Significance of fracture toughness test results of beam welds in evaluation of brittle fracture performance of girth welded pipe joints

被引:2
|
作者
Ohata, Mitsuru
Toyoda, Masao
Ishikawa, Nobuyuk
Shinmiya, Toyohisa
机构
[1] Osaka Univ, Grad Sch Engn, Div Mat & Mfg Sci, Suita, Osaka 5650871, Japan
[2] JFE Steel Corp, Steel Res Lab, Fukuyama, Hiroshima 7218510, Japan
关键词
beam welds; linepipe; Charpy impact testing; three-point bend testing; fracture; toughness; FPD (fracture path deviation); toughness transition curve; Weibull stress; plastic constraint; fracture performance;
D O I
10.1115/1.2767652
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
High power beam welds, such as electron beam welds or laser welds, sometimes provide fracture path deviation (FPD) in standardized Charpy V-notch fracture toughness testing due to narrow bead profile together with higher overmatching in strength between weld metal and base metal. Moreover it should be noted that these typical features of beam welds might result in a plastic constraint loss around both the notch and crack tip in fracture toughness test specimens. Even in the temperature range where FPD would not occur the fracture toughness test results could not necessarily be an intrinsic value of such beam welds. These fracture properties make it difficult to evaluate fracture performance of girth welded pipe joints. In this paper the estimation method of intrinsic fracture toughness of beam weld metal itself using standard toughness test specimens is proposed on the basis of "Weibull stress criterion." The predicted intrinsic fracture toughness was found to be lower than the test results both in standard Charpy specimen and in three-point bend specimen with fatigue precrack. The assessment of brittle fracture performance of girth welded pipeline was conductedfirom the estimated intrinsic fracture toughness of girth welds by means of Weibull stress criterion. It was demonstrated that the low intrinsic fracture toughness of beam welds could not directly lead to the low fracture performance of a pipe joint under tensile loading. This is because of a lower plastic constraint compared to a three-point bend specimen due to difference in loading mode together with constraint loss in pipe joints and shielding effect of straining in weld metal due to highly overmatched narrow welds.
引用
收藏
页码:609 / 618
页数:10
相关论文
共 50 条
  • [21] Effects of Heat-Affected Zone Microstructure on Fracture Toughness of Two X70 Pipe Girth Welds
    Dong-Yeob Park
    Babak Shalchi Amirkhiz
    Jean-Philippe Gravel
    Yiyu Wang
    Leijun Li
    Renata Zavadil
    Jie Liang
    Pei Liu
    Anqiang He
    Muhammad Arafin
    Metallurgical and Materials Transactions A, 2017, 48 : 3248 - 3260
  • [22] Effects of Heat-Affected Zone Microstructure on Fracture Toughness of Two X70 Pipe Girth Welds
    Park, Dong-Yeob
    Amirkhiz, Babak Shalchi
    Gravel, Jean-Philippe
    Wang, Yiyu
    Li, Leijun
    Zavadil, Renata
    Liang, Jie
    Liu, Pei
    He, Anqiang
    Arafin, Muhammad
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2017, 48A (07): : 3248 - 3260
  • [23] Fracture toughness evaluation for dissimilar steel joints by Charpy impact test
    Takashima, Yasuhito
    Ito, Yusuke
    Lu, Fenggui
    Minami, Fumiyoshi
    WELDING IN THE WORLD, 2019, 63 (05) : 1243 - 1254
  • [24] Fracture toughness evaluation for dissimilar steel joints by Charpy impact test
    Yasuhito Takashima
    Yusuke Ito
    Fenggui Lu
    Fumiyoshi Minami
    Welding in the World, 2019, 63 : 1243 - 1254
  • [25] Effect of the Morphology of Structure on the Resistance of Welded Joints of High-Strength Pipe Steels to Brittle Fracture
    L. A. Efimenko
    A. A. Ramus’
    Metal Science and Heat Treatment, 2016, 57 : 559 - 563
  • [26] Effect of the Morphology of Structure on the Resistance of Welded Joints of High-Strength Pipe Steels to Brittle Fracture
    Efimenko, L. A.
    Ramus', A. A.
    METAL SCIENCE AND HEAT TREATMENT, 2016, 57 (9-10) : 559 - 563
  • [27] Evaluation of the fracture toughness of butt-welded joints using the boundary effect model
    Li, Yao
    Lu, Pengmin
    Wang, Binhua
    Hu, Xiaozhi
    Li, Datao
    Xiang, Qingyi
    ENGINEERING FRACTURE MECHANICS, 2022, 274
  • [28] Microstructure and fracture toughness of electron beam welded joints of 30CrMnSiNi2A steel
    Chen, Furong
    Huo, Lixing
    Zhang, Yufeng
    Zhang, Li
    Liu, Fangjun
    Chen, Gang
    2002, China Welding (11):
  • [29] Microstructure and fracture toughness of electron beam welded joints of 30CrMnSiNi2A steel
    Chen, Furong
    Huo, Lixing
    Zhang, Yufeng
    Zhang, Li
    Liu, Fangjun
    Chen, Gang
    Welding Research Abroad, 2003, 49 (01): : 13 - 17
  • [30] Microstructure and fracture toughness of electron beam welded joints of 30CrMnSiNi2A steel
    陈芙蓉
    霍立兴
    张玉凤
    张莉
    刘方军
    陈刚
    China Welding, 2002, (01) : 22 - 26