In Vitro Monitoring of Magnesium-Based Implants Degradation by Surface Analysis and Optical Spectroscopy

被引:11
作者
Hassan, Hafiz Wajahat [1 ]
Rahmati, Maryam [2 ,3 ]
Barrantes, Alejandro [2 ,3 ]
Haugen, Havard Jostein [2 ,3 ]
Mirtaheri, Peyman [1 ]
机构
[1] Oslo Metropolitan Univ, Fac Technol Art & Design, Dept Mech Elect & Chem Engn, N-0130 Oslo, Norway
[2] Univ Oslo, Inst Clin Dent, Dept Biomat, N-0317 Oslo, Norway
[3] Univ Oslo, Oral Res Lab, N-0317 Oslo, Norway
关键词
degradation of magnesium; optical spectroscopy; partial-least-squares regression; bubble formation; in vitro monitoring; NEAR-INFRARED SPECTROSCOPY; VIVO CORROSION; ALLOYS; HYDROGEN; PH; EVOLUTION; COATINGS;
D O I
10.3390/ijms23116099
中图分类号
Q5 [生物化学]; Q7 [分子生物学];
学科分类号
071010 ; 081704 ;
摘要
Magnesium (Mg)-based degradable alloys have attracted substantial attention for tissue engineering applications due to their biodegradability and potential for avoiding secondary removal surgeries. However, insufficient data in the existing literature regarding Mg's corrosion and gas formation after implantation have delayed its wide clinical application. Since the surface properties of degradable materials constantly change after contact with body fluid, monitoring the behaviour of Mg in phantoms or buffer solutions could provide some information about its physicochemical surface changes over time. Through surface analysis and spectroscopic analysis, we aimed to investigate the structural and functional properties of degradable disks. Since bubble formation may lead to inflammation and change pH, monitoring components related to acidosis near the cells is essential. To study the bubble formation in cell culture media, we used a newly developed Mg alloy (based on Mg, zinc, and calcium), pure Mg, and commercially available grade 2 Titanium (Ti) disks in Dulbecco's Modified Eagle Medium (DMEM) solution to observe their behaviour over ten days of immersion. Using surface analysis and the information from near-infrared spectroscopy (NIRS), we concluded on the conditions associated with the medical risks of Mg alloy disintegration. NIRS is used to investigate the degradation behaviour of Mg-based disks in the cell culture media, which is correlated with the surface analysis where possible.
引用
收藏
页数:15
相关论文
共 55 条
  • [1] The in vivo and in vitro corrosion of high-purity magnesium and magnesium alloys WZ21 and AZ91
    Abidin, Nor Ishida Zainal
    Rolfe, Barbara
    Owen, Helen
    Malisano, Julian
    Martin, Darren
    Hofstetter, Joelle
    Uggowitzer, Peter J.
    Atrens, Andrej
    [J]. CORROSION SCIENCE, 2013, 75 : 354 - 366
  • [2] [Anonymous], 2012, PRACTICAL GUIDE SPEC, DOI [DOI 10.1201/B11894, 10.1201/b11894]
  • [3] Arrabal R., 2022, Encyclopedia of Materials: Metals and Alloys, V1st ed., P87
  • [4] Review of Recent Developments in the Field of Magnesium Corrosion
    Atrens, Andrej
    Song, Guang-Ling
    Liu, Ming
    Shi, Zhiming
    Cao, Fuyong
    Dargusch, Matthew S.
    [J]. ADVANCED ENGINEERING MATERIALS, 2015, 17 (04) : 400 - 453
  • [5] Application of Near-Infrared Spectroscopy for Monitoring and Control of Cell Culture and Fermentation
    Cervera, Albert E.
    Petersen, Nanna
    Lantz, Anna Eliasson
    Larsen, Anders
    Gernaey, Krist V.
    [J]. BIOTECHNOLOGY PROGRESS, 2009, 25 (06) : 1561 - 1581
  • [6] Inflammatory response to magnesium-based biodegradable implant materials
    Costantino, M. D.
    Schuster, A.
    Helmholz, H.
    Meyer-Rachner, A.
    Willumeit-Roemer, R.
    Luthringer-Feyerabend, B. J. C.
    [J]. ACTA BIOMATERIALIA, 2020, 101 : 598 - 608
  • [7] Near-infrared spectroscopy as a tool for in vivo analysis of human muscles
    Curra, Antonio
    Gasbarrone, Riccardo
    Cardillo, Alessandra
    Trompetto, Carlo
    Fattapposta, Francesco
    Pierelli, Francesco
    Missori, Paolo
    Bonifazi, Giuseppe
    Serranti, Silvia
    [J]. SCIENTIFIC REPORTS, 2019, 9 (1)
  • [8] EILERS P, 2003, J CHEMOMETR, V17, P360, DOI DOI 10.1002/CEM.804
  • [9] In vivo degradation performance of micro-arc-oxidized magnesium implants: A micro-CT study in rats
    Fischerauer, S. F.
    Kraus, T.
    Wu, X.
    Tangl, S.
    Sorantin, E.
    Haenzi, A. C.
    Loeffler, J. F.
    Uggowitzer, P. J.
    Weinberg, A. M.
    [J]. ACTA BIOMATERIALIA, 2013, 9 (02) : 5411 - 5420
  • [10] Corrosion Behavior of Magnesium Based Foam Structure in Hank's Solution
    Franciska, P. L.
    Erryani, A.
    Annur, D.
    Kartika, I.
    [J]. 4TH INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS SCIENCE AND TECHNOLOGY, 2016, 2017, 202