Investigating the strength of Ti/TiB interfaces at multiple scales using density functional theory, molecular dynamics, and cohesive zone modeling

被引:13
作者
Attarian, Siamak [1 ]
Xiao, Shaoping [1 ]
机构
[1] Univ Iowa, Technol Inst, Dept Mech Engn, Iowa City, IA 52242 USA
基金
美国国家科学基金会;
关键词
Metal matrix composite; Metal; ceramic interface; Cohesive zone modeling; Stacking fault energies; Molecular dynamics simulations; IN-SITU PREPARATION; MICROSTRUCTURE EVOLUTION; MECHANICAL-PROPERTIES; TITANIUM-ALLOYS; 1ST PRINCIPLES; EQUIAXED ALPHA; PURE TI; COMPOSITE; SIMULATIONS; NUCLEATION;
D O I
10.1016/j.ceramint.2022.07.259
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Titanium/titanium boride (Ti/TiB) composites are interesting technological materials with prospective appli-cations in the aerospace, automotive, and biomedical industries. However, not much has been studied about the failure mechanisms of these composites. This article thoroughly investigates the adhesion and strength of two well-known Ti/TiB interface variants formed during the production of Ti/TiB composites below and above 910 degrees C, respectively. The studies were carried out using different theoretical methods at multiple scales, including density functional theory (DFT), molecular dynamics (MD), cohesive zone modeling (CZM), and the finite element method (FEM). First, we employed DFT to investigate the interfacial adhesion and strength of the selected planes. Then, MD simulations were utilized to study the misfit dislocation networks and derive inter-facial CZMs for FEM modeling and simulation of composites. Our FEM simulations showed that the Ti/TiB interface has sufficient strength to transfer the shear load from Ti to TiB without debonding at room temperature. The results have confirmed the same phenomenon observed in some experimental studies and interpreted this phenomenon from a multiscale point of view. The research findings can be used in quantifying the failure stress of TiB whiskers directly from tension tests on Ti/TiB composites by ruling out the possibility of interface debonding.
引用
收藏
页码:33185 / 33199
页数:15
相关论文
共 77 条
[61]   The effects of friction-stir process parameters on the fabrication of Ti/SiC nano-composite surface layer [J].
Shamsipur, Ali ;
Kashani-Bozorg, Seyed Farshid ;
Zarei-Hanzaki, Abbas .
SURFACE & COATINGS TECHNOLOGY, 2011, 206 (06) :1372-1381
[62]   Determination of interfacial mechanical properties of ceramic composites by the compression of micro-pillar test specimens [J].
Shih, Chunghao ;
Katoh, Yutai ;
Leonard, Keith J. ;
Bei, Hongbin ;
Lara-Curzio, Edgar .
JOURNAL OF MATERIALS SCIENCE, 2013, 48 (15) :5219-5224
[63]   In situ neutron diffraction observations of Ti-TiB composites [J].
Singh, Harshpreet ;
Hayat, Muhammad ;
He, Zhen ;
Peterson, Vanessa K. ;
Das, Raj ;
Cao, Peng .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2019, 124
[64]   Effect of TiB2 content on microstructure and properties of in situ Ti-TiB composites [J].
Singh, Harshpreet ;
Hayat, Muhammad ;
Zhang, Hongzhou ;
Das, Raj ;
Cao, Peng .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2019, 26 (07) :915-924
[65]  
Smith M., 2009, ABAQUS/Standard User's Manual, Version 6.9
[66]   3D ink-extrusion printing and sintering of Ti, Ti-TiB and Ti-TiC microlattices [J].
Song, Binna ;
Kenel, Christoph ;
Dunand, David C. .
ADDITIVE MANUFACTURING, 2020, 35
[67]   Anisotropic elastic and thermal properties of titanium borides by first-principles calculations [J].
Sun, Liang ;
Gao, Yimin ;
Xiao, Bing ;
Li, Yefei ;
Wang, Guoliang .
JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 579 :457-467
[68]   Characterization of nanoscale deformation in a discontinuously reinforced titanium composite using AFM and nanolithography [J].
Tanaka, Y. ;
Yang, J. -M. ;
Liu, Y. F. ;
Kagawa, Y. .
SCRIPTA MATERIALIA, 2007, 56 (03) :209-212
[69]   LAMMPS-a flexible simulation tool for particle-based materials modeling at the atomic, meso, and continuum scales [J].
Thompson, Aidan P. ;
Aktulga, H. Metin ;
Berger, Richard ;
Bolintineanu, Dan S. ;
Brown, W. Michael ;
Crozier, Paul S. ;
Veld, Pieter J. in 't ;
Kohlmeyer, Axel ;
Moore, Stan G. ;
Nguyen, Trung Dac ;
Shan, Ray ;
Stevens, Mark J. ;
Tranchida, Julien ;
Trott, Christian ;
Plimpton, Steven J. .
COMPUTER PHYSICS COMMUNICATIONS, 2022, 271
[70]   FIBER DEBONDING AND BREAKAGE IN A WHISKER-REINFORCED METAL [J].
TVERGAARD, V .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 190 (1-2) :215-222