Critical current density and a.c. losses of Ag-sheathed Bi2223 tapes with Sr-V-O barriers

被引:8
作者
Maeda, H [1 ]
Inaba, T
Sato, M
Zhang, PX
Chen, WP
机构
[1] Kitami Inst Technol, Dept Mat Sci, Kitami, Hokkaido 0908507, Japan
[2] Japan Sci & Technol Corp, CREST, Tsukuba, Ibaraki 3050047, Japan
[3] Toyohashi Univ Technol, Toyohashi, Aichi 4418580, Japan
[4] Tohoku Univ, Mat Res Inst, Sendai, Miyagi 0908577, Japan
来源
PHYSICA C | 2001年 / 357卷
关键词
Bi2223 multifilamentary tapes; SVO barriers; critical current density; ac losses;
D O I
10.1016/S0921-4534(01)00499-3
中图分类号
O59 [应用物理学];
学科分类号
摘要
Ag-sheathed Bi2223 multifilamentary tapes with 19 filaments with Sr-V-O (SVO) barriers have been prepared using powder-in-tube method. The SVO barriers are arranged inside and/or outside each filament. The critical current density J(c) at 77 K strongly depends on the preparation conditions such as the heat-treatment temperature and intermediate rolling. For the barrier tapes the J(c) values are higher than those of the non-barrier tapes for all the barrier configurations. Furthermore, for all the barrier tapes the transport a.c. losses at 77 K in self-field are lower than those of the non-barrier tapes. In particular, the inside-barrier tapes will give us an excellent possibility to reduce the over all J(c) and the ease to fabricate to tape shape. (C) 2001 Published by Elsevier Science B.V.
引用
收藏
页码:1230 / 1233
页数:4
相关论文
共 10 条
  • [1] Ayai N., 1999, Advances in Superconductivity XI. Proceedings of the 11th International Symposium on Superconductivity (ISS'98), P911
  • [2] PREPARATION OF THE HIGH-TC PHASE OF BI-SR-CA-CU-O SUPERCONDUCTOR
    ENDO, U
    KOYAMA, S
    KAWAI, T
    [J]. JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS & EXPRESS LETTERS, 1988, 27 (08): : L1476 - L1479
  • [3] Novel resistive interfilamentary carbonate barriers in multifilamentary low AC loss Bi(2223)-tapes
    Goldacker, W
    Quilitz, M
    Obst, B
    Eckelmann, H
    [J]. IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 1999, 9 (02) : 2155 - 2158
  • [4] Reducing ac losses of Bi(2223) multifilamentary tapes by oxide barriers
    Huang, YB
    Flukiger, R
    [J]. PHYSICA C, 1998, 294 (1-2): : 71 - 82
  • [5] Maeda H, 1998, ADV CRYOG ENG, V44, P561
  • [6] Microstructures and superconducting properties of V doped Bi2223 tapes
    Maeda, H
    Kakimoto, K
    Kikuchi, M
    Willis, JO
    Watanabe, K
    Tanaka, Y
    Kumakura, H
    [J]. APPLIED SUPERCONDUCTIVITY, 1997, 5 (1-6) : 151 - 156
  • [7] Effect of V, Ir-doping on the Jc properties of Bi2223 tapes
    Maeda, H
    Kakimoto, K
    Kikuchi, M
    Watanabe, K
    Tanaka, Y
    Kumakura, H
    [J]. IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 1999, 9 (02) : 2541 - 2544
  • [8] Fabrication and properties of Ag-sheathed Bi2223 tapes with Sr6V2O11 oxide barriers between filaments
    Maeda, H
    Zhang, PX
    Watanabe, K
    Matsushita, T
    Otabe, ES
    [J]. PHYSICA C, 2000, 335 (1-4): : 35 - 38
  • [10] AC LOSSES OF AG-SHEATHED (BI, PB)(2)SR2CA2CU3OX MONOFILAMENTARY AND MULTIFILAMENTARY TAPES
    OOTA, A
    FUKUNAGA, T
    MATSUI, M
    YUHYA, S
    HIRAOKA, M
    [J]. PHYSICA C, 1995, 249 (1-2): : 157 - 165