Mechanical stability of resin-dentin bond components

被引:102
作者
Carrilho, MRD
Tay, FR
Pashley, DH
Tjäderhane, L
Carvalho, RM
机构
[1] Univ Sao Paulo, Fac Odontol, Dept Operat Dent Endodont & Dent Mat, Bauru Sch Dent, BR-17012901 Bauru, SP, Brazil
[2] Univ Helsinki, Cent Hosp, Dept Oral & Maxillofacial Dis, Helsinki, Finland
[3] Univ Helsinki, Inst Dent, Helsinki, Finland
[4] Med Coll Georgia, Sch Dent, Dept Oral Biol & Maxillofacial Pathol, Augusta, GA 30912 USA
[5] Prince Philip Dent Hosp, Sch Dent, Dept Conservat Dent, Hong Kong, Hong Kong, Peoples R China
[6] Univ Estadual Campinas, Dept Restorat Dent, Piracicaba Sch Dent, Piracicaba, SP, Brazil
基金
巴西圣保罗研究基金会;
关键词
resin composite; adhesives; collagen fibrils; dentin; mechanical properties; durability;
D O I
10.1016/j.dental.2004.06.001
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: To evaluate the effects of long-term storage on the mechanical properties of the components of resin-dentin bonds, that is, resin composite, adhesive system, demineralized and mineralized dentin. Methods: Specimens of resin composite (Z250) and adhesive systems (Single Bond-SB; One-Step-OS and Clearfil Liner Bond 2V-CL) were cast in molds. Dentin specimens were prepared from dentin discs obtained from the crowns of extracted human molars. Specimens of demineralized dentin were obtained by immersion of dentin discs for 6 days in 0.5 mol/l EDTA (pH 7.0). Both dentin and resin-based substrates were shaped to hourglass or I-beam specimens that were used to determine the true stress (TS) or apparent modulus of elasticity (E), respectively. Control specimens were subjected to tensile testing at 0.6 mm/min after 24 h of immersion in distilled water. Experimental specimens were stored at 37 degreesC in either distilled water or mineral oil and tested after 12 months. The data of each group were individually analyzed by ANOVA and Tukey's test. Results: Both TS and E of the resin-based materials decreased significantly after 12 months of storage in water (p < 0.05), except the TS of SB (p > 0.05). No changes were observed for specimens of mineralized dentin, regardless of storage condition (p > 0.05). Storage of demineralized dentin in water did not cause any significant effect in either TS or E (p > 0.05), however, significant reductions of TS and E of demineralized dentin occurred after storage in oil for 1 year (p < 0.05). Significance: Storage time and medium may be deleterious to the mechanical properties of the resin-dentin bond components, which ultimately could compromise the durability of resin-dentin bonds. (C) 2004 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:232 / 241
页数:10
相关论文
共 54 条
[2]   The influence of water storage and C-factor on the dentin-resin composite microtensile bond strength and debond pathway utilizing a filled and unfilled adhesive resin [J].
Armstrong, SR ;
Keller, JC ;
Boyer, DB .
DENTAL MATERIALS, 2001, 17 (03) :268-276
[3]   EFFECT OF CROSS-LINKING AGENT CONTENT, MONOMER FUNCTIONALITY, AND REPEAT UNIT CHEMISTRY ON PROPERTIES OF UNFILLED RESINS [J].
BEATTY, MW ;
SWARTZ, ML ;
MOORE, BK ;
PHILLIPS, RW ;
ROBERTS, TA .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1993, 27 (03) :403-413
[4]   TENSILE STRENGTH AND MODULUS OF ELASTICITY OF TOOTH STRUCTURE AND SEVERAL RESTORATIVE MATERIALS [J].
BOWEN, RL ;
RODRIGUEZ, MS .
JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 1962, 64 (03) :378-&
[6]   Dentin bond durability after three years using a dentin bonding agent with and without priming [J].
Burrow, MF ;
Satoh, M ;
Tagami, J .
DENTAL MATERIALS, 1996, 12 (5-6) :302-307
[7]  
Carrilho MRO, 2004, AM J DENT, V17, P104
[8]  
Carvalho R M, 2001, J Adhes Dent, V3, P309
[9]  
Carvalho R M, 2000, J Adhes Dent, V2, P193
[10]   In vitro study on the dimensional changes of human dentine after demineralization [J].
Carvalho, RM ;
Yoshiyama, M ;
Pashley, EL ;
Pashley, DH .
ARCHIVES OF ORAL BIOLOGY, 1996, 41 (04) :369-377