A new model for multilayer ceramic composites

被引:7
作者
Dey, A. [2 ]
Dey, P. [1 ]
Datta, S. [1 ]
Mukhopadhyay, A. K. [2 ]
机构
[1] Bengal Engn & Sci Univ, Sch Mat Sci & Engn, Sibpur 711103, Howrah, India
[2] Cent Glass & Ceram Res Inst, Analyt Facil Div, Mech Test Sect, Kolkata, India
关键词
alumina; ceramics; composite; controlled; crack; delamination; energy; fracture; interface; lanthanum phosphate; Modeling; multilayer; toughness; weak;
D O I
10.1080/10426910802104278
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An attempt was made in the present work, to develop a model for design of multilayer ceramic composites (MLC) with high failure energy. The model considered the failure process of a notched MLC beam comprised of N number of matrix layers of thickness t(m) each, separated by (N-1) very thin interfacial layer of thickness t(i) (<< t(m)) and loaded in a three-point bend configuration. The model was developed on the basis of changes in compliance and stored elastic energy of the MLC beam as a function of crack growth process. Finally, the amount of energy consumed per unit volume, E-con MLC, during controlled propagation of interfacial cracks in the MLC beam was evaluated by the proposed model. The main advantage of the controlled interfacial crack growth process was that the amount of energy consumed per unit volume by the MLC could also enhance substantially with the number of failed matrix layers. The predictions of the model were made for a strong matrix/weak interface design of MLC system. The optimally designed MLC beam was comprised of 20 numbers of 150 mu m alumina matrix layers separated by 19 numbers of very thin (7 mu m) lanthanum phosphate interfaces. For the purpose of verification, it was put under a three-point bend configuration with a loading span of 38mm. The predictions compared favorably with experimental data from literature as well as our own work. Further, it was found out that in the present alumina/lanthanum phosphate/alumina MLC system, the predicted failure energy (57.9KJm(-3)), improved by a factor of 8.68times over that (6.67KJm(-3)) of the matrix alumina layer phase. This enhancement in failure energy suggested the achievement of significant toughening in the proposed new design of the chosen MLC system. Finally, the influence of key design parameters like the total number of layers, layer thickness, etc., and of inherent material properties like failure stress of matrix, strain energy release rate of interface, etc. on the mechanical behavior of the proposed alumina/lanthanum phosphate/alumina MLC design were also discussed.
引用
收藏
页码:513 / 527
页数:15
相关论文
共 46 条
[11]   Tape cast multilayer composite of nano zirconia with high toughness [J].
Ghosh, S. ;
Guha, A. ;
Krishna, K. M. ;
Mukhopadhyay, A. K. ;
Maiti, H. S. .
MATERIALS AND MANUFACTURING PROCESSES, 2006, 21 (07) :662-668
[12]  
Ghosh S., 2005, T INDIAN CERAM SOC, V64, P101, DOI [10.1080/0371750X.2005.11012195, DOI 10.1080/0371750X.2005.11012195]
[13]   CALCULATION, MEASUREMENT, AND CONTROL OF INTERFACE STRENGTH IN COMPOSITES [J].
GUPTA, V ;
YUAN, J ;
MARTINEZ, D .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1993, 76 (02) :305-315
[14]   CRACK DEFLECTION AT AN INTERFACE BETWEEN DISSIMILAR ELASTIC-MATERIALS - ROLE OF RESIDUAL-STRESSES [J].
HE, MY ;
EVANS, AG ;
HUTCHINSON, JW .
INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 1994, 31 (24) :3443-3455
[15]   CRACK DEFLECTION AT AN INTERFACE BETWEEN DISSIMILAR ELASTIC-MATERIALS [J].
HE, MY ;
HUTCHINSON, JW .
INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 1989, 25 (09) :1053-1067
[16]   Oxidation of MoSi2/SiC nanolayered composite [J].
Hirvonen, JP ;
Torri, P ;
Lappalainen, R ;
Likonen, J ;
Kung, H ;
Jervis, JR ;
Nastasi, M .
JOURNAL OF MATERIALS RESEARCH, 1998, 13 (04) :965-973
[17]   Hertzian contact fatigue on alumina/alumina-zirconia laminated composites [J].
Jiménez-Piqué, E ;
Ceseracciu, L ;
Chalvet, F ;
Anglada, M ;
de Portu, G .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2005, 25 (15) :3393-3401
[18]   TRANSITION BETWEEN COHESIVE AND INTERFACIAL FAILURE IN A LAMINATE [J].
KENDALL, K .
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL PHYSICAL AND ENGINEERING SCIENCES, 1975, 344 (1637) :287-302
[19]   A high-strain-rate superplastic ceramic [J].
Kim, BN ;
Hiraga, K ;
Morita, K ;
Sakka, Y .
NATURE, 2001, 413 (6853) :288-291
[20]   Mullite-aluminum phosphate laminated composite fabricated by tape casting [J].
Kim, DK ;
Kriven, WM .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2003, 86 (11) :1962-1964