Effect and mechanism of B2O3 on apparent viscosity of slag during smelting of vanadium-titanium magnetite in the Blast Furnace
被引:11
|
作者:
Lin, Yin-he
论文数: 0引用数: 0
h-index: 0
机构:
Pangang Grp Res Inst Co Ltd, Inst Resources & Environm Sci, Panzhihua 617000, Sichuan, Peoples R ChinaPangang Grp Res Inst Co Ltd, Inst Resources & Environm Sci, Panzhihua 617000, Sichuan, Peoples R China
Lin, Yin-he
[1
]
Wen, Yong-cai
论文数: 0引用数: 0
h-index: 0
机构:
Pangang Grp Res Inst Co Ltd, Inst Resources & Environm Sci, Panzhihua 617000, Sichuan, Peoples R ChinaPangang Grp Res Inst Co Ltd, Inst Resources & Environm Sci, Panzhihua 617000, Sichuan, Peoples R China
Wen, Yong-cai
[1
]
Fu, Wei-guo
论文数: 0引用数: 0
h-index: 0
机构:
Pangang Grp Res Inst Co Ltd, Inst Resources & Environm Sci, Panzhihua 617000, Sichuan, Peoples R ChinaPangang Grp Res Inst Co Ltd, Inst Resources & Environm Sci, Panzhihua 617000, Sichuan, Peoples R China
Fu, Wei-guo
[1
]
Rao, Jia-ting
论文数: 0引用数: 0
h-index: 0
机构:
Pangang Grp Res Inst Co Ltd, Inst Resources & Environm Sci, Panzhihua 617000, Sichuan, Peoples R ChinaPangang Grp Res Inst Co Ltd, Inst Resources & Environm Sci, Panzhihua 617000, Sichuan, Peoples R China
Rao, Jia-ting
[1
]
机构:
[1] Pangang Grp Res Inst Co Ltd, Inst Resources & Environm Sci, Panzhihua 617000, Sichuan, Peoples R China
High Ti-bearing Blast Furnace Slag;
perovskite;
anosovite;
apparent viscosity;
B2O3;
D O I:
10.1051/metal/2016038
中图分类号:
TF [冶金工业];
学科分类号:
0806 ;
摘要:
Considering the low fluidity and the difficulties in separating high Ti-bearing blast furnace slag from hot metal, the effect of B2O3 on apparent viscosity under argon atmosphere was studied from 1340 degrees C to 1475 degrees C using Brookfield Rotational Viscometer, Metallographic Microscope, et al. The results showed that the addition of B2O3 could decrease melting temperature of high Ti-bearing blast furnace slag and increased its fluidity. With increasing the amount of B2O3 from 0 to 3%, mass fraction of perovskite in high Ti-bearing blast furnace slag gradually decreased, but four times the mass fraction of anosovite. The Ti(C, N) appeared enrichment in the high Ti-bearing blast furnace slag, and the enrichment changed with the addition of B2O3 increasing.