The effect of Fe species distribution and acidity of Fe-ZSM-5 on the hydrothermal stability and SO2 and hydrocarbons durability in NH3-SCR reaction

被引:47
作者
Shi, Xiaoyan [1 ]
He, Hong [1 ]
Xie, Lijuan [1 ]
机构
[1] Chinese Acad Sci, Res Ctr Ecoenvironm Sci, State Key Joint Lab Environm Simulat & Pollut Con, Beijing 100085, Peoples R China
基金
国家高技术研究发展计划(863计划); 中国国家自然科学基金;
关键词
Iron-ZSM-5; Ammonia selective catalytic reduction; Removal of nitrogen oxide; SO2; durability; Hydrothermal stability; SELECTIVE CATALYTIC-REDUCTION; NITRIC-OXIDE; DENO(X) CATALYSTS; NOX REDUCTION; SCR; NH3; MECHANISM; STATE; ZEOLITES; AMMONIA;
D O I
10.1016/S1872-2067(14)60268-0
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
Fe-exchanged ZSM-5 catalysts prepared from Na+ and H+ forms of ZSM-5 were evaluated for the selective catalytic reduction of NOx by NH3 (NH3-SCR). Fe-H-ZSM-5 showed higher SCR activity than Fe-Na-ZSM-5 both when fresh and after hydrothermal aging at 750 degrees C in 5% H2O/air. The Fe species distribution and acidity of Fe-H-ZSM-5 and Fe-Na-ZSM-5 were found to be different. The dealumination of the zeolite framework of Fe-H-ZSM-5 during hydrothermal aging was found to be more severe compared with that of Fe-Na-ZSM-5. The durability of Fe-H-ZSM-5 and Fe-Na-ZSM-5 in NH3-SCR was compared using SO2 tolerance and hydrocarbon resistance experiments. The effect of water and SO2 on the activity of the two catalysts was similar, such that their activity decreased at low temperatures and increased at high temperatures. Fe-Na-ZSM-5 showed better propene resistance than Fe-H-ZSM-5. The SO2 and propene poisoning of the two Fe-ZSM-5 catalysts were found to be reversible. (C) 2015, Dalian Institute of Chemical Physics, Chinese Academy of Sciences. Published by Elsevier B.V. All rights reserved.
引用
收藏
页码:649 / 656
页数:8
相关论文
共 39 条
[1]   Hydrothermal deactivation of Fe-ZSM-5 catalysts for the selective catalytic reduction of NO with NH3 [J].
Brandenberger, Sandro ;
Kroecher, Oliver ;
Casapu, Maria ;
Tissler, Arno ;
Althoff, Roderik .
APPLIED CATALYSIS B-ENVIRONMENTAL, 2011, 101 (3-4) :649-659
[2]   The determination of the activities of different iron species in Fe-ZSM-5 for SCR of NO by NH3 [J].
Brandenberger, Sandro ;
Kroecher, Oliver ;
Tissler, Arno ;
Althoff, Roderik .
APPLIED CATALYSIS B-ENVIRONMENTAL, 2010, 95 (3-4) :348-357
[3]   Estimation of the fractions of different nuclear iron species in uniformly metal-exchanged Fe-ZSM-5 samples based on a Poisson distribution [J].
Brandenberger, Sandro ;
Kroecher, Oliver ;
Tissler, Arno ;
Althoff, Roderik .
APPLIED CATALYSIS A-GENERAL, 2010, 373 (1-2) :168-175
[4]   The role of Bronsted acidity in the selective catalytic reduction of NO with ammonia over Fe-ZSM-5 [J].
Brandenberger, Sandro ;
Kroecher, Oliver ;
Wokaun, Alexander ;
Tissler, Arno ;
Althoff, Roderik .
JOURNAL OF CATALYSIS, 2009, 268 (02) :297-306
[5]   The State of the Art in Selective Catalytic Reduction of NOx by Ammonia Using Metal-Exchanged Zeolite Catalysts [J].
Brandenberger, Sandro ;
Kroecher, Oliver ;
Tissler, Arno ;
Althoff, Roderik .
CATALYSIS REVIEWS-SCIENCE AND ENGINEERING, 2008, 50 (04) :492-531
[6]   Catalytic behaviour of hybrid LNT/SCR systems: Reactivity and in situ FTIR study [J].
Castoldi, L. ;
Bonzi, R. ;
Lietti, L. ;
Forzatti, P. ;
Morandi, S. ;
Ghiotti, G. ;
Dzwigaj, S. .
JOURNAL OF CATALYSIS, 2011, 282 (01) :128-144
[7]   Activity and durability of Fe/ZSM-5 catalysts for lean burn NOx reduction in the presence of water vapor [J].
Chen, HY ;
Sachtler, WMH .
CATALYSIS TODAY, 1998, 42 (1-2) :73-83
[8]   NMR studies of Cu/zeolite SCR catalysts hydrothermally aged with urea [J].
Cheng, Yisun ;
Hoard, John ;
Lambert, Christine ;
Kwak, Ja Hun ;
Peden, Charles H. F. .
CATALYSIS TODAY, 2008, 136 (1-2) :34-39
[9]   The influence of cocations H, Na, and Ba on the properties of Cu-faujasite for the selective catalytic reduction of NO by NH3:: An Operando DRIFT study [J].
Coq, B ;
Delahay, G ;
Durand, R ;
Berthomieu, D ;
Ayala-Villagomez, E .
JOURNAL OF PHYSICAL CHEMISTRY B, 2004, 108 (30) :11062-11068
[10]   Selective catalytic reduction of nitric oxide with ammonia on Fe-ZSM-5 catalysts prepared by different methods [J].
Delahay, G ;
Valade, D ;
Guzmán-Vargas, A ;
Coq, B .
APPLIED CATALYSIS B-ENVIRONMENTAL, 2005, 55 (02) :149-155