Effect of the ferrite morphology on hydrogen embrittlement of MAG welded 304 austenitic stainless steel

被引:20
作者
Zhou, Chilou [1 ]
Dai, Pengzhi [1 ]
Wu, Hao [1 ]
He, Mohan [1 ]
Liu, Xianhui [1 ]
Chu, Paul K. [2 ,3 ]
机构
[1] South China Univ Technol, Sch Mech & Automot Engn, Guangzhou 510641, Peoples R China
[2] City Univ Hong Kong, Dept Phys, Dept Mat Sci & Engn, Tat Chee Ave, Hong Kong, Peoples R China
[3] City Univ Hong Kong, Dept Biomed Engn, Kowloon, Tat Chee Ave, Hong Kong, Peoples R China
基金
中国国家自然科学基金;
关键词
Ferrite morphology; Hydrogen segregation; Hydrogen embrittlement; Austenitic stainless steel weld; Metal active gas arc welding; MECHANICAL-PROPERTIES; TENSILE PROPERTIES; FAILURE-MECHANISM; DELTA-FERRITE; BEHAVIOR; MICROSTRUCTURE; DEPENDENCE; PRESSURE; FRACTURE;
D O I
10.1016/j.apsusc.2022.154866
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Ferrite usually plays an important role in the hydrogen embrittlement (HE) of austenitic stainless steel (gamma-SS) weld. However, there are few investigations on the effect of ferrite morphology on HE. In this study, the relationship between the ferrite morphology and HE of metal active gas (MAG) welded 304 austenitic stainless steel is investigated. Hydrogen distribution testing and simulation reveal that the ferrite/austenite interfaces become the hydrogen segregation regions and the degree of hydrogen segregation at the interface is affected by ferrite morphology, which shows the order of lathy ferrite > reticular ferrite > skeletal ferrite. The slow strain rate tensile (SSRT) test indicates that the susceptibility to HE of welds containing lathy ferrite, skeletal ferrite and reticular ferrite reaches 34.6%, 30.7% and 33.2%, respectively. It can be found that the HE resistance shows the order of skeletal ferrite > reticular ferrite > lathy ferrite, which corresponds to the order of increasing hydrogen segregation. Hence, the ferrite morphology influences the resistance to HE of welds by affecting hydrogen segregation at the ferrite/austenite interface. A similar ferrite morphological dependence is observed from the weld fractures.
引用
收藏
页数:10
相关论文
共 44 条
[1]   Fatigue behavior of stainless steels with different ferrite and austenite volume fraction in 3%NaCl solution [J].
Akita, M ;
Nakajima, M ;
Tokaji, K .
TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2003, 89 (08) :863-870
[2]  
[Anonymous], 2009, 10111 EN
[3]  
BEACHEM CD, 1972, METALL TRANS, V3, P437
[4]   ADSORPTION OF HYDROGEN ON PD(100) [J].
BEHM, RJ ;
CHRISTMANN, K ;
ERTL, G .
SURFACE SCIENCE, 1980, 99 (02) :320-340
[5]   HYDROGEN INDUCED DUCTILITY LOSSES IN AUSTENITIC STAINLESS-STEEL WELDS [J].
BROOKS, JA ;
WEST, AJ .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1981, 12 (02) :213-223
[6]   INTERACTION OF HYDROGEN WITH A PALLADIUM(110) SURFACE [J].
CATTANIA, MG ;
PENKA, V ;
BEHM, RJ ;
CHRISTMANN, K ;
ERTL, G .
SURFACE SCIENCE, 1983, 126 (1-3) :382-391
[7]   Effect of welding speed on microstructures, mechanical properties and corrosion behavior of GTA-welded AISI 201 stainless steel sheets [J].
Chuaiphan, Wichan ;
Srijaroenpramong, Loeshpahn .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2014, 214 (02) :402-408
[8]   Hydrogen embrittlement behavior of SUS301L-MT stainless steel laser-arc hybrid welded joint localized zones [J].
Fu, Z. H. ;
Yang, B. J. ;
Shan, M. L. ;
Li, T. ;
Zhu, Z. Y. ;
Ma, C. P. ;
Zhang, X. ;
Gou, G. Q. ;
Wang, Z. R. ;
Gao, W. .
CORROSION SCIENCE, 2020, 164
[9]  
Fujii T., 1982, AM SOC MET, P361
[10]   Effect of hydrogen charging on the microstructure of duplex stainless steel [J].
Glowacka, A ;
Swiatnicki, WA .
JOURNAL OF ALLOYS AND COMPOUNDS, 2003, 356 :701-704