Wear characteristics of austenitic steel and martensitic steel at high temperature

被引:8
作者
Bai, Zhixiong [1 ]
Su, Ning [1 ]
Yang, Hang [1 ]
Wu, Xiaochun [1 ]
机构
[1] Shanghai Univ, Sch Mat Sci & Engn, Shanghai 200072, Peoples R China
关键词
austenitic steel; martensitic steel; wear; oxide; high temperature; microstructure; SLIDING WEAR; OXIDATION WEAR; CARBON-STEELS; MILD WEAR; DIE; RESISTANCE; BEHAVIOR; H13; MICROSTRUCTURE; DEFORMATION;
D O I
10.1088/2053-1591/ac86b9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Wear under high temperature is one of the mechanisms of die failure. Therefore, wear resistance at high temperature is an important parameter for selecting die materials. In this work, the wear resistance of SDHA austenitic steel (6Mn14Cr3Mo2Si1V2 steel) and 4Cr5Mo2V martensitic steel at 400 degrees C-700 degrees C was investigated using a friction and wear tester. The wear behaviour and oxide type were investigated using a scanning electron microscope (SEM) and by X-ray diffraction (XRD), respectively. The results show that the oxides on the worn surface at the test temperatures are Fe2O3 and Fe3O4. With increasing test temperature, from 400 degrees C to 700 degrees C, the wear volume of the two steels initially decreases and then increases. Between these two temperatures, the wear volume of SDHA austenitic steel increased from 29.7 mm(3) to 81.2 mm(3), a 173.4% increase. The wear volume of 4Cr5Mo2V martensitic steel increased from 34.7 mm(3) to 134.7 mm(3), a 267.4% increase. Hence, SDHA austenitic steel has better wear resistance than 4Cr5Mo2V martensitic steel. This is attributed to excellent hardness stability at high temperature. The coarse M7C3 carbides in 4Cr5Mo2V martensitic steel cause peeling and delamination of the oxide layer, reducing wear resistance at 700 degrees C.
引用
收藏
页数:13
相关论文
共 45 条
[21]   Development of a hot stamped channel section with axially tailored properties - experiments and models [J].
Omer, Kaab ;
George, Ryan ;
Bardelcik, Alexander ;
Worswick, Michael ;
Malcolm, Skye ;
Detwiler, Duane .
INTERNATIONAL JOURNAL OF MATERIAL FORMING, 2018, 11 (01) :149-164
[22]   Heat Treatment Optimization and Properties Correlation for H11-Type Hot-Work Tool Steel [J].
Podgornik, B. ;
Pus, G. ;
Zuzek, B. ;
Leskovsek, V. ;
Godec, M. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (02) :455-462
[23]   REVIEW OF OXIDATIONAL WEAR .1. THE ORIGINS OF OXIDATIONAL WEAR [J].
QUINN, TFJ .
TRIBOLOGY INTERNATIONAL, 1983, 16 (05) :257-271
[24]   APPLICATION OF THE OXIDATIONAL THEORY OF MILD WEAR TO THE SLIDING WEAR OF LOW-ALLOY STEEL [J].
QUINN, TFJ ;
ROWSON, DM ;
SULLIVAN, JL .
WEAR, 1980, 65 (01) :1-20
[25]  
Roberts WH., 1961, ASLE Trans, V4, P20, DOI [10.1080/05698196108972416, DOI 10.1080/05698196108972416]
[26]   Research on Oxidation Wear Behavior of a New Hot Forging Die Steel [J].
Shi, Yuanji ;
Wu, Xiaochun .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (01) :176-185
[27]   The role of oxidation in the wear of alloys [J].
Stott, FH .
TRIBOLOGY INTERNATIONAL, 1998, 31 (1-3) :61-71
[28]   Sliding wear of austenitic and austenitic-ferritic stainless steels [J].
Straffelini, G ;
Trabucco, D ;
Molinari, A .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2002, 33 (03) :613-624
[29]   MILD WEAR OF A LOW-ALLOY STEEL AT TEMPERATURES UP TO 500-DEGREES-C [J].
SULLIVAN, JL ;
ATHWAL, SS .
TRIBOLOGY INTERNATIONAL, 1983, 16 (03) :123-131
[30]   Multifractal Detrended Fluctuation Analysis on Friction Coefficient During the Friction Process [J].
Sun, Guodong ;
Zhu, Hua ;
Ding, Cong ;
Zhou, Yuankai .
JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 2018, 140 (01)