Effect of heat treatment on microstructure and properties of semi-solid squeeze casting AZ91D

被引:14
|
作者
You, Zhi-yong [1 ]
Jiang, Ao-xue [1 ]
Duan, Zhuang-zheng [1 ]
Qiao, Gang-ping [1 ]
Gao, Jing-lei [2 ]
Guo, Ling-bing [2 ]
机构
[1] Taiyuan Univ Technol, Coll Mat Sci & Engn, Taiyuan 030024, Peoples R China
[2] Shanxi Huaxiang Grp Co Ltd, Linfen 011600, Shanxi, Peoples R China
关键词
AZ91D; semi-solid squeeze casting; solution aging treatment; microstructure; mechanical properties; TG146; 22; A; MECHANICAL-PROPERTIES; HOT EXTRUSION; COMPOSITE; EVOLUTION; BEHAVIOR; SICP;
D O I
10.1007/s41230-020-9103-9
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Semi-solid AZ91D magnesium alloy billets were prepared by near-liquidus heat holding. Semi-solid squeeze casting was conducted at 575, 585 and 595 degrees C, respectively, with 1 mm center dot s(-1)squeeze speed. The semisolid squeeze casting AZ91D samples were heat treated by T4 (solution at 415 degrees C for 24 h) and T6 (solution at 415 degrees C for 24 h + 220 degrees C for 8 h) processes, respectively. The microstructure and mechanical properties of the alloy in different states were investigated by means of OM, SEM and tensile testing machine. The results show that compared to as-cast alloy, the grain size of the semi-solid squeezed AZ91D decreased significantly, and with the increase of semi-solid squeeze temperature, the grain size of AZ91D increased. The grains of the alloy were refined by T4 treatment, and further refined by T6 treatment. T6 treatment greatly improved the tensile strength, elongation, and hardness, but did not significantly improve yield strength. After 575 degrees C squeeze casting and T6 treatment, the ultimate tensile strength (UTS) reached 285 MPa, the elongation reached 13.36%, and the hardness also reached the maximum (106.8 HV), but the yield strength (YS) was only 180 MPa. During the process of semi-solid squeeze casting and heat treatment, the matrix grain was refined and a large number of precipitated and secondary precipitated phases of Mg(17)Al(12)appeared. Both the average size of matrix grain and secondary precipitated phase decreased, while the volume fraction of secondary precipitated phase increased. All these resulted in high tensile strength, elongation and hardness.
引用
收藏
页码:219 / 226
页数:8
相关论文
共 50 条
  • [21] Microstructure and Mechanical Properties of the AlCrFeCoNip/AZ91D Composites After Heat Treatment
    Chen, Yongsheng
    Sun, Xiaomei
    Zhang, Xiaochen
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2024, 77 (06) : 1537 - 1544
  • [22] Cyclic deformation and twinning in a semi-solid processed AZ91D magnesium alloy
    Patel, H. A.
    Chen, D. L.
    Bhole, S. D.
    Sadayappan, K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 528 (01): : 208 - 219
  • [23] Reheating microstructure of refined AZ91D magnesium alloy in semi-solid state
    Jiang, JF
    Luo, SJ
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2004, 14 (06) : 1074 - 1081
  • [24] Effect of Ca, RE elements and semi-solid processing on the microstructure and creep properties of AZ91 alloy
    Nami, B.
    Shabestari, S. G.
    Razavi, H.
    Mirdamadi, Sh.
    Miresmaeili, S. M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (03): : 1261 - 1267
  • [25] Effect of selective laser melting on microstructure and properties of AZ91D alloy
    Zhu, Z.
    Zhang, M.
    Chen, C.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2019, 50 (12) : 1484 - 1494
  • [26] Microstructure evolution and mechanical properties of rheo-squeeze casting AZ91-Ca alloy during heat treatment
    Zhang, Yang
    Li, Xiao-ping
    Sun, Shun-ping
    Lu, Ya-lin
    Wu, Guo-hua
    CHINA FOUNDRY, 2017, 14 (06) : 485 - 491
  • [27] Microstructure evolution and mechanical properties of rheo-squeeze casting AZ91-Ca alloy during heat treatment
    Yang Zhang
    Xiao-ping Li
    Shun-ping Sun
    Ya-lin Lu
    Guo-hua Wu
    China Foundry, 2017, 14 : 485 - 491
  • [28] Low cycle fatigue properties of friction stir welded joints of a semi-solid processed AZ91D magnesium alloy
    Ni, D. R.
    Chen, D. L.
    Yang, J.
    Ma, Z. Y.
    MATERIALS & DESIGN, 2014, 56 : 1 - 8
  • [29] Effect of Heat Treatment on the Microstructure and Mechanical Properties of the Friction Stir Processed AZ91D Magnesium Alloy
    Govindaraju, M.
    Vignesh, R. Vaira
    Padmanaban, R.
    METAL SCIENCE AND HEAT TREATMENT, 2019, 61 (5-6) : 311 - 317