Simultaneous enhancement of mechanical and electrical properties of Cu-Ni-Si alloys via thermo-mechanical process

被引:45
作者
Wang, Changsheng [1 ]
Fu, Huadong [1 ,2 ,3 ]
Zhang, Hongtao [1 ]
He, Xingqun [1 ]
Xie, Jianxin [1 ,2 ,3 ]
机构
[1] Univ Sci & Technol Beijing, Beijing Adv Innovat Ctr Mat Genome Engn, Inst Adv Mat & Technol, Beijing 100083, Peoples R China
[2] Inst Adv Mat & Technol, Beijing Lab Metall Mat & Proc Modern Transportat, Beijing 100083, Peoples R China
[3] Univ Sci & Technol Beijing, Inst Adv Mat & Technol, Key Lab Adv Mat Proc, Minist Educ, Beijing 100083, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2022年 / 838卷
基金
中国国家自然科学基金;
关键词
Thermo-mechanical treatment; Cu-Ni-Si alloy; Precipitation strengthening; Microstructure; HIGH-STRENGTH; CR ALLOY; MICROSTRUCTURE; CONDUCTIVITY; IMPROVEMENT; HARDNESS; TENSILE;
D O I
10.1016/j.msea.2022.142815
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Developing high-performance copper alloys while simultaneously improving ultimate tensile strength (UTS) and electrical conductivity (EC) has been a key challenge and direction. Two thermo-mechanical processes were employed in this study to achieve simultaneous enhancement of UTS and EC of the Cu-3.08Ni-0.61Si-0.17Zn0.17Cr-0.04P alloy. After the two-stage cold-rolling and aging process (85% cold-rolling + 450 degrees C@60 min aging + 95% cold-rolling + 450 degrees C@30 min aging, referred to as Process A), the alloy's UTS and EC of the alloy are 856 +/- 26 MPa and 52.4 +/- 0.8% international annealed copper standard (IACS). The mechanical and electrical properties of the alloy with process A are much better than those of the alloy with single stage cold-rolling and aging treatment process (85% cold-rolling + 450@60 min aging, 786 +/- 12 MPa, 47.5 +/- 0.9% IACS). The UTS of the alloy reaches 905 +/- 11 MPa with pre-aging + two-stage cold-rolling-aging (450 degrees C@90 min pre-aging + process A, referred to as process B), and the EC reaches 52.5 +/- 0.2% IACS, indicating that process B enhanced the strength over process A. A large number of nano-scale delta-Ni2Si precipitates are observed in the samples after primary aging of process A and pre-aging of process B, leading to a more diffuse dislocation distribution during subsequent cold-rolling and then promoting further precipitation of the solute atoms during subsequent aging processes. In the samples treated by both process A and B, there are two sizes of delta-Ni2Si phase precipitates, simultaneously enhancing UTS and EC of the Cu-Ni-Si alloy.
引用
收藏
页数:12
相关论文
共 50 条
[41]   The effect of Zr element on the microstructure and properties of Cu-Ni-Si alloys [J].
Liu, Fuqiang ;
Zhang, Xiao ;
Zhang, Xiaocui ;
Liu, Qing ;
Qi, Fugong ;
Li, Chunyan ;
Chen, Liang ;
Ding, Haimin .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2025, 36 :2747-2759
[42]   Precipitation driven nano-twinning: Simultaneous enhancement of mechanical and electrical properties in Cu-Ni-Sn alloys [J].
Yang, Fei ;
Wu, Canhui ;
Li, Ruifeng ;
Xu, Yusong ;
Zhou, Lichu ;
Fang, Feng ;
Dong, Liming ;
Kim, Hyoung Seop ;
Huo, Wenyi ;
Yu, Tianbo .
SCRIPTA MATERIALIA, 2025, 267
[43]   Effect of Thermo-mechanical Treatment on Microstructure and Properties of Cu-15Ni-8Sn Alloy [J].
Xing Yan ;
Li Zhou ;
Gan Xueping ;
Li Si ;
Zhang Yang ;
Zhang Xianwei ;
Song Kexing .
RARE METAL MATERIALS AND ENGINEERING, 2018, 47 (01) :286-292
[44]   Effect of Ti addition on tensile properties of Cu-Ni-Si alloys [J].
Eungyeong Lee ;
Seungzeon Han ;
Kwangjun Euh ;
Sunghwan Lim ;
Sangshik Kim .
Metals and Materials International, 2011, 17 :569-576
[45]   Effect of V addition on hardness and electrical conductivity in Cu-Ni-Si alloys [J].
Han, S. Z. ;
Gu, J. H. ;
Lee, J. H. ;
Que, Z. P. ;
Shin, J. H. ;
Lim, S. H. ;
Kim, S. S. .
METALS AND MATERIALS INTERNATIONAL, 2013, 19 (04) :637-641
[46]   Effect of high contents of nickel and silicon on the microstructure and properties of Cu-Ni-Si alloys [J].
Tao, Shiping ;
Lu, Zhenlin ;
Xie, Hui ;
Zhang, Jinlong ;
Wei, Xin .
MATERIALS RESEARCH EXPRESS, 2022, 9 (04)
[47]   Enhanced mechanical and electrical properties of Cu-Ni-Be alloys through rotary swaging and aging treatment [J].
Zhou, Kaixuan ;
Zhao, Yonghao ;
Mao, Qingzhong ;
Li, Shunqiang ;
Liu, Jizi .
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 236 :1-18
[48]   Effect of Ti addition on tensile properties of Cu-Ni-Si alloys [J].
Lee, Eungyeong ;
Han, Seungzeon ;
Euh, Kwangjun ;
Lim, Sunghwan ;
Kim, Sangshik .
METALS AND MATERIALS INTERNATIONAL, 2011, 17 (04) :569-576
[49]   Microstructure and thermo-mechanical properties of NiTi shape memory alloys [J].
Hornbogen, E .
ADVANCED MATERIALS FORUM II, 2004, 455-456 :335-341
[50]   Mechanical and electrical properties and microstructure in Cu-Ni-Be alloys [J].
Ota, Satoshi ;
Muramatsu, Naokuni ;
Sengoku, Kazumasa ;
Watanabe, Chihiro ;
Monzen, Ryoichi .
Zairyo/Journal of the Society of Materials Science, Japan, 2007, 56 (06) :531-536