Physical properties characterization of WO3 films grown by hot-filament metal oxide deposition

被引:26
|
作者
Diaz-Reyes, J. [1 ]
Delgado-Macuil, R. J. [1 ]
Dorantes-Garcia, V. [2 ]
Perez-Benitez, A. [3 ]
Balderas-Lopez, J. A. [4 ]
Ariza-Ortega, J. A. [1 ]
机构
[1] Inst Politecn Nacl, Ctr Invest Biotecnol Aplicada, Tepetitla 90700, Tlaxcala, Mexico
[2] Preparatoria Simon Bolivar Benemerita Univ Autono, Puebla 74200, Mexico
[3] Benemerita Univ Autonoma Puebla, Fac Ciencias Quim, Puebla 72570, Mexico
[4] Inst Politecn Nacl, Unidad Prof Interdisciplinaria Biotecnol, Mexico City 07340, DF, Mexico
来源
MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS | 2010年 / 174卷 / 1-3期
关键词
Compound semiconductors; Hot Filament Metal Oxide Deposition; Novel Materials and Technological; Advances for electrochromics; Semiconductors growth; WO3; semiconductors; TUNGSTEN TRIOXIDE FILMS; THIN-FILMS; RAMAN-SPECTROSCOPY; AMORPHOUS WO3; COATINGS; DYNAMICS; PROGRESS;
D O I
10.1016/j.mseb.2010.03.061
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
WO3 is grown by hot-filament metal oxide deposition (HFMOD) technique under atmospheric pressure and an oxygen atmosphere. By X-ray diffraction obtains that WO3 presents mainly monoclinic crystalline phase. The chemical stoichiometry is obtained by X-ray Photoelectron Spectroscopy (XPS). The IR spectrum of the as-grown WO3 presents broad peaks in the range of 1100 to 3600 cm(-1). A broad band in the 2200 to 3600 cm(-1) region and the peaks sited at 1645 and 1432 cm(-1) are well resolved, which are originated from moisture and are assigned to nu(OH) and delta(OH) modes of adsorbed water and the corresponding tungsten oxide vibrations are in infrared region from 400 to 1453 cm(-1) and around 3492 cm(-1), which correspond to tungsten-oxygen (W-O) stretching, bending and lattice modes. The Raman spectrum shows intense peaks at 801, 710, 262 and 61 cm(-1) that are typical Raman peaks of crystalline WO3 (m-phase) that correspond to stretching vibrations of the bridging oxygen, which are assigned to W-O stretching (nu) and W-O bending (delta) modes, respectively. By transmittance measurements obtains that the WO3 band gap can be varied from 2.92 to 3.13 eV in the investigated annealing temperature range. (c) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:182 / 186
页数:5
相关论文
共 50 条
  • [1] Structural properties of WO3 dependent of the annealing temperature deposited by hot-filament metal oxide deposition
    Flores-Mena, J. E.
    Diaz-Reyes, J.
    Balderas-Lopez, J. A.
    REVISTA MEXICANA DE FISICA, 2012, 58 (06) : 504 - 509
  • [2] Developments in hot-filament metal oxide deposition (HFMOD)
    Durrant, Steven F.
    Trasferetti, Benedito C.
    Scanninio, Jair
    Davanzo, Celso U.
    Rouxinol, Francisco P. M.
    Gelamo, Rogerio V.
    de Moraes, Mario A. Bica
    THIN SOLID FILMS, 2008, 516 (05) : 789 - 793
  • [3] Characterization of Nanoporous WO3 Films Grown via Ballistic Deposition
    Smid, Bretislav
    Li, Zhenjun
    Dohnalkova, Alice
    Arey, Bruce W.
    Smith, R. Scott
    Matolin, Vladimir
    Kay, Bruce D.
    Dohnalek, Zdenek
    JOURNAL OF PHYSICAL CHEMISTRY C, 2012, 116 (19) : 10649 - 10655
  • [4] Hot-filament metal oxide deposition (HFMOD): A novel method for depositing thin films of metallic oxides
    Rouxinol, FP
    Trasferetti, BC
    Landers, R
    de Moraes, MAB
    JOURNAL OF THE BRAZILIAN CHEMICAL SOCIETY, 2004, 15 (02) : 324 - 326
  • [5] Impact of Methanol Concentration on Properties of Ultra-Nanocrystalline Diamond Films Grown by Hot-Filament Chemical Vapour Deposition
    Mosinska, Lidia
    Szczesny, Robert
    Trzcinski, Marek
    Naparty, Mieczyslaw Karol
    MATERIALS, 2022, 15 (01)
  • [6] Effect of surface treatment on hot-filament chemical vapour deposition grown diamond films
    Ali, M.
    Urgen, M.
    Atta, M. A.
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2012, 45 (04)
  • [7] Controlled Growth of WO3 Pyramidal Thin Film via Hot-Filament Chemical Vapor Deposition: Electrochemical Detection of Ethylenediamine
    Imran, Mohammad
    Kim, Eun-Bi
    Kwak, Dong-Heui
    Akhtar, Mohammad Shaheer
    Ameen, Sadia
    CHEMOSENSORS, 2021, 9 (09)
  • [8] Effect of deposition pressure on the properties of amorphous carbon films by hot-filament chemical vapor deposition
    Zhai, Zihao
    Shen, Honglie
    Chen, Jieyi
    Li, Xuemei
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2019, 30 (11) : 10145 - 10151
  • [9] Tantalum carbide films synthesized by hot-filament chemical vapor deposition technique
    Ali, M.
    Urgen, M.
    Atta, M. A.
    SURFACE & COATINGS TECHNOLOGY, 2012, 206 (11-12) : 2833 - 2838
  • [10] Annealing effects on the structural and optical properties of vanadium oxide film obtained by the hot-filament metal oxide deposition technique (HFMOD)
    Scarminio, Jair
    Catarini da Silva, Paulo Rogerio
    Gelamo, Rogerio Valentim
    Bica de Moraes, Mario Antonio
    MATERIA-RIO DE JANEIRO, 2017, 22 (01):