Influence of Zn concentration on stretch formability at room temperature of Mg-Zn-Ce alloy

被引:120
作者
Chino, Yasumasa [1 ]
Huang, Xinsheng [1 ]
Suzuki, Kazutaka [1 ]
Sassa, Kensuke [1 ]
Mabuchi, Mamoru [2 ]
机构
[1] Natl Inst Adv Ind Sci & Technol, Mat Res Inst Sustainable Dev, Moriyama Ku, Nagoya, Aichi 4638560, Japan
[2] Kyoto Univ, Dept Energy Sci & Technol, Grad Sch Energy Sci, Sakyo Ku, Kyoto 6068501, Japan
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2010年 / 528卷 / 02期
关键词
Magnesium alloys; Sheet forming; Rolling; Texture; Solid solution hardening; Solid solution softening; MAGNESIUM SINGLE-CRYSTALS; DEFORMATION-BEHAVIOR; TEXTURE; SHEETS; ENHANCEMENT; DUCTILITY; STRENGTH; CERIUM;
D O I
10.1016/j.msea.2010.09.081
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The relationship between the Zn concentration and stretch formability of the rolled Mg-xwt.%Zn-0.2wt.%Ce (Mg-xZn-0.2Ce here after) alloys was investigated. Zn addition of a dilute concentration of more than 0.5 wt.% effectively modified the basal plane texture, which was characterized by the splitting basal pole toward the TD. However, further Zn addition showed no strong effect on the distribution and intensity of the basal plane texture. The Mg-1.5Zn-0.2Ce alloy showed significant stretch formability. On the other hand, further Zn addition deteriorated the stretch formability of the Mg-xZn-0.2Ce alloys, although it showed no effect on the distribution and intensity of the basal plane texture. The deterioration of the stretch formability of the Mg-xZn-0.2Ce alloys with high Zn concentrations was suggested to be ascribed to solid solution hardening. Moreover, it was suggested that not only the texture but also solid solution softening plays an important role in the enhanced stretch formability of the Mg-xZn-0.2Ce alloys. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:566 / 572
页数:7
相关论文
共 39 条
[1]  
AKHTAR A, 1968, T JPN I MET, VS 9, P692
[2]   SOLID SOLUTION STRENGTHENING OF MAGNESIUM SINGLE CRYSTALS .I. ALLOYING BEHAVIOUR IN BASAL SLIP [J].
AKHTAR, A ;
TEGHTSOONIAN, E .
ACTA METALLURGICA, 1969, 17 (11) :1339-+
[3]   SOLID SOLUTION STRENGTHENING OF MAGNESIUM SINGLE CRYSTALS .2. EFFECT OF SOLUTE ON EASE OF PRISMATIC SLIP [J].
AKHTAR, A ;
TEGHTSOONIAN, E .
ACTA METALLURGICA, 1969, 17 (11) :1351-+
[4]   TENSILE-COMPRESSIVE YIELD ASYMMETRIES IN HIGH-STRENGTH WROUGHT MAGNESIUM ALLOYS [J].
BALL, EA ;
PRANGNELL, PB .
SCRIPTA METALLURGICA ET MATERIALIA, 1994, 31 (02) :111-116
[5]   Solid-solution hardening and softening in Mg-Zn alloys [J].
Blake, A. H. ;
Caceres, C. H. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 483-84 (1-2 C) :161-163
[6]  
Cáceres CH, 2002, PHYS STATUS SOLIDI A, V194, P147, DOI 10.1002/1521-396X(200211)194:1<147::AID-PSSA147>3.0.CO
[7]  
2-L
[8]  
Caceres CH, 2001, J Light Met, V1, P151, DOI [DOI 10.1016/S1471-5317(01)00008-6, 10.1016/S1471-5317(01)00008-6]
[9]  
CHAPMAN JA, 1962, J I MET, V91, P39
[10]   Mechanical properties and press formability at room temperature of AZ31 Mg alloy processed by single roller drive rolling [J].
Chino, Y ;
Mabuchi, M ;
Kishihara, R ;
Hosokawa, H ;
Yamada, Y ;
Wen, C ;
Shinojima, K ;
Iwasaki, H .
MATERIALS TRANSACTIONS, 2002, 43 (10) :2554-2560