Hardness and Swelling Behaviour of Epoxidized Natural Rubber/Recycled Acrylonitrile-Butadiene Rubber (ENR 50/NBRr) Blends

被引:3
作者
Ahmad, Hazwani Syaza [1 ]
Ismail, Hanafi [1 ]
Rashid, Azura A. [1 ]
机构
[1] Univ Sains Malaysia, Sch Mat & Mineral Resources Engn, Engn Campus, Nibong Tebal 14300, Penang, Malaysia
来源
PROCEEDING OF THE 3RD INTERNATIONAL CONFERENCE OF GLOBAL NETWORK FOR INNOVATIVE TECHNOLOGY 2016 (3RD IGNITE-2016): ADVANCED MATERIALS FOR INNOVATIVE TECHNOLOGIES | 2017年 / 1865卷
关键词
ENR; 50; NBRr; Hardness; Swelling; CURING CHARACTERISTICS; MECHANICAL-PROPERTIES; RESISTANCE; POWDER;
D O I
10.1063/1.4993344
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This recent work is to investigate the hardness and swelling behaviour of epoxidized natural rubber/recycled acrylonitrile-butadiene rubber (ENR 50/NBRr) blends. ENR 50/NBRr blends were prepared by two-roll mills with five different loading of NBRr from 5 to 35 phr. Results indicated that the hardness of ENR 50/NBRr blends increased as recycled NBR increased due to the improvement in crosslink density of the blends. Increasing NBRr content gives ENR 50/NBRr blends better resistance towards swelling. Higher degree of crosslinking will increase the swelling resistance and reduce the penetration of toluene into the blends. The presence of polar group in ENR 50 and NBRr give better hardness properties and swelling behaviour of the ENR 50/NBRr blends compared to the NR/NBRr blends.
引用
收藏
页数:5
相关论文
共 14 条
[1]   Comparison properties of natural rubber/virgin acrylonitrile-butadiene rubber and natural rubber/recycled acrylonitrile-butadiene rubber blends [J].
Ahmad, H. S. ;
Ismail, H. ;
Azura, A. R. .
IRANIAN POLYMER JOURNAL, 2015, 24 (03) :185-195
[2]   Statistical mechanics of cross-linked polymer networks II Swelling [J].
Flory, PJ ;
Rehner, J .
JOURNAL OF CHEMICAL PHYSICS, 1943, 11 (11) :521-526
[3]   The effect of a compatibilizer on curing characteristics, mechanical properties and oil resistance of styrene butadiene rubber/epoxidized natural rubber blends [J].
Ismail, H ;
Hairunezam, HM .
EUROPEAN POLYMER JOURNAL, 2001, 37 (01) :39-44
[4]   Styrene butadiene rubber/epoxidized natural rubber blends: dynamic properties, curing characteristics and swelling studies [J].
Ismail, H ;
Suzaimah, S .
POLYMER TESTING, 2000, 19 (08) :879-888
[5]  
Ismail H, 2003, IRAN POLYM J, V12, P373
[6]   Effect of filler loading on cure time and swelling behaviour of SMR L/ENR 25 and SMR L/SBR blends [J].
Ismail, H ;
Poh, BT ;
Tan, KS ;
Moorthy, M .
POLYMER INTERNATIONAL, 2003, 52 (05) :685-691
[7]   The comparison properties of recycle rubber powder, carbon black, and calcium carbonate filled natural rubber compounds [J].
Ismail, H ;
Nordin, R ;
Noor, AM .
POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, 2002, 41 (05) :847-862
[8]   Curing characteristics and mechanical properties of natural rubber/chloroprene rubber and epoxidized natural rubber/chloroprene rubber blends [J].
Ismail, H ;
Leong, HC .
POLYMER TESTING, 2001, 20 (05) :509-516
[9]  
Ismail H., 2005, International Journal of Polymeric Materials and Polymeric Biomaterials, V54, P9, DOI [10.1080/00914030390224256, DOI 10.1080/00914030390224256]
[10]   Characterization of styrene butadiene rubber/recycled acrylonitrile-butadiene rubber (SBR/NBRr) blends: The effects of epoxidized natural rubber (ENR-50) as a compatibilizer [J].
Noriman, N. Z. ;
Ismail, H. ;
Rashid, A. A. .
POLYMER TESTING, 2010, 29 (02) :200-208