EBSD characterization of secondary microcracks in the heat affected zone of a X100 pipeline steel weld joint

被引:61
|
作者
Li, Xueda [1 ]
Ma, Xiaoping [2 ]
Subramanian, S. V. [2 ]
Shang, Chengjia [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
[2] McMaster Univ, Dept Mat Sci & Engn, Hamilton, ON L8S 4L8, Canada
关键词
Pipeline steel; Welding; Secondary microcracks; EBSD; Brittle fracture; CRYSTALLOGRAPHIC MECHANISM; CRACK-PROPAGATION; CLEAVAGE FRACTURE; STRESS; MICROSTRUCTURE; MARTENSITE; MORPHOLOGY; TOUGHNESS;
D O I
10.1007/s10704-015-0024-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In order to get better understanding of the mechanism of cleavage fracture in the heat affected zone (HAZ) of X100 pipeline steel, secondary microcracks underneath the brittle fracture surface of a Charpy impacted sample with the notch located in the HAZ were characterized using electron backscattered diffraction. Since the coarse grained (CG) HAZ and inter-critically reheated coarse grained (ICCG) HAZ are well accepted as the weakest region in the HAZ, the cleavage secondary microcracks in these two regions were observed respectively. Initiation and propagation of cleavage microcracks were discussed. The results show that the fracture behavior is obviously influenced by local microstructure. There are more secondary microcracks in the ICCGHAZ than in the CGHAZ which shows different probability for microcrack nucleation. Fracture mechanism changes from nucleation control in the CGHAZ to propagation control in the ICCGHAZ. The main reason for the increased possibility of secondary microcracks formation and the change in fracture mechanism is due to the formation of coarse necklacing martensite-austenite constituent in the ICCGHAZ. The results also show that high angle boundary, with the misorientation larger than 45 degrees, is effective in deflecting or arresting brittle cracks, while low angle boundary (15 degrees-45 degrees) seems not. Most preferred crack planes are {100}, with decreasing probability of {110}, {112}, {123}.
引用
收藏
页码:131 / 139
页数:9
相关论文
共 50 条
  • [21] Microstructure and toughness of heat-affected zone of weld joint for pipeline steels with high deformability
    Jia S.
    Wang Y.
    Tan F.
    Liu Q.
    Cailiao Yanjiu Xuebao, 7 (517-523): : 517 - 523
  • [22] Effect of Electrochemical Hydrogen Charging on Hydrogen Embrittlement and Mechanical Properties of Quenched Tempered X100 Pipeline Steel
    Davani, Reza Khatib Zadeh
    Entezari, Ehsan
    Mohtadi-Bonab, M. A.
    Yadav, Sandeep
    Cabezas, Jhon Freddy Aceros
    Szpunar, Jerzy
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2024, 24 (01) : 318 - 330
  • [23] Microstructural analysis of fracture in heat-affected zone of two x70 pipeline steel weldments
    Wang, Yiyu
    Park, Dong-Yeob
    Li, Leijun
    CANADIAN METALLURGICAL QUARTERLY, 2018, 57 (02) : 129 - 139
  • [24] Investigation on cold cracking susceptibility of X100 pipeline steel
    Yan C.
    Yuan Y.
    Zhang K.
    Wu L.
    Wang B.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (12): : 41 - 46
  • [25] Effect of secondary peak temperature on microstructure and toughness in ICCGHAZ of laser-arc hybrid welded X100 pipeline steel joints
    Qi, Xiaonan
    Di, Hongshuang
    Wang, Xiaonan
    Liu, Zhenguang
    Misra, R. D. K.
    Huan, Pengcheng
    Gao, Yuan
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (04): : 7838 - 7849
  • [26] Effect of Crystallographic Texture on Anisotropy of Yield Strength in X100 Pipeline Steel
    ZONG Cui
    ZHU Guo-hui
    MAO Wei-min
    Journal of Iron and Steel Research(International), 2013, 20 (08) : 66 - 71
  • [27] Ductile failure of X100 pipeline steel - Experiments and fractography
    Ghajar, Rahmatollah
    Mirone, Giuseppe
    Keshavarz, Arash
    MATERIALS & DESIGN, 2013, 43 : 513 - 525
  • [28] Effect of Crystallographic Texture on Anisotropy of Yield Strength in X100 Pipeline Steel
    Cui Zong
    Guo-hui Zhu
    Wi-min Mao
    Journal of Iron and Steel Research International, 2013, 20 : 66 - 71
  • [29] A Comparative Analysis on Microstructure and Fracture Mechanism of X100 Pipeline Steel CGHAZ Between Laser Welding and Arc Welding
    Qi, Xiaonan
    Di, Hongshuang
    Sun, Qian
    Wang, Xiaonan
    Chen, Xiaming
    Gao, Yuan
    Liu, Zhenguang
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (11) : 7006 - 7015
  • [30] Effects of cleavage triggers and constraint on brittle fracture in steel weld heat affected zone
    Shimada, Yusuke
    Kayamori, Yoichi
    Inoue, Takehiro
    Tagawa, Tetsuya
    THERMEC 2011, PTS 1-4, 2012, 706-709 : 951 - +