Mechanical Properties and Microstructures of Severely Plastic Deformed Pure Titanium by Mechanical Milling and Spark Plasma Sintering

被引:2
作者
Kubota, Masahiro [1 ]
Ohno, Takuya [1 ]
机构
[1] Nihon Univ, Dept Mech Engn, Coll Ind Technol, Narashino, Chiba 2758575, Japan
来源
NANOMATERIALS BY SEVERE PLASTIC DEFORMATION: NANOSPD5, PTS 1 AND 2 | 2011年 / 667-669卷
关键词
Mechanical milling; severe plastic deformation; spark plasma sintering; pure titanium; powder consolidation; composite materials;
D O I
10.4028/www.scientific.net/MSF.667-669.559
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Severe plastic deformation (SPD) was applied to pure titanium powder by mechanical milling (MM) process with stearic acid, added as a process control agent (PCA), by using a vibrational ball mill, and MMed powders possessing large strains were subsequently consolidated into bulk materials by spark plasma sintering (SPS) in order to enhance the hardness and strength of pure titanium. Changes in the hardness and constituent phases of the MMed powders have been examined by microhardness measurements and X-ray diffraction. The hardness and microstructure of the SPS materials have also been studied by hardness measurements and optical microscopy. The Vickers microhardness of the pure titanium powders with PCA 0.25 g increased sharply from 189 HV to 513 HV after 8 h of the mechanical milling (MM) process. Formation of TiH2 as the solid-state reaction product occurred in the MMed powder during 4 and 8 h of the MM process. The near full density was obtained for the SPS materials under the condition of an applied pressure at 49 MPa with a sintering temperature at 1073 K for 0.5 h. The Vickers hardness of the SPS material fabricated from 8 h MMed powder with PCA 0.50 g exhibited a maximum value of 1253 HV.
引用
收藏
页码:559 / 564
页数:6
相关论文
共 17 条
[1]  
[Anonymous], 1999, 030859 JCPDS INT CTR
[2]  
[Anonymous], 1999, 321383 JCPDS INT CTR
[3]  
[Anonymous], 1999, 381420 JCPDS INT CTR
[4]  
ElEskandarany MS, 1996, MAT SCI ENG A-STRUCT, V217, P265, DOI 10.1016/S0921-5093(96)10344-0
[5]  
JAEGER NAF, 2001, ENG MAT SER, P343
[6]  
Kobashi M., 2001, J JAPAN I LIGHT META, V53, P427
[7]   Properties of nano-structured pure Al produced by mechanical grinding and spark plasma sintering [J].
Kubota, Masahiro .
JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 434 (SPEC. ISS.) :294-297
[8]  
Lu L., 1998, MECH ALLOYING
[9]   APPLICATION OF MECHANICAL ALLOYING TO CHEMICAL REFINING [J].
MCCORMICK, PG .
MATERIALS TRANSACTIONS JIM, 1995, 36 (02) :161-169
[10]  
Murty BS, 1998, INT MATER REV, V43, P101, DOI 10.1179/095066098790105654