Influence of gaseous hydrogen on the notched tensile strength of D6ac steel

被引:27
作者
Chang, TL
Tsay, LW
Chen, C
机构
[1] Natl Taiwan Univ, Coll Engn, Inst Mat Sci & Engn, Taipei 106, Taiwan
[2] Natl Taiwan Ocean Univ, Inst Mat Engn, Chilung 202, Taiwan
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2001年 / 316卷 / 1-2期
关键词
notched tensile strength; D6ac steel; gaseous hydrogen embrittlement;
D O I
10.1016/S0921-5093(01)01217-5
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Slow displacement-rate tensile tests were performed on D6ac. tempered specimens to investigate the influence of gaseous hydrogen pressure on the notched tensile strength (NTS) and the associated fracture characteristics. The susceptibility to hydrogen embrittlement of specimens at a given pressure was determined by the NTS loss, which tended to decrease as the tempering temperature increased. The NTS loss for T-300 (300 degreesC tempered) and T-450 (450 degreesC tempered) specimens increased with rising hydrogen pressure up to 5 x 10(5) Pa. and then remained nearly the same up to the pressure of 2 x 10(6) Pa, while no deteriorated NTS in hydrogen has been found for T-600 (600 degreesC tempered) specimens. The extent of intergranular fracture and/or the region of flat fracture on tensile fractured surfaces were consistent with the correlation of hydrogen pressure and NTS loss. The smaller the intergranular and/or flat fracture regions, the greater the resistance to hydrogen embrittlement of the specimen would be expected. Besides the effect of notch tip blunting, the excellent performance of T-600 specimens in hydrogen could be attributed partly to the presence of less continuous carbides at prior austenite grain boundaries. In contrast, T-300 specimens with grain boundary carbides in a more continuous manner were highly susceptible to hydrogen embrittlement. (C) 2001 Elsevier Science BY, All rights reserved.
引用
收藏
页码:153 / 160
页数:8
相关论文
共 28 条
[1]   EFFECTS OF MN, P, AND MO ON SULFIDE STRESS CRACKING RESISTANCE OF HIGH-STRENGTH LOW-ALLOY STEELS [J].
ASAHI, H ;
SOGO, Y ;
UENO, M ;
HIGASHIYAMA, H .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (09) :2171-2177
[2]   EFFECTS OF STRENGTHENING MECHANISMS ON SULFIDE STRESS CRACKING RESISTANCE OF LOW STRENGTH STEELS [J].
ASAHI, H ;
YAGI, A ;
UENO, M .
ISIJ INTERNATIONAL, 1993, 33 (11) :1190-1195
[3]  
*ASM, 1981, MET HDB, V4, P122
[4]  
BEACHEM CD, 1972, METALL TRANS, V3, P437
[5]  
Bernstein I.M., 1980, ADV CORROSION SCI TE, P53, DOI DOI 10.1007/978-1-4615-9065-1_2
[6]  
BIRNBAUM HK, 1977, ENV SENSITIVE FRACTU, P326
[7]  
CAIN WM, 1965, PETR ENG MAY, P78
[8]  
EWALDS HL, 1984, FRACTURE MECH, P113
[9]   The effect of stress concentration on hydrogen embrittlement of a low alloy steel [J].
Hardie, D ;
Liu, S .
CORROSION SCIENCE, 1996, 38 (05) :721-733
[10]  
HARDIE D, 1976, EFFECT HYDROGEN BEHA, P251