Carbon dioxide laser application enhances the effect of silane primer on the shear bond strength between porcelain and composite resin

被引:19
作者
Chen, Jian-Rong [2 ]
Oka, Kenji [1 ]
Kawano, Takanori [1 ]
Goto, Takaharu [1 ]
Ichikawa, Tetsuo [1 ]
机构
[1] Univ Tokushima, Inst Hlth Biosci, Dept Oral & Maxillofacial Prosthodont & Oral Impl, Tokushima 7708504, Japan
[2] Tongji Univ, Sch Stomatol, Dept Prosthodont, Shanghai 200072, Peoples R China
关键词
Carbon dioxide laser; Shear bond strength; Silane coupling agent; METAL-CERAMIC RESTORATIONS; FRACTURE-RESISTANCE; SURFACE TREATMENTS; REPAIR MATERIALS; AGENTS; RAMAN; EXPOSURE; SYSTEMS; DESIGNS; SILICA;
D O I
10.4012/dmj.2009-106
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The purpose of this study was to evaluate the effect of carbon dioxide laser irradiation on the performance of silane coupling agent as an adhesion promoter. The carbon dioxide laser used in this study was Opelaser 03S II, which irradiated the silane coupling agent applied on the adhesive surface of porcelain. Before and after thermal cycling, shear bond strength was measured using a universal testing machine. Without primer treatment, most of the specimens failed adhesively before reaching the end of the thermal cycling period. For the specimens irradiated with carbon dioxide laser after primer treatment, their shear bond strengths before and after thermal cycling were higher than those treated with primer only -with a significantly pronounced difference between these two groups especially after thermal cycling. Therefore, a combined surface treatment which involved silane application followed by laser treatment was feasible and efficacious for chairside porcelain repair.
引用
收藏
页码:731 / 737
页数:7
相关论文
共 28 条
[11]   BOND STRENGTHS OF INTRAORAL PORCELAIN REPAIR MATERIALS [J].
DIAZARNOLD, AM ;
SCHNEIDER, RL ;
AQUILINO, SA .
JOURNAL OF PROSTHETIC DENTISTRY, 1989, 61 (03) :305-309
[12]   IMPACT OF LASER ON DENTAL CARIES [J].
GOLDMAN, L ;
GOLDMAN, B ;
HORNBY, P ;
MEYER, R .
NATURE, 1964, 203 (494) :417-&
[13]   THE INFLUENCE OF SURFACE CONDITIONS AND SILANE AGENTS ON THE BOND OF RESIN TO DENTAL PORCELAIN [J].
HAYAKAWA, T ;
HORIE, K ;
AIDA, M ;
KANAYA, H ;
KOBAYASHI, T ;
MURATA, Y .
DENTAL MATERIALS, 1992, 8 (04) :238-240
[14]   Bond durability of the resin-bonded and silane treated ceramic surface [J].
Hooshmand, T ;
van Noort, R ;
Keshvad, A .
DENTAL MATERIALS, 2002, 18 (02) :179-188
[15]   DENTINAL TEMPERATURE TRANSIENTS CAUSED BY EXPOSURE TO CO2-LASER IRRADIATION AND POSSIBLE PULPAL DAMAGE [J].
JEFFREY, IWM ;
LAWRENSON, B ;
SAUNDERS, EM ;
LONGBOTTOM, C .
JOURNAL OF DENTISTRY, 1990, 18 (01) :31-36
[16]   Comparison of the load at failure of soldered and nonsoldered porcelain-fused-to-metal crowns [J].
Kang, MS ;
Ercoli, C ;
Galindo, DF ;
Graser, GN ;
Moss, ME ;
Tallents, RH .
JOURNAL OF PROSTHETIC DENTISTRY, 2003, 90 (03) :235-240
[17]  
Kawano F, 1998, Dent Mater J, V17, P41
[18]   Evaluation of porcelain surface treatments and agents for composite-to-porcelain repair [J].
Kupiec, KA ;
Wuertz, KM ;
Barkmeier, WW ;
Wilwerding, TM .
JOURNAL OF PROSTHETIC DENTISTRY, 1996, 76 (02) :119-124
[19]   LASERS IN DENTISTRY - COMPARING WAVELENGTHS [J].
KUTSCH, VKM .
JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 1993, 124 (02) :49-54
[20]   FRACTURE RESISTANCE OF METAL CERAMIC RESTORATIONS WITH TWO DIFFERENT MARGIN DESIGNS AFTER EXPOSURE TO MASTICATORY SIMULATION [J].
Michalakis, Konstantinos X. ;
Stratos, Athanasios ;
Hirayama, Hiroshi ;
Kang, Kiho ;
Touloumi, Foteini ;
Oishi, Yukio .
JOURNAL OF PROSTHETIC DENTISTRY, 2009, 102 (03) :172-178