Influence of preparation design on fracture resistance of different monolithic zirconia crowns: A comparative study

被引:8
作者
Findakly, Meelad Basil [1 ]
Jasim, Haider Hasan [1 ]
机构
[1] Mustansiriyah Univ, Coll Dent, Dept Conservat Dent, Palestine St, Baghdad 14022, Iraq
关键词
Monolithic zirconia; Translucent; Ceramic; Feather-edge; Shoulder; CERAMIC CROWNS; SINGLE CROWNS; STRENGTH; TRANSLUCENCY; THICKNESS; STRESS; LOAD;
D O I
10.4047/jap.2019.11.6.324
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
PURPOSE. The aim of the study was to evaluate and compare the fracture resistance and modes of fracture of monolithic zirconia crowns with two preparation designs. MATERIALS AND METHODS. Forty human maxillary first premolar teeth were extracted for orthodontic purposes and divided into two main groups (n=20): Group A: monolithic traditional zirconia; Group B: monolithic translucent zirconia. The groups were further subdivided into two subgroups (n=10): (A1, B1) shoulder margin design; (A2, B2) feather-edge margin design. Teeth were prepared with either a 1 mm shoulder margin design or a feather-edge margin design. The prepared teeth were scanned using a digital intraoral scanner. The crowns were cemented using self-adhesive resin cement. All cemented teeth were stored in water for 7 days and thermocycling was done before testing. All samples were subjected to compressive axial loading until fracture. The fractographic analysis was done to assess the modes of fracture of the tested samples. RESULTS. The highest mean values of fracture resistance were recorded in kilonewton and were in the order of subgroup A1 (2.903); subgroup A2 (2.3); subgroup B1 (1.854) and subgroup B2 (1.523). One-way ANOVA showed a statistically significant difference among the 4 subgroups. Concerning modes of fracture, the majority of samples in subgroups A1 and B1 were fracture of restoration and/or tooth, while in subgroups A2 and B2, the majority of samples fractured through the central fossa. CONCLUSION. Even though all the tested crowns fractured at a higher level than the maximum occlusal forces, the shoulder margin design was better than the feather-edge margin design and the monolithic traditional zirconia was better than the monolithic translucent zirconia in terms of fracture strength.
引用
收藏
页码:324 / 330
页数:7
相关论文
共 34 条
  • [1] [Anonymous], 1994, 11405 ISOTR
  • [2] [Anonymous], 2017, FIR HTC SPEED OP INS
  • [3] Effect of preparation design on the fracture resistance of zirconia crown copings
    Beuer, Florian
    Aggstaller, Hans
    Edelhoff, Daniel
    Gernet, Wolfgang
    [J]. DENTAL MATERIALS JOURNAL, 2008, 27 (03) : 362 - 367
  • [4] In vitro performance of full-contour zirconia single crowns
    Beuer, Florian
    Stimmelmayr, Michael
    Gueth, Jan-Frederik
    Edelhoff, Daniel
    Naumann, Michael
    [J]. DENTAL MATERIALS, 2012, 28 (04) : 449 - 456
  • [5] Maximising the fracture resistance of dentine-bonded all-ceramic crowns
    Burke, FJT
    [J]. JOURNAL OF DENTISTRY, 1999, 27 (03) : 169 - 173
  • [6] Chitmongkolsuk Somsak, 2002, Eur J Prosthodont Restor Dent, V10, P15
  • [7] Church Todd D., 2017, General Dentistry, V65, P48
  • [8] de Lima E., 2015, Current Oral Health Reports, V2, P169
  • [9] Dolidze T, 2017, EUR SCI J, V12, P465
  • [10] Jalalian Ezatollah, 2011, J Dent Res Dent Clin Dent Prospects, V5, P41