Kinetics of apatite formation on a calcium-silicate cement for root-end filling during ageing in physiological-like phosphate solutions
被引:78
作者:
Gandolfi, Maria Giovanna
[1
,2
]
Taddei, Paola
[3
]
Tinti, Anna
[3
]
Dorigo, Elettra De Stefano
[4
]
Rossi, Piermaria Luigi
[1
]
Prati, Carlo
[2
]
机构:
[1] Univ Bologna, Dept Earth Sci, Bologna, Italy
[2] Univ Bologna, Lab Biomat & Oral Pathol, Dept Odontostomatol Sci, Endodont Clin Sect, Bologna, Italy
[3] Univ Bologna, Dept Biochem, I-40126 Bologna, Italy
[4] Univ Trieste, Dept Biomed, Unit Dent Sci & Biomat, Trieste, Italy
关键词:
Calcium-silicate cements;
MTA cements;
Portland cement;
Ageing;
Phosphate solutions;
Apatite;
Calcite;
MINERAL TRIOXIDE AGGREGATE;
IN-VITRO BIOACTIVITY;
ACCELERATED PORTLAND-CEMENT;
RAMAN-SPECTROSCOPY;
SETTING PROPERTIES;
LONG-TERM;
HYDRATION;
MTA;
BIOCOMPATIBILITY;
CONSTITUTION;
D O I:
10.1007/s00784-009-0356-3
中图分类号:
R78 [口腔科学];
学科分类号:
1003 ;
摘要:
The bioactivity of calcium silicate mineral trioxide aggregate (MTA) cements has been attributed to their ability to produce apatite in presence of phosphate-containing fluids. This study evaluated surface morphology and chemical transformations of an experimental accelerated calcium-silicate cement as a function of soaking time in different phosphate-containing solutions. Cement discs were immersed in Dulbecco's phosphate-buffered saline (DPBS) or Hank's balanced salt solution (HBSS) for different times (1-180 days) and analysed by scanning electron microscopy connected with an energy dispersive X-ray analysis (SEM-EDX) and micro-Raman spectroscopy. SEM-EDX revealed Ca and P peaks after 14 days in DPBS. A thin Ca- and P-rich crystalline coating layer was detected after 60 days. A thicker multilayered coating was observed after 180 days. Micro-Raman disclosed the 965-cm(-1) phosphate band at 7 days only on samples stored in DPBS and later the 590- and 435-cm(-1) phosphate bands. After 60-180 days, a layer similar to 200-900 mu m thick formed displaying the bands of carbonated apatite (at 1,077, 965, 590, 435 cm(-1)) and calcite (at 1,088, 713, 280 cm(-1)). On HBSS-soaked, only calcite bands were observed until 90 days, and just after 180 days, a thin apatite-calcite layer appeared. Micro-Raman and SEM-EDX demonstrated the mineralization induction capacity of calcium-silicate cements (MTAs and Portland cements) with the formation of apatite after 7 days in DPBS. Longer time is necessary to observe bioactivity when cements are immersed in HBSS.