Research on Binderless Tungsten Carbide Prepared by Spark Plasma Sintering

被引:7
|
作者
Li, Xiaoqiang [1 ]
Xiao, Zhangyi [1 ]
Yang, Chao [1 ]
Qu, Shengguan [1 ]
机构
[1] S China Univ Technol, Sch Mech & Automot Engn, Guangzhou 510640, Guangdong, Peoples R China
来源
ADVANCES IN ENGINEERING DESIGN AND OPTIMIZATION, PTS 1 AND 2 | 2011年 / 37-38卷
关键词
Pure WC powders; Particle size; Spark plasma sintering; GROWTH;
D O I
10.4028/www.scientific.net/AMM.37-38.980
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Commerical pure WC powders of 0.2, 0.4, 0.8, 2.0 and 3.0 mu m in diameter were sintered by spark plasma sintering process at 1300 degrees C, respectively. By analyzing the XRD patterns of the initial powders and the microstructure of the sintered samples, it is affirmed that the powders with an average size of 0.8 pm exhibits the best activity and sintering property. To optimize sintering temperature, the sintering of 0.8 mu m powders was carried out at 1200-1700 degrees C. The specimen sintered at 1300 degrees C has a density of 15.49 g/cm(3) and an average grain size of about 0.7 mu m, and exhibits the most excellent mechanical properties. The corresponding Vickers hardness and transverse rupture strength are 2469 HV and 1656 MPa, respectively.
引用
收藏
页码:980 / 984
页数:5
相关论文
共 50 条
  • [21] Spark-Plasma-Sintering (SPS) of tungsten carbide and titanium carbonitride nanopowders
    Zalite, I.
    Angerer, P.
    Yu, L. G.
    Khor, K. A.
    ANNUAL CONFERENCE ON FUNCTIONAL MATERIALS AND NANOTECHNOLOGIES - FM&NT 2011, 2011, 23
  • [22] Adhesive wear performance of self-lubricating functionally graded cemented tungsten carbide prepared by spark plasma sintering
    Parihar, Rityuj Singh
    Sahu, Raj Kumar
    Setti, Srinivasu Gangi
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2022, 104
  • [23] Spark plasma sintering of tantalum carbide
    Khaleghi, Evan
    Lin, Yen-Shan
    Meyers, Marc A.
    Olevsky, Eugene A.
    SCRIPTA MATERIALIA, 2010, 63 (06) : 577 - 580
  • [24] Spark plasma sintering of tungsten carbide nanopowders obtained through DC arc plasma synthesis
    Chuvil'deev, V. N.
    Blagoveshchenskiy, Yu. V.
    Nokhrin, A. V.
    Boldin, M. S.
    Sakharov, N. V.
    Isaeva, N. V.
    Shotin, S. V.
    Belkin, O. A.
    Popov, A. A.
    Smirnova, E. S.
    Lantsev, E. A.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 708 : 547 - 561
  • [25] MECHANICAL PROPERTY OF BORON CARBIDE CERAMICS PREPARED BY SPARK PLASMA REACTIVE SINTERING
    Zhang, S.
    Wang, C. B.
    Chen, G.
    Shen, Q.
    Zhang, L. M.
    PROCESSING AND PROPERTIES OF ADVANCED CERAMICS AND COMPOSITES II, 2010, 220 : 197 - 203
  • [26] Graphite nanoplatelets toughened zirconium carbide ceramics prepared by spark plasma sintering
    Wei, Xiao-Feng
    Song, Jia-Xin
    Liu, Ji-Xuan
    Qin, Yuan
    Li, Fei
    Liang, Yongcheng
    Zhang, Guo-Jun
    CERAMICS INTERNATIONAL, 2021, 47 (06) : 8461 - 8467
  • [27] SPARK PLASMA SINTERING OF NANOCRYSTALLINE BINDERLESS WC HARD METALS
    Dopita, Milan
    Sriram, Chidambaram Rajagopalan
    Chmelik, David
    Salomon, Anton
    Seifert, Hans Juergen
    NANOCON 2010, 2ND INTERNATIONAL CONFERENCE, 2010, : 133 - 139
  • [28] Material properties of tungsten carbide-alumina composites fabricated by spark plasma sintering
    Chen, Wei-Hsio
    Lin, Hao-Tung
    Nayak, Pramoda K.
    Huang, Jow-Lay
    CERAMICS INTERNATIONAL, 2014, 40 (09) : 15007 - 15012
  • [29] Spark Plasma Sintering of high-strength ultrafine-grained tungsten carbide
    Nokhrin, A. V.
    Chuvil'deev, V. N.
    Blagoveshchenskiy, Yu V.
    Boldin, M. S.
    Sakharov, N. V.
    Isaeva, N. V.
    Popov, A. A.
    Lantcev, E. A.
    Belkin, O. A.
    Smirnova, E. S.
    5TH INTERNATIONAL SCIENTIFIC WORKSHOP ON ADVANCED TECHNOLOGIES OF MATERIALS FIELD-ASSISTED CONSOLIDATION, 2017, 218
  • [30] Initial stage sintering of binderless tungsten carbide powder under microwave radiation
    Demirskyi, Dmytro
    Ragulya, Andrey
    Agrawal, Dinesh
    CERAMICS INTERNATIONAL, 2011, 37 (02) : 505 - 512