Hot ductility behavior and HAZ hot cracking susceptibility of 7475-T7351 aluminum alloy

被引:5
|
作者
Yang, JG [1 ]
Ou, BL [1 ]
机构
[1] Natl Cent Univ, Dept Mech Engn, Chungli 320, Taiwan
关键词
aluminum alloy; hot cracking; heat-affected zone (HAZ); grain boundary liquation; hot ductility test; brittle temperature range (BTR);
D O I
10.1034/j.1600-0692.2001.300305.x
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The elevated temperature mechanical properties and hot crack susceptibility of the aluminum alloys, 7475-T7351 and 7005-T1 were evaluated using a Gleeble hot-ductility test. The 7475 alloy exhibited lower hot ductility and strength, significantly poorer ductility recovery on cooling from the nil-strength temperature, considerably wider brittle temperature range (BTR) and crack susceptible region (CSR), and thus greater susceptibility to heat-affected zone (HAZ) hot cracking, as compared to the 7005 alloy. Longitudinal samples of 7475 had a lower crack susceptibility than short-transverse 7475 samples. The results showed good agreement with those of the spot-Varestraint tests. Scanning electron microscopy (SEM) revealed that the ductility loss was accompanied by fracture transition from ductile transgranular mode to brittle intergranular mode. The HAZ hot cracking in alloy 7475 due to the loss of ductility was primarily caused by liquation of low-melting-point grain boundary segregates or eutectics that contained high amounts of Mg, Cu, and Zn.
引用
收藏
页码:146 / 157
页数:12
相关论文
共 50 条
  • [21] Evaluation of hot cracking susceptibility on laser welded aluminum alloy using coaxially arranged multiple-beam laser
    Kang, Minjung
    Kim, Cheolhee
    JOURNAL OF LASER APPLICATIONS, 2020, 32 (02)
  • [22] Investigation of hot cracking susceptibility in welding of AA5052 aluminium alloy
    Omprakasam, S.
    Marimuthu, K.
    Yoganandh, J.
    Raghu, R.
    MATERIALS AND MANUFACTURING PROCESSES, 2024, 39 (02) : 269 - 279
  • [23] Investigation of hot cracking behavior of AZ91 magnesium alloy
    Wang, YS
    Ding, WJ
    Wang, QD
    Zhu, YP
    ACTA METALLURGICA SINICA, 2001, 37 (05) : 527 - 530
  • [24] Effect of cooling rate on hot cracking susceptibility of T10 steel
    Sun, Quanzhi
    Li, Zhijun
    Zhong, Honggang
    Xu, Zhengqi
    Liang, Jianping
    Zhai, Qijie
    TMS 2009 138TH ANNUAL MEETING & EXHIBITION - SUPPLEMENTAL PROCEEDINGS, VOL 3: GENERAL PAPER SELECTIONS, 2009, : 461 - +
  • [25] Hot Cracking Susceptibility of Twin Roll Cast Al-Mg Alloy Welds
    Tirkes, Sueha
    Batigun, Caner
    Ankara, Alpay
    CANADIAN METALLURGICAL QUARTERLY, 2010, 49 (01) : 73 - 80
  • [26] Grain refinement in as-cast 7475 aluminum alloy under hot equal-channel angular pressing
    Goloborodko, A
    Sitdikov, O
    Sakai, T
    Kaibyshev, R
    Miura, H
    MATERIALS TRANSACTIONS, 2003, 44 (04) : 766 - 774
  • [27] Dynamic recrystallization behavior of 7085 aluminum alloy during hot deformation
    Li, Dong-feng
    Zhang, Duan-zheng
    Liu, Sheng-dan
    Shan, Zhao-jun
    Zhang, Xin-ming
    Wang, Qin
    Han, Su-qi
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2016, 26 (06) : 1491 - 1497
  • [28] Hot deformation behavior and constitutive modeling of homogenized 6026 aluminum alloy
    Chen, Liang
    Zhao, Guoqun
    Yu, Junquan
    MATERIALS & DESIGN, 2015, 74 : 25 - 35
  • [29] EVALUATION OF SUSCEPTIBILITY TO HOT CRACKING OF WE43 MAGNESIUM ALLOY WELDS IN TRANSVARESTRAINT TEST
    Scibisz, B.
    Adamiec, J.
    ARCHIVES OF METALLURGY AND MATERIALS, 2010, 55 (01) : 131 - 141
  • [30] Comparison of Hot Cracking Susceptibility of TIG and Laser Beam Welded Alloy 718 by Varestraint Testing
    Alvarez, Pedro
    Vazquez, Lexuri
    Ruiz, Noelia
    Rodriguez, Pedro
    Magana, Ana
    Niklas, Andrea
    Santos, Fernando
    METALS, 2019, 9 (09)