Low-temperature fabrication of anorthite ceramics from kaolinite and calcium carbonate with boron oxide addition

被引:60
作者
Mergen, A
Aslanoglu, VZ
机构
[1] Eti Holdings AS, ARGE Dairesi Baskanligi, Ankara, Turkey
[2] Sakarya Univ, Adapazari, Turkey
关键词
sintering; anorthite; kaolinite; calcite; boron oxide;
D O I
10.1016/S0272-8842(02)00215-8
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Anorthite ceramics were fabricated by using groleg kaolinite, calcite and quartz with addition of boron oxide and without the need of very fine particles. Single phase anorthite ceramic with a density of 87% of the therotical was obtained at a sintering temperature of 950 degreesC. Moreover. no single anorthite phase could be obtained from boron free specimens even at a sintering temperature of 1100 degreesC. SEM investigation revealed that although boron free samples contain very small crystals together with some larger grains, boron containing samples generally had a fine grained matrix of crystals. (C) 2003 Elsevier Ltd and Techna S.r.l. All rights reserved.
引用
收藏
页码:667 / 670
页数:4
相关论文
共 31 条
[31]   Effects of CuO addition on the electrical responses of the low-temperature sintered Pb(Zr0.52Ti0.48)O3-Pb(Mg1/3Nb2/3)O3-Pb(Zn1/3Nb2/3)O3 ceramics [J].
Chao, Xiaolian ;
Ma, Difei ;
Gu, Rui ;
Yang, Zupei .
JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 491 (1-2) :698-702