Dynamic failure of titanium: Temperature rise and adiabatic shear band formation

被引:71
作者
Guo, Yazhou [1 ,3 ,4 ]
Ruan, Qichao [1 ,3 ,4 ]
Zhu, Shengxin [2 ]
Wei, Q. [1 ,5 ]
Lu, Jianan [1 ,3 ,4 ]
Hu, Bo [1 ,3 ,4 ]
Wu, Xihui [1 ,3 ,4 ]
Li, Yulong [1 ,3 ,4 ]
机构
[1] Northwestern Polytech Univ, Sch Aeronaut, Xian 710072, Peoples R China
[2] Beijing Inst Technol, Inst Adv Struct Technol, Beijing 100081, Peoples R China
[3] Northwestern Polytech Univ, Shaanxi Key Lab Impact Dynam & Engn Applicat, Xian 710072, Peoples R China
[4] Northwestern Polytech Univ, Joint Int Res Lab Impact Dynam & Engn Applicat, Xian 710072, Peoples R China
[5] Univ N Carolina, Dept Mech Engn, Charlotte, NC 28223 USA
基金
中国国家自然科学基金;
关键词
Adiabatic shear; ASB; Titanium; Temperature; High speed photography; Shear compression; HIGH-STRAIN; MICROSTRUCTURAL EVOLUTION; MECHANICAL-BEHAVIOR; LOCALIZATION; DEFORMATION; RECRYSTALLIZATION; PROPAGATION; ALLOY; RANGE; WORK;
D O I
10.1016/j.jmps.2019.103811
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
One of the most important issues related to dynamic shear localization is the correlation among the stress collapse, temperature elevation and adiabatic shear band (ASB) formation. In this work, the adiabatic shear failure process of pure titanium was investigated by dynamic shear-compression tests synchronically combined with high-speed photography and infrared temperature measurement. The time sequence of important events such as stress collapse, ASB initiation, temperature rise and crack formation was recorded. The key characteristics of ASB, such as width, critical strain, temperature, propagation speed and cooling rate were systematically studied. The maximum propagation velocity of ASB is found in this work to be about 1900 m/s, about 0.6Cs (Cs is the shear wave speed). The maximum temperature within ASB is in the range of 350-650 degrees C, while the material close to ASB is also heated. The cooling rate of ASB is on the order of 106 degrees C/s, indicating that it needs a few hundreds of microseconds for the ASB to cool down to the ambient temperature. One important observation is that the apparent temperature rise occurs after ASB initiation, which indicates that it might not be the causation but the consequences of ASB. Further efforts are called for confirmation of this notion because of its significance. (C) 2019 Elsevier Ltd. All rights reserved.
引用
收藏
页数:23
相关论文
共 67 条
  • [41] A shear-compression specimen for large strain testing
    D. Rittel
    S. Lee
    G. Ravichandran
    [J]. Experimental Mechanics, 2002, 42 (1) : 58 - 64
  • [42] Dynamic Recrystallization as a Potential Cause for Adiabatic Shear Failure
    Rittel, D.
    Landau, P.
    Venkert, A.
    [J]. PHYSICAL REVIEW LETTERS, 2008, 101 (16)
  • [43] Dynamic recrystallization and adiabatic shear localization
    Rodriguez-Martinez, J. A.
    Vadillo, G.
    Rittel, D.
    Zaera, R.
    Fernandez-Saez, J.
    [J]. MECHANICS OF MATERIALS, 2015, 81 : 41 - 55
  • [44] A comparative study on the microstructure and mechanical behavior of titanium: Ultrafine grain vs. coarse grain
    Sun, Xiangyu
    Guo, Yazhou
    Wei, Qiuming
    Li, Yulong
    Zhang, Shuangyin
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 669 : 226 - 245
  • [45] The plastic distortion of metals
    Taylor, GI
    Quinney, H
    [J]. PHILOSOPHICAL TRANSACTIONS OF THE ROYAL SOCIETY OF LONDON SERIES A-CONTAINING PAPERS OF A MATHEMATICAL OR PHYSICAL CHARACTER, 1932, 230 : 323 - 362
  • [46] The latent energy remaining in a metal after cold working.
    Taylor, GI
    Quinney, H
    [J]. PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-CONTAINING PAPERS OF A MATHEMATICAL AND PHYSICAL CHARACTER, 1934, 143 (A849) : 0307 - 0326
  • [47] THE STRUCTURE OF ADIABATIC SHEAR BANDS IN A TITANIUM-ALLOY
    TIMOTHY, SP
    HUTCHINGS, IM
    [J]. ACTA METALLURGICA, 1985, 33 (04): : 667 - 676
  • [48] Shear localization: A historical overview
    Walley, S. M.
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2007, 38A (11): : 2629 - 2654
  • [49] NUMERICAL EXPERIMENTS ON ADIABATIC SHEAR BAND FORMATION IN ONE DIMENSION
    WALTER, JW
    [J]. INTERNATIONAL JOURNAL OF PLASTICITY, 1992, 8 (06) : 657 - 693
  • [50] Microstructure and mechanical properties of tantalum after equal channel angular extrusion (ECAE)
    Wei, Q
    Jiao, T
    Mathaudhu, SN
    Ma, E
    Hartwig, KT
    Ramesh, KT
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 358 (1-2): : 266 - 272