Long-term thermal aging of parylene conformal coating under high humidity and its effects on tin whisker mitigation

被引:7
|
作者
Sivakumar, Preeth [1 ]
Du, Surbhi Mahajan [2 ]
Selter, Matt [2 ]
Ballard, Imani [2 ]
Daye, John [2 ]
Cho, Junghyun [1 ,3 ]
机构
[1] SUNY Binghamton, Dept Mech Engn, Binghamton, NY 13902 USA
[2] Kansas City Natl Secur Campus, Honeywell FM&T, Kansas City, MO 64147 USA
[3] SUNY Binghamton, Mat Sci & Engn Program, Binghamton, NY 13902 USA
关键词
Parylene; Tin whiskers; Coating degradation; Adhesion; High-temperature; High-humidity; Aging; GAMMA-METHACRYLOXYPROPYLTRIMETHOXYSILANE; SPONTANEOUS GROWTH; RESIDUAL-STRESS; ADHESION; DEGRADATION; MECHANISM; SURFACES; FILMS; TIME;
D O I
10.1016/j.polymdegradstab.2021.109667
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Usage of pure tin (Sn) or Sn-rich alloy in electronics industry is growing, which makes them more susceptible to the spontaneous growth of tin whiskers. The risk of having these whiskers can be dramatically mitigated by applying a conformal coating such as parylene C. The purpose of this paper is to investigate the degradation of parylene C coating (with two thicknesses, 12.5 mu m and 25 mu m) during thermal aging in high humidity environment (85 degrees C/85% relative humidity for up to 5000 h) and its effect on the tin whisker mitigation property. It was observed that under the high temperature and high humidity (HTHH) environment, the oxidation occurs at early times, followed by bond scission, resulting in the loss in strength and modulus of the parylene coating. After 2500 h of aging, due to the degradation of the silane agent at the tin/parylene interface, the adhesion of the parylene coating on the tin surface was significantly weakened, which resulted in extensive corrosion of the tin solderpads. The loss of adhesion of the coating, along with the corrosion of the tin surface facilitated tin whisker nucleation at the interface while the loss of mechanical strength and the brittleness made the growing whiskers penetrate easily through the coating. Tin whiskers with a smaller diameter were buckled and grew along the delaminated interfacial region while those with a larger diameter penetrated and continued to grow through the coating. Although the thicker parylene coating helped delay the complete penetration and increase the critical diameter of whiskers for complete penetration, it showed more tin whisker activities and easy penetration by large diameter whiskers due to poorer adhesion. Hence, the effectiveness of the parylene coating on tin whisker mitigation will depend on its degradation kinetics of mechanical properties and adhesion under such harsh conditions. (C) 2021 Elsevier Ltd. All rights reserved.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Discoloration Effects of High-Dose γ-Irradiation and Long-Term Thermal Aging of (U) HMW-PE
    Koemmling, Anja
    Chatzigiannakis, Emmanouil
    Beckmann, Joerg
    Wachtendorf, Volker
    von der Ehe, Kerstin
    Braun, Ulrike
    Jaunich, Matthias
    Schade, Ulrich
    Wolff, Dietmar
    INTERNATIONAL JOURNAL OF POLYMER SCIENCE, 2017, 2017
  • [2] Influence of Relative Humidity on the Mechanical Properties of Palm Leaf Manuscripts: Short-Term Effects and Long-Term Aging
    Zhang, Wenjie
    Wang, Shan
    Guo, Hong
    MOLECULES, 2024, 29 (23):
  • [3] Predicting viscoelastic behavior and crack propagation in EPDM rubber under long-term thermal aging
    Hou, Nan
    Guo, Qiang
    Zairi, Fahmi
    Tian, Linan
    Ding, Ning
    ENGINEERING FRACTURE MECHANICS, 2025, 315
  • [4] Evaluation of Long-term Durability of Thermal Insulation Paint under Aging Conditions in Railway Sites
    Park, Juyeop
    Kang, Donghoon
    JOURNAL OF THE KOREAN SOCIETY FOR NONDESTRUCTIVE TESTING, 2022, 42 (01) : 43 - 50
  • [5] Long-term thermal stability of NPB molecule under high-vacuum
    Shim, Seob
    Kim, Hayeong
    Choi, Eunmi
    An, Jong-Ki
    Kang, Goru
    Kwon, Ohyun
    Chung, Nak-Kwan
    Kim, Jin-Tae
    Yun, Ju-Young
    ORGANIC ELECTRONICS, 2020, 77
  • [6] A promising hydroxyapatite whisker with long-term and high-efficiency antibacterial performance and its potential application in implant
    Jiang, Zhimin
    Gong, Zhiqiang
    Song, Wei
    Wu, Peiyao
    Deng, Chaodong
    Chen, Qinghua
    Yan, Tingting
    INORGANIC CHEMISTRY COMMUNICATIONS, 2022, 146
  • [7] Effects of interfacial microstructure on mechanical properties of Stellite-hardfaced coating during long-term aging
    Wu, Yuxiao
    Schmitt, Thomas
    Bousser, Etienne
    Khelfaoui, Fadila
    Najarian, Vahe
    Klemberg-Sapieha, Jolanta-Ewa
    Brochu, Myriam
    SURFACE & COATINGS TECHNOLOGY, 2020, 398
  • [8] Superior Long-Term Performance of Composite Phase Change Material with High-Density Polyethylene under Thermal Aging Process
    Suyitno, Budhi Muliawan
    Rahmalina, Dwi
    Ismail, Ismail
    Rahman, Reza Abdu
    REVUE DES COMPOSITES ET DES MATERIAUX AVANCES-JOURNAL OF COMPOSITE AND ADVANCED MATERIALS, 2023, 33 (03): : 145 - 151
  • [9] Characterization and gas sensing properties of graphene/polyaniline nanocomposite with long-term stability under high humidity
    Karouei, Seyedeh Faezeh Hashemi
    Moghaddam, Hossain Milani
    Niavol, Someyeh Saadat
    JOURNAL OF MATERIALS SCIENCE, 2021, 56 (06) : 4239 - 4253
  • [10] Characterization and gas sensing properties of graphene/polyaniline nanocomposite with long-term stability under high humidity
    Seyedeh Faezeh Hashemi Karouei
    Hossain Milani Moghaddam
    Someyeh Saadat Niavol
    Journal of Materials Science, 2021, 56 : 4239 - 4253