Relationship between microstructure and mechanical properties of friction stir processed AISI 316L steel produced by selective laser melting

被引:38
作者
Peng, Pai [1 ,2 ]
Wang, Kuaishe [1 ,2 ]
Wang, Wen [1 ,2 ]
Han, Peng [1 ,2 ]
Zhang, Ting [1 ,2 ]
Liu, Qiang [1 ,2 ]
Zhang, Shengyi [1 ,2 ]
Wang, Hongduo [1 ]
Qiao, Ke [1 ,2 ]
Liu, Jian [3 ,4 ]
机构
[1] Xian Univ Architecture & Technol, Sch Met Engn, Xian 710055, Peoples R China
[2] Natl & Local Joint Engn Res Ctr Funct Mat Proc, Xian 710055, Peoples R China
[3] Chinese Acad Sci, Ningbo Inst Mat Technol & Engn, CAS Key Lab Magnet Mat & Devices, Ningbo 315201, Peoples R China
[4] Chinese Acad Sci, Ningbo Inst Mat Technol & Engn, Zhejiang Prov Key Lab Magnet Mat & Applicat Techn, Ningbo 315201, Peoples R China
基金
中国国家自然科学基金;
关键词
Selective laser melting; Friction stir processing; AISI; 316L; Microstructure; Nano-hardness; Mechanical properties; AUSTENITIC STAINLESS-STEEL; STACKING-FAULT ENERGY; CRACK GROWTH-BEHAVIOR; SUB-GRAIN STRUCTURE; DISLOCATION DENSITIES; HEAT-TREATMENT; HIGH-STRENGTH; DEFORMATION; ALLOY; EVOLUTION;
D O I
10.1016/j.matchar.2020.110283
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, AISI 316L steel produced through selective laser melting (SLMed 316L) was successfully modified through friction stir processing (FSP) technology. The microstructure, microhardness, nano-hardness and tensile properties of SLMed 316L were studied and the results were discussed. The effects of microstructure evolution, including grain size, grain orientation and dislocations, on both macroscopic and microscopic mechanical behavior of the material were examined. The relationship between grain orientation and nano-hardness was corrected for the Berkovich nanoindenter. It was demonstrated that FSP could effectively eliminate the holes and cracks of SLMed 316L, leading to refined, homogenous and dense microstructure. During FSP, SLMed 316L sustained both continuous and discontinuous dynamic recrystallization. Subsequently to FSP, the grain size was refined from 6.6 to 0.9 mu m total dislocation density decreased from 2.43 x 10(15) to 1.04 x 10(15) m(-2) , while geometrically necessary dislocation density increased from 2.16 x 10(14) to 8.25 x 10(14 )m(-2). The average microhardness and nano-hardness increased from 272 to 218 HV and 3.61 to 4.18 GPa, respectively. The yield and tensile strengths increased by 29% and 18%, respectively, while elongation was maintained. The main factors affecting the strength of SLMed 316L was grain size, followed by grain orientation and dislocation density.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Microstructure and properties of CLAM/316L steel friction stir welded joints
    Tang, Wenshen
    Yang, Xinqi
    Li, Shengli
    Li, Huijun
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2019, 271 : 189 - 201
  • [32] Effect of annealing and strain rate on the microstructure and mechanical properties of austenitic stainless steel 316L manufactured by selective laser melting
    Zhou, Zhi-Ping
    Tan, Zhi-Heng
    Lv, Jin-Long
    Zhang, Shu-Ye
    Liu, Di
    ADVANCES IN MANUFACTURING, 2024,
  • [33] Effect of energy density and scanning strategy on densification, microstructure and mechanical properties of 316L stainless steel processed via selective laser melting
    Larimian, Taban
    Kannan, Manigandan
    Grzesiak, Dariusz
    AlMangour, Bandar
    Borkar, Tushar
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 770
  • [34] Influence of Heat Treatment of Steel AISI316L Produced by the Selective Laser Melting Method on the Properties of Welded Joint
    Mohyla, Petr
    Hajnys, Jiri
    Gembalova, Lucie
    Zapletalova, Andrea
    Krpec, Pavel
    MATERIALS, 2022, 15 (05)
  • [35] Effect of post-heat treatment cooling on microstructure and mechanical properties of selective laser melting manufactured austenitic 316L stainless steel
    Waqar, Saad
    Liu, Jiangwei
    Sun, Qidong
    Guo, Kai
    Sun, Jie
    RAPID PROTOTYPING JOURNAL, 2020, 26 (10) : 1739 - 1749
  • [36] Microstructure and Mechanical Properties of 316L Stainless Steel Filling Friction Stir-Welded Joints
    L. Zhou
    K. Nakata
    T. Tsumura
    H. Fujii
    K. Ikeuchi
    Y. Michishita
    Y. Fujiya
    M. Morimoto
    Journal of Materials Engineering and Performance, 2014, 23 : 3718 - 3726
  • [37] Tensile Properties of Selective Laser Melted 316L Stainless Steel
    Yu Chenfan
    Zhao Congcong
    Zhang Zhefeng
    Liu Wei
    ACTA METALLURGICA SINICA, 2020, 56 (05) : 683 - 692
  • [38] Investigation on elastic properties and unconventional plasticity of 316L stainless steel processed by selective laser melting technology
    Ara, Ismat
    Eshkabilov, Sulaymon
    Azarmi, Fardad
    Sevostianov, Igor
    Tangpong, Xiangqing W.
    PROGRESS IN ADDITIVE MANUFACTURING, 2022, 7 (06) : 1169 - 1181
  • [39] Microstructure and Mechanical Properties of 316L Stainless Steel Filling Friction Stir-Welded Joints
    Zhou, L.
    Nakata, K.
    Tsumura, T.
    Fujii, H.
    Ikeuchi, K.
    Michishita, Y.
    Fujiya, Y.
    Morimoto, M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2014, 23 (10) : 3718 - 3726
  • [40] Anisotropy in Microstructure and Impact Toughness of 316L Austenitic Stainless Steel Produced by Selective Laser Melting
    Zong Xuewen
    Liu Wenjie
    Yang Yumeng
    Zhang Shuzhe
    Chen Zhen
    RARE METAL MATERIALS AND ENGINEERING, 2020, 49 (12) : 4031 - 4040