Failure assessment diagram analysis of creep crack initiation in 316H stainless steel

被引:35
作者
Davies, CM
O'Dowd, NP
Dean, DW
Nikbin, KM
Ainsworth, RA
机构
[1] Univ London Imperial Coll Sci Technol & Med, Dept Mech Engn, London SW7 2AZ, England
[2] British Energy Plc, Gloucester GL4 3RS, England
关键词
failure assessment diagram; creep crack initiation; stainless steel;
D O I
10.1016/S0308-0161(03)00107-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work the time dependent failure assessment diagram (TDFAD) approach is applied to the study of crack initiation in Type 316H stainless steel, a material commonly used in high temperature applications. A TDFAD has been constructed for the steel at a temperature of 550 degreesC, and was found to be relatively insensitive to time. The TDFAD procedure is then applied to predict initiation times, at increments of creep crack growth Deltaa = 0.2 and 0.5 mm, for tests on compact tension specimens and the results compared to experimentally determined values. It has been found that initiation time predictions are sensitive to the creep toughness values, and to the limit load (or reference stress) solution used. Conservative predictions of initiation times have been achieved through the use of the lower bound creep toughness values in conjunction with the plane strain limit load solution. The plane stress limit load solution has given conservative predictions for all bounds of creep toughness used. (C) 2003 Elsevier Ltd. All rights reserved.
引用
收藏
页码:541 / 551
页数:11
相关论文
共 15 条
[1]  
*AFCEN RCC MR, 1995, DES CONSTR RUL MECH
[2]   Failure assessment diagrams for high temperature defect assessment [J].
Ainsworth, RA ;
Hooton, DG ;
Green, D .
ENGINEERING FRACTURE MECHANICS, 1999, 62 (01) :95-109
[3]  
[Anonymous], 2010, Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials, P1
[4]  
[Anonymous], 2001, R6 ASS INT STRUCT CO
[5]  
*ASME, 1990, CAS ASME BOIL PRESS
[6]  
BETTINSON AD, 2002, THESIS IMPERIAL COLL
[7]  
BETTINSON AD, 2002, ASME PVP, V434, P143
[8]  
Dean DW, 2001, CREEP AND FRACTURE OF ENGINEERING MATERIALS AND STRUCTURES, P751
[9]   Development and use of the R5 procedures for the assessment of defects in high temperature plant [J].
Dean, DW ;
Ainsworth, RA ;
Booth, SE .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2001, 78 (11-12) :963-976
[10]  
DEAN DW, 2001, CREEP FATIGUE ELEVAT, P315