Wear behaviour of Mg alloys and their composites - a review

被引:26
作者
Dey, Abhijit [1 ]
Pandey, Krishna Murari [2 ]
机构
[1] Madanapalle Inst Technol & Sci, Dept Mech Engn, Madanapalle, India
[2] Natl Inst Technol, Dept Mech Engn, Silchar, India
关键词
Magnesium alloys; Wear mechanism; Delamination; Oxidation; Plastic yielding; AZ91D MAGNESIUM ALLOY; TEMPERATURE MECHANICAL-PROPERTIES; TRIBOLOGICAL BEHAVIOR; MICROSTRUCTURAL EVOLUTION; MATRIX COMPOSITES; SILICON-CARBIDE; AS-CAST; FRICTION; RESISTANCE; COATINGS;
D O I
10.3139/146.111707
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Magnesium metal matrix composites (MMCs) have generated keen interest in recent times for potential usage in automotive and aerospace industries owing to their superior strength to weight ratio and high temperature resistance. With the concurrent attention to the requirements of high wear resistance and weight reduction, research into magnesium based MMCs has produced significant contributions in the automotive industry in the last few decades. Materials possessing high wear resistance under dry sliding conditions are associated with a stable tribo-layer on the worn surface and the formation of fine equiaxed wear debris. For abrasive wear, the influence of sliding speed, applied load, wearing surface hardness, reinforcement fracture toughness, percentages of reinforcement and morphology are critical parameters in relation to the wear regime encountered by the material. In this review, contemporary wear theories, issues associated with counter-face wear, and wear mechanisms are discussed in detail. Other areas of research relevant to abrasive wear of Al-based Mg alloys and Mg MMCs containing discontinuous reinforcement phases, such as the role of the reinforcement phase, are presented. Major effects such as interfacial transition, agglomerating phenomenon, formation, and distribution of in-situ Mg2Si, MgAl2O4, beta-Mg(17)Al(12)and MgO in the metallic matrix, filler-matrix bonding and phase transition are discussed in this article.
引用
收藏
页码:1050 / 1070
页数:21
相关论文
共 87 条
[1]   Dry sliding wear behavior of SiCp/QE22 magnesium alloy matrix composites [J].
Abachi, P. ;
Masoudi, A. ;
Purazrang, K. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 435 :653-657
[2]  
Ai XL, 2011, MAGNESIUM ALLOYS - DESIGN, PROCESSING AND PROPERTIES, P351
[3]   Dry sliding wear behavior of magnesium alloys [J].
An, J. ;
Li, R. G. ;
Lu, Y. ;
Chen, C. M. ;
Xu, Y. ;
Chen, X. ;
Wang, L. M. .
WEAR, 2008, 265 (1-2) :97-104
[4]   Tribological Characteristics of Mg-3Al-0.4Si-0.1Zn Alloy at Elevated Temperatures of 50-200 °C [J].
An, J. ;
Zhang, Y. X. ;
Lv, X. X. .
TRIBOLOGY LETTERS, 2018, 66 (01)
[5]   Dry Sliding Wear Behavior and a Proposed Criterion for Mild to Severe Wear Transition of Mg-3Al-0.4Si-0.1Zn Alloy [J].
An, J. ;
Sun, W. ;
Niu, X. D. .
TRIBOLOGY LETTERS, 2017, 65 (03)
[6]   Electroless deposition of Ni-P-B4C composite coating on AZ91D magnesium alloy and investigation on its wear and corrosion resistance [J].
Araghi, A. ;
Paydar, M. H. .
MATERIALS & DESIGN, 2010, 31 (06) :3095-3099
[7]   THE WEAR OF METALS UNDER UNLUBRICATED CONDITIONS [J].
ARCHARD, JF ;
HIRST, W .
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL AND PHYSICAL SCIENCES, 1956, 236 (1206) :397-&
[8]  
Asi K. M., 2010, MAT SCI ENG A-STRUCT, V527, P2027, DOI [10.1016/j.msea.2009.11.061, DOI 10.1016/J.MSEA.2009.11.061]
[9]   Wear behaviour of AZ91D alloy at low sliding speeds [J].
Aung, Naing Naing ;
Zhou, Wei ;
Lim, Lennie E. N. .
WEAR, 2008, 265 (5-6) :780-786
[10]  
Avedesian MichaelM., 1999, ASM Specialty Handbook