechanical properties of Ti3AlC2 were investigated. Nearly full-dense Ti3AlC2 samples could be obtained after sintering the powders in the 1300-1400 degrees C temperature range for 3min under a pressure of 20MPa. The as-prepared Ti3AlC2 samples have finer grains, which results in higher mechanical properties. The Ti3AlC2 samples prepared at 1350 degrees C show a higher hardness of 3.84 +/- 0.06 GPa and flexural strength of 746.8 +/- 6 MPa.
引用
收藏
页码:E126 / E131
页数:6
相关论文
共 50 条
  • [31] Pressureless sintering and properties of Cu/Ti3AlC2 composites
    Huang Zhenying
    Zhai Hongxiang
    Ai Mingxing
    Wang Yi
    Zhang Hongbing
    HIGH-PERFORMANCE CERAMICS V, PTS 1 AND 2, 2008, 368-372 : 998 - 1000
  • [32] Preparation of Ti3AlC2 and Ti2AlC by self-propagating high-temperature synthesis
    Zhou, AG
    Wang, CA
    Ge, ZB
    Wu, LF
    JOURNAL OF MATERIALS SCIENCE LETTERS, 2001, 20 (21) : 1971 - 1973
  • [33] Synthesis of high-purity powder Ti3AlC2 materials by pressureless sintering
    Peng, CQ
    Wang, CA
    Huang, Y
    RARE METAL MATERIALS AND ENGINEERING, 2005, 34 : 540 - 543
  • [34] Synthesis of high-purity powder Ti3AlC2 materials by pressureless sintering
    Peng, Chunqing
    Wang, Changan
    Huang, Yong
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2005, 34 (SUPPL. 1 PART 1): : 542 - 543
  • [35] Preparation of Ti3AlC2 matrix composites by selective laser melting combined with pressureless sintering
    Shao, Huang
    Liu, Tingting
    Zhang, Kai
    Zhang, Changdong
    Jiang, Shuxin
    Xiong, Zhiwei
    Liao, Wenhe
    ADVANCES IN APPLIED CERAMICS, 2020, 119 (03) : 158 - 165
  • [36] Preparation, Microstructure, and Mechanical Properties of TiB2 Using Ti3AlC2 as a Sintering Aid
    Zheng, Liya
    Li, Fangzhi
    Zhou, Yanchun
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2012, 95 (06) : 2028 - 2034
  • [37] Preparation of Bulk Ti2AlC Using Ti3AlC2 Powders as a Starting Material
    Chen, Xinhua
    Zhai, Hongxiang
    Li, Shibo
    Zhou, Yang
    Huang, Zhenying
    CHINESE CERAMICS COMMUNICATIONS, 2010, 105-106 : 83 - 86
  • [38] Preparation of high-strength (Ta,W)C solid-solutions by spark plasma sintering
    Demirskyi, Dmytro
    Yoshimi, Kyosuke
    Suzuki, Tohru S.
    Vasylkiv, Oleg O.
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2023, 20 (05) : 2747 - 2759
  • [39] Machinable Ti2AlC ceramics produced by spark plasma sintering
    Guo Junming
    Wang Baosen
    Chen Kexin
    Zhou Heping
    RARE METAL MATERIALS AND ENGINEERING, 2007, 36 (05) : 865 - 868
  • [40] Synthesis of layered ternary carbide Ti3ALC2 by atmospheric sintering
    Xue, Maoquan
    Li, Changsheng
    Tang, Hua
    Zhenkong Kexue yu Jishu Xuebao/Journal of Vacuum Science and Technology, 2014, 34 (03): : 300 - 304