Effect of multiple laser peening on microstructural, fatigue and fretting-wear behaviour of austenitic stainless steel

被引:42
作者
Praveenkumar, K. [1 ,2 ,3 ]
Swaroop, S. [2 ]
Manivasagam, Geetha [1 ,3 ]
机构
[1] Vellore Inst Technol, Sch Mech Engn, Vellore 632014, Tamil Nadu, India
[2] Vellore Inst Technol, Sch Adv Sci, Surface Modificat Lab, Vellore 632014, Tamil Nadu, India
[3] Vellore Inst Technol, Ctr Biomat Cellular & Mol Theranost, Vellore 632014, Tamil Nadu, India
关键词
Austenitic stainless steel; Laser peening; TEM; EBSD; Compressive residual stress; RESIDUAL-STRESS STATE; MECHANICAL-PROPERTIES; AISI; 304-STAINLESS-STEEL; PHASE-TRANSFORMATION; CORROSION-RESISTANCE; SURFACE MODIFICATION; TITANIUM BORIDE; GRAIN-SIZE; ALLOY; ALUMINUM;
D O I
10.1016/j.surfcoat.2022.128611
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The present work investigates the influence of laser peening without coating (LPwC) on the fatigue and fretting wear behaviour of AISI 304 alloy subjected to one and five peening passes peened at 9 GW cm(-2). Laser peened samples were characterised for microstructure, residual stress, phase evolution and hardness. After LPwC, the samples induced maximum compressive residual stress of-380 and-581 MPa for one and five peening passes at 50 mu m from the surface. Microhardness was increased to 31 % and 71 % for one and five pass samples at 50 mu m depth. The microstructure of laser peening samples was characterised using a transmission electron microscope (TEM) and electron backscattered diffraction (EBSD). Dislocation density was increased after peening with twin twin interaction observed in both the peening cases and martensite induced at the junction of the twin-twin in five-time peened samples. Low angle grain fraction increased from 29 % (unpeened) to 41 % (one pass) and 63 % (five passes), and grain refinement was observed, where the average grain size reduced from 22.28 mu m (unpeened) to 18.36 mu m (one pass) and 9.51 mu m (five passes) for LPwC samples. Fretting wear behaviour at various loading (5, 10 and 20 N) displayed significant improvement in wear resistance of LPwC samples, as evident from lower wear volume loss. Fatigue testing performed at R = 0.1 exhibited an improvement in fatigue life of 1.4 and 2.4 times for one and five pass samples compared to unpeened samples at a stress amplitude of 450 MPa. Fatigue fractography revealed a decrease in striation spacing for LPwC samples (979 nm/cycle and 565 nm/cycle for one-and five-time peening) with a delay in crack-propagation rate.
引用
收藏
页数:15
相关论文
共 85 条
  • [51] Residual stress distribution and elevated temperature fatigue behaviour of laser peened Ti-6Al-4V with a curved surface
    Praveenkumar, K.
    Mylavarapu, Phani
    Sarkar, Aritra
    Samuel, E. Isaac
    Nagesha, A.
    Swaroop, S.
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2022, 156
  • [52] Residual Stress Distribution, Phase Transformation, and Wettability Characteristics of Laser Peened Austenitic Stainless Steel
    Praveenkumar, K.
    Swaroop, S.
    Manivasagam, Geetha
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (08) : 6846 - 6857
  • [53] Effects of grain size gradients on the fretting wear of a specially-processed low carbon steel against AISI E52100 bearing steel
    Rai, Prabhat K.
    Shekhar, S.
    Mondal, K.
    [J]. WEAR, 2018, 412 : 1 - 13
  • [54] Influence of laser peening without coating on microstructure and fatigue limit of Ti-15V-3Al-3Cr-3Sn
    Rajan, S. Sudhagara
    Manivasagam, Geetha
    Ranganathan, Mohan
    Swaroop, S.
    [J]. OPTICS AND LASER TECHNOLOGY, 2019, 111 : 481 - 488
  • [55] Effect of ultrasonic surface rolling on surface layer properties and fretting wear properties of titanium alloy Ti5Al4Mo6V2Nb1Fe
    Ren, Zhaojun
    Lai, Fuqiang
    Qu, Shengguan
    Zhang, Yalong
    Li, Xiaoqiang
    Yang, Chao
    [J]. SURFACE & COATINGS TECHNOLOGY, 2020, 389
  • [56] High temperature dry sliding wear behaviour of laser powder bed fused Inconel 718
    Samuel, Calvin
    Arivarasu, M.
    Prabhu, T. Ram
    [J]. ADDITIVE MANUFACTURING, 2020, 34
  • [57] Wear and friction of 6061-T6 aluminum alloy treated by laser shock processing
    Sánchez-Santana, U
    Rubio-González, C
    Gomez-Rosas, G
    Ocaña, JL
    Molpeceres, C
    Porro, J
    Morales, M
    [J]. WEAR, 2006, 260 (7-8) : 847 - 854
  • [58] Retardation of crack initiation and growth in austenitic stainless steels by laser peening without protective coating
    Sano, Y
    Obata, M
    Kubo, T
    Mukai, N
    Yoda, M
    Masaki, K
    Ochi, Y
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 417 (1-2): : 334 - 340
  • [59] Improvement in fatigue performance of friction stir welded A6061-T6 aluminum alloy by laser peening without coating
    Sano, Y.
    Masaki, K.
    Gushi, T.
    Sano, T.
    [J]. MATERIALS & DESIGN, 2012, 36 : 809 - 814
  • [60] Laser Peening without Coating as a Surface Enhancement Technology
    Sano, Yuji
    Akita, Koichi
    Masaki, Kiyotaka
    Ochi, Yasuo
    Altenberger, Igor
    Scholtes, Berthold
    [J]. JOURNAL OF LASER MICRO NANOENGINEERING, 2006, 1 (03): : 161 - 166