Effect of long-term storage on nanomechanical and morphological properties of dentin-adhesive interfaces

被引:28
作者
Anchieta, Rodolfo Bruniera [1 ,4 ]
Machado, Lucas Silveira [2 ,4 ]
Martini, Ana Paula [1 ]
dos Santos, Paulo Henrique [1 ,2 ]
Giannini, Marcelo [3 ]
Janal, Malvin [4 ]
Tovar, Nick [4 ]
Sundfeld, Renato Herman [2 ]
Rocha, Eduardo Passos [1 ]
Coelho, Paulo G. [4 ]
机构
[1] Univ Estadual Paulista, UNESP, Aracatuba Dent Sch, Dept Dent Mat & Prosthodont, Aracatuba, SP, Brazil
[2] Univ Estadual Paulista, UNESP, Aracatuba Dent Sch, Dept Restorat Dent, Aracatuba, SP, Brazil
[3] Univ Estadual Campinas, Piracicaba Dent Sch, Dept Restorat Dent, Piracicaba, SP, Brazil
[4] NYU, Dept Biomat & Biomimet, New York, NY 10010 USA
基金
巴西圣保罗研究基金会;
关键词
Dentin; Hybrid layer; Hydrolytic degradation; Mechanical properties; Dentin-adhesive interface; SELF-ETCH ADHESIVES; MECHANICAL-PROPERTIES; MICROMECHANICAL ANALYSIS; WATER SORPTION; RESIN; SYSTEMS; BONDS; DEGRADATION; DURABILITY; INDENTATION;
D O I
10.1016/j.dental.2014.11.010
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Introduction. To evaluate the influence of storage time on the elastic modulus, micromorphology, nanoleakage, and micromechanical behavior of the dentin-adhesive interfaces of five adhesive systems (Scotchbond Multi-Purpose, Clearfil SE Bond, One Up Bond F, Adper Easy One, and Filtek LS Adhesive) after 24 h (T0) and 12 months (T1). Methods. Fifty teeth were restored and distributed according to each adhesive system (n = 10). At least four specimens were obtained from each tooth. One specimen was evaluated under SEM to obtain the micromorphology of dentin-adhesive interface (DAI). Two specimens were used to assess nanoleakage, one tested in T0 and the other in T1. The last specimen was used for nanoindentation, in T0 and T1, to obtain the initial and final mechanical properties of DAI structures. Two non-restored teeth were evaluated under SEM to obtain the dentin morphology. Laboratorial data were used to build 15 finite element models to assess the maximum principal stress in each time of analysis. Results. Storage resulted in hydrolysis of the dentin-adhesive interfaces for all groups. Silver impregnation increased for all groups after 1 year storage (p < .05), except for Clearfil SE Bond. In general, a decrease in elastic modulus values was observed for all groups from T0 to T1 (p < .05), mainly at the hybrid layer. The FEAs showed higher stress levels at T1 than T0 simulations for all adhesives. Conclusion. At T1, degradation occurred at the dentin-adhesive interface formed by all adhesives, and the intensity of degradation differed depending on the type of adhesive system used. The interface formed by the self-etching primer containing the 10-MDP functional monomer showed the highest stability among the adhesive systems after 12 months of storage. (C) 2014 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:141 / 153
页数:13
相关论文
共 47 条
[1]  
Anchieta R.B., 2011, INT J CLIN DENT, V4, P199
[2]   Localized mechanics of dentin self-etching adhesive system [J].
Anchieta, Rodolfo Bruniera ;
Rocha, Eduardo Passos ;
Ko, Ching-Chang ;
Sundfeld, Renato Herman ;
Martin, Manoel, Jr. ;
Archangelo, Carlos Marcelo .
JOURNAL OF APPLIED ORAL SCIENCE, 2007, 15 (04) :321-326
[3]  
[Anonymous], E1457742007 ISO 4
[4]   Dental adhesion review: Aging and stability of the bonded interface [J].
Breschi, Loyenzo ;
Mazzoni, Annalisa ;
Ruggeri, Alessandra ;
Cadenaro, Milena ;
Di Lenarda, Robeyto ;
Dorigo, Elettya De Stefano .
DENTAL MATERIALS, 2008, 24 (01) :90-101
[5]  
Carrilho MRO, 2005, AM J DENT, V18, P315
[6]   A challenge to the conventional wisdom that simultaneous etching and resin infiltration always occurs in self-etch adhesives [J].
Carvalho, RM ;
Chersoni, S ;
Frankenberger, R ;
Pashley, DH ;
Prati, C ;
Tay, FR .
BIOMATERIALS, 2005, 26 (09) :1035-1042
[7]   Light-curing Time and Aging Effects on the Nanomechanical Properties of Methacrylate- and Silorane-based Restorations [J].
Catelan, A. ;
Pollard, T. ;
Bedran-Russo, A. K. ;
dos Santos, P. H. ;
Ambrosano, G. M. B. ;
Aguiar, F. H. B. .
OPERATIVE DENTISTRY, 2014, 39 (04) :389-397
[8]   A critical review of the durability of adhesion to tooth tissue: Methods and results [J].
De Munck, J ;
Van Landuyt, K ;
Peumans, M ;
Poitevin, A ;
Lambrechts, P ;
Braem, M ;
Van Meerbeek, B .
JOURNAL OF DENTAL RESEARCH, 2005, 84 (02) :118-132
[9]   Long-term nano-mechanical properties of biomodified dentin-resin interface components [J].
Dos Santos, Paulo Henrique ;
Karol, Sachin ;
Pedran-Russo, Ana Karina .
JOURNAL OF BIOMECHANICS, 2011, 44 (09) :1691-1694
[10]   Nanoleakage, ultramorphological characteristics, and microtensile bond strengths of a new low-shrinkage composite to dentin after artificial aging [J].
Duarte, Sillas, Jr. ;
Phark, Jin-Ho ;
Varjao, Fabiana Mansur ;
Sadan, Avishai .
DENTAL MATERIALS, 2009, 25 (05) :589-600