The effects of an inorganic corrosion inhibitor on the electrochemical behavior of superhydrophobic micro-nano structured Ni films in 3.5% NaCl solution

被引:47
|
作者
Nezhad, A. H. Noorbakhsh [1 ]
Davoodi, A. [1 ,2 ]
Zahrani, E. Mohammadi [1 ]
Arefinia, R. [3 ]
机构
[1] Ferdowsi Univ Mashhad, Fac Engn, Dept Met & Mat Engn, Mashhad 917751111, Razavi Khorasan, Iran
[2] Harvard Univ, John A Paulson Sch Engn & Appl Sci, Cambridge, MA 02138 USA
[3] Ferdowsi Univ Mashhad FUM, Fac Engn, Dept Chem Engn, Mashhad 917751111, Razavi Khorasan, Iran
关键词
Ni film; Corrosion inhibitor; EIS; Corrosion resistance; Electrodeposition; Superhydrophobicity; DISLOCATION-DRIVEN GROWTH; HYDROPHOBIC NICKEL FILM; STEP ELECTRODEPOSITION; FABRICATION; SURFACE; RESISTANCE; COATINGS; SELF; ALLOY; ANTICORROSION;
D O I
10.1016/j.surfcoat.2020.125946
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The application of hierarchically micro-nano structured superhydrophobic Ni films with increased surface roughness is known as an attractive corrosion protection strategy because the chemically modified film with a low surficial free energy is capable of keeping water molecules and aggressive species away from the coating/electrolyte interface by trapping air pockets within the micro-nano structured layer. Furthermore, corrosion inhibitors are widely used for corrosion mitigation in a broad range of industrial applications. This study tends to investigate the corrosion resistance of electrodeposited superhydrophobic Ni films in the presence of sodium molybdate (0 M, 0.03 M, 0.06 M, 0.1 M) as an inorganic corrosion inhibitor in a 3.5 wt% NaCl solution at 25 degrees C, up to 120 h. The micro-nano structured superhydrophobic Ni film with a mean thickness of 4 mu m was electrodeposited on a Cu substrate via a two-step electrodeposition process at 60 degrees C including 8 min of electrodeposition at a constant current density of 20 mA/cm(2), followed by 1 min of electrodeposition at a constant current density of 50 mA/cm(2) and a subsequent chemical modification step in stearic acid solution. Investigation of surface topography of the film by atomic force microscopy technique (AFM) revealed that the root-mean-square of height and the skewness of the film were equal to 14.4 nm and 0.21, respectively. The morphology of the film consisted of micro-nano cones in the size range of 50 to 1000 nm. The superhydrophobic film demonstrated a passivation behavior and a pitting potential. The EIS study identified the Ni film as a non-ideal capacitor and an equivalent circuit model with two parallel time-constants fitted to the EIS data. Upon 120 h of immersion of the superhydrophobic film in the electrolyte in the presence of 0.1 M of sodium molybdate, the corrosion inhibitor efficiency of about 80% was achieved and the Ni film demonstrated the best passivation behavior and the lowest corrosion current density.
引用
收藏
页数:16
相关论文
共 50 条
  • [21] Characterizing the Electrochemical Corrosion Behaviour of a Ni- 28wt.%Al Composite Coating in 3.5% NaCl Solution
    Onyeachu, B. I.
    Peng, X.
    Oguzie, E. E.
    Ogukwe, C. E.
    Digbo, I.
    PORTUGALIAE ELECTROCHIMICA ACTA, 2015, 33 (02) : 69 - 83
  • [22] Fabrication and Electrochemical Corrosion Behavior of PEO Coatings on Strip-Cast AZ31Mg Alloy in 3.5% NaCl Solution
    Kumar, Arumugam Madhan
    Kwon, Sun Hwan
    Jung, Hwa Chul
    Park, Young Hee
    Kim, Hea Jeong
    Shin, Kwang Seon
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2014, 53 (23) : 9703 - 9713
  • [23] Corrosion behavior of wire-arc additive manufactured and as-cast Ni-Al bronze in 3.5 wt% NaCl solution
    Xu, Cheng
    Peng, Yong
    Chen, Liang-Yu
    Zhang, Tian-Yang
    He, Shen
    Wang, Ke-Hong
    CORROSION SCIENCE, 2023, 215
  • [24] Electrochemical Corrosion Behavior of Magnetron-Sputtered Al-Mo Gradient-Coated Steel in 3.5 wt.% NaCl Solution
    Venugopal, A.
    Narayanan, P. Ramesh
    Sharma, S. C.
    George, Koshy M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (03) : 790 - 799
  • [25] Effects of Aging Treatment on Corrosion Behavior of a Tensile Deformed Al-Cu-Mn-Fe-Zr Alloy in 3.5% NaCl Solution
    Tian, Qing
    Yang, Qiu-Mei
    Lin, Yong-Cheng
    Wang, Jun-Quan
    Zhu, Xu-Hao
    MATERIALS, 2021, 14 (17)
  • [26] Adsorption Behavior and Corrosion Inhibition Mechanism of Three Amino Acids on Mild Steel in 3.5% NaCl Solution: Electrochemical and Computational Studies
    Han, Dong
    Li, Jiarun
    Wang, Ning
    Wan, Kai
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2020, 15 (10): : 9631 - 9657
  • [27] Electrochemical behavior of amorphous alloy Zr55Al10Cu30Ni5 in 3.5%NaCl solution
    Wang, C
    Zhang, QS
    Jiang, F
    Zhang, HF
    Hu, ZQ
    ACTA METALLURGICA SINICA, 2002, 38 (07) : 765 - 769
  • [28] Effects of Ca and Ag addition and heat treatment on the corrosion behavior of Mg-7Sn alloys in 3.5 wt.% NaCl solution
    Li, Wandong
    SURFACE AND INTERFACE ANALYSIS, 2022, 54 (06) : 631 - 641
  • [29] Tribological behavior of electroless Ni-B-Mo coatings under dry and lubricated conditions and corrosion resistance in 3.5% NaCl solution
    Mukhopadhyay, Arkadeb
    Barman, Tapan K.
    Sahoo, Prasanta
    JURNAL TRIBOLOGI, 2018, 18 : 108 - 123
  • [30] Electrochemical Behavior of Three 90Cu-10Ni Tubes from Different Manufacturers After Immersion in 3.5% NaCl Solution
    Ekerenam, Okpo O.
    Ma, Aili
    Zheng, Yugui
    Emori, Wilfred
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (04) : 1701 - 1716