Effects of different cooling rates on the microstructure, crystallographic features, and hydrogen induced cracking of API X80 pipeline steel

被引:54
作者
Ramirez, Mario F. G. [1 ]
Hernandez, Jose W. C. [2 ,3 ,4 ]
Ladino, Duberney H. [5 ]
Masoumi, Mohammad [6 ]
Goldenstein, Helio [2 ,3 ,4 ]
机构
[1] Univ Santiago Cali, Fac Ingn, Campus Pampalinda,Calle 5 62, Cali, Colombia
[2] Univ Sao Paulo, Dept Engn Metalurg & Mat, Av Prof Mello Moraes, Sao Paulo, SP, Brazil
[3] Univ Sao Paulo, Escola Politecn, Av Prof Mello Moraes, Sao Paulo, SP, Brazil
[4] EPUSP PMT, Av Prof Mello Moraes, Sao Paulo, SP, Brazil
[5] Fac Ingn Mecan, Campus Aguas Claras, Villavicencio, Colombia
[6] Univ Fed ABC, Ctr Engn Modelagem & Ciencias Sociais Aplicadas, BR-09210580 Santo Andre, SP, Brazil
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2021年 / 14卷
关键词
HSLA; Electron backscattered diffraction; Strain distribution; Grain orientation; HIC; SULFIDE STRESS CRACKING; HEAT-AFFECTED ZONES; MECHANICAL-PROPERTIES; ACICULAR FERRITE; BEHAVIOR; TEXTURE; IMPACT; PROPAGATION; ENVIRONMENT; TOUGHNESS;
D O I
10.1016/j.jmrt.2021.07.060
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hydrogen-Induced Cracking (HIC) is a primary failure mechanism of pipeline-welded joints in the absence of external loading in the oil and gas exploration industries. Three different cooling rates after austenitization were used to simulate in the laboratory different regions of the heat-affected zone (HAZ) formed when welding an API X80 pipeline steel specially designed to enhance the HIC resistance. The samples were characterized with regard to microstructure and crystallography as well as HIC resistance. The HIC resistance test used NACE TM0284-2011 methodology. The microstructure and its homogeneity varied as a function of cooling rates. Samples containing inclusions and segregation zone from the segregation bands of specimens showed reduced HIC resistance, while specimens containing only acicular ferrite and granular bainite coupled with the absence of segregation zone showed significant improvement in HIC resistance. The best HIC resistance results came from samples presenting fine acicular ferrite consisting of fine interlocking plates, with divergent crystallographic orientations, preventing the formation of localized strain distribution inside the grain and at grain boundaries. It was also found that a large proportion of medium-angle boundaries prevent microcrack initiation and the trans granular mode of crack propagation. (c) 2021 The Author(s). Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:1848 / 1861
页数:14
相关论文
共 50 条
[21]   Effects of Cooling Paths on Through-Thickness Microstructure and Mechanical Properties of Heavy Gauge X80 Pipeline Steel [J].
Xu-Dong Li ;
Cheng-Ning Li ;
Guo Yuan ;
Guo-Dong Wang .
Acta Metallurgica Sinica (English Letters), 2017, 30 :483-492
[22]   Effects of finish rolling deformation on hydrogen-induced cracking and hydrogen-induced ductility loss of high-vanadium TMCP X80 pipeline steel [J].
Li, Longfei ;
Song, Bo ;
Cui, Xiaokang ;
Liu, Zhen ;
Wang, Lei ;
Cheng, Wensen .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2020, 45 (55) :30828-30844
[23]   Effects of internal hydrogen and surface-absorbed hydrogen on the hydrogen embrittlement of X80 pipeline steel [J].
Zhou, Chengshuang ;
Ye, Baoguo ;
Song, Yangyang ;
Cui, Tiancheng ;
Xu, Peng ;
Zhang, Lin .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2019, 44 (40) :22547-22558
[24]   The mechanism of failure by hydrogen induced cracking in an acidic environment for API 5L X70 pipeline steel [J].
Mohtadi-Bonab, M. A. ;
Szpunar, J. A. ;
Basu, R. ;
Eskandari, M. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2015, 40 (02) :1096-1107
[25]   Microstructure and Properties of an X80 Pipeline Steel Manufactured by Untraditional TMCP [J].
Deng, Wei ;
Gao, Xiuhua ;
Qin, Xiaomei ;
Zhao, Dewen ;
Du, Linxiu .
ADVANCED SCIENCE LETTERS, 2011, 4 (03) :1088-1092
[26]   Fatigue crack growth law of API X80 pipeline steel under various stress ratios based on J-integral [J].
Li, L. ;
Yang, Y. H. ;
Xu, Z. ;
Chen, G. ;
Chen, X. .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2014, 37 (10) :1124-1135
[27]   Effect of Ultra Fast Cooling on the Alloy Cost Reduction of the X80 Pipeline Steel [J].
Zhou, Feng ;
Wu, Kaiming M. ;
Zhang, Cong ;
Isayev, Oleg ;
Hodgson, Peter D. .
STEEL RESEARCH INTERNATIONAL, 2016, 87 (04) :511-518
[28]   Microstructure - Texture Related Toughness Anisotropy of API-X80 Pipeline Steel [J].
Garcia, Orlando Leon ;
Petrov, Roumen ;
Bae, Jin-Ho ;
Kestens, Leo ;
Kang, Ki Bong .
THERMEC 2006 SUPPLEMENT: 5TH INTERNATIONAL CONFERENCE ON PROCESSING AND MANUFACTURING OF ADVANCED MATERIALS, 2007, 15-17 :840-845
[29]   Effect of Nb on microstructure and corrosion resistance of X80 pipeline steel [J].
Xia, Fan ;
Li, Zhiwei ;
Ma, Ming ;
Zhao, Yonggang ;
Wu, Changjun ;
Su, Xuping ;
Peng, Haoping .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2023, 203
[30]   Investigation of the hydrogen induced cracking behaviour of API 5L X65 pipeline steel [J].
Jack, Tonye Alaso ;
Pourazizi, Reza ;
Ohaeri, Enyinnaya ;
Szpunar, Jerzy ;
Zhang, Jiming ;
Qu, Jinbo .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2020, 45 (35) :17671-17684