Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: Crack-inhibiting and multiple strengthening mechanisms

被引:406
作者
Li, Ruidi [1 ]
Wang, Minbo [1 ]
Li, Zhiming [1 ,2 ]
Cao, Peng [3 ,4 ]
Yuan, Tiechui [1 ]
Zhu, Hongbin [5 ]
机构
[1] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
[2] Max Planck Inst Eisenforsch GmbH, Max Planck Str 1, D-40237 Dusseldorf, Germany
[3] Univ Auckland, Dept Chem & Mat Engn, Private Bag 92019, Auckland 1142, New Zealand
[4] Victoria Univ Wellington, MacDiarmid Inst Adv Mat & Nanotechnol, POB 600, Wellington, New Zealand
[5] CRRC Ind Acad Co Ltd, Beijing 100070, Peoples R China
基金
中国国家自然科学基金;
关键词
Additive manufacturing; Selective laser melting; Aluminum alloys; Al-Mg-Sc; Hot cracking; Strengthening mechanism; ALUMINUM-ALLOYS; HEAT-TREATMENT; AL-12SI ALLOY; GRAIN-SIZE; MICROSTRUCTURE; BEHAVIOR; SUSCEPTIBILITY; TEMPERATURE; INFILTRATION; RESISTANCE;
D O I
10.1016/j.actamat.2020.03.060
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To develop high-strength Al alloys for selective laser melting (SLM) additive manufacturing, we designed a series of Al-Mg(-Si)-Sc-Zr alloys and additively manufactured them using atomized alloy powders. In the absence of Si, the developed Al-xMg-0.2Sc-0.1Zr (x = 1.5, 3.0 and 6.0 wt%) alloys are all susceptible to hot cracking and the average crack density increases with increasing Mg content. The addition of 1.3 wt% Si into the Al-6Mg-0.2Sc-0.1Zr alloys effectively inhibits hot cracking during SLM and simultaneously refines the microstructure, and thus leading to enhanced mechanical properties in the as-printed samples. By further fine-tuning the alloy compositions, we designed a new alloy Al-8.0Mg-1.3Si-0.5Mn-0.5Sc-0.3Zr. This new alloy demonstrates significantly refined microstructure consisting of submicron cells with coherent Al-3(Sc, Zr) nano-particle (2-15 nm) residing in the cell and intergranular Al-Mg2Si eutectic (Mg2Si diameter 10-100 nm). High-density stacking faults and a unique 9R phase are formed in the as-printed sample. The tensile strength and elongation of the as-printed sample are up to 497 MPa and 11%, respectively. After the aging treatment, the tensile strength reaches 550 MPa, while the ductility ranges from 8% to 17%, depending on the aging conditions. In addition to solid solution strengthening, grain boundary strengthening and nanoparticle strengthening, the high-density stacking faults also contributes to strengthening. (C) 2020 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:83 / 98
页数:16
相关论文
共 69 条
[1]   Microstructures and mechanical behavior of Inconel 718 fabricated by selective laser melting [J].
Amato, K. N. ;
Gaytan, S. M. ;
Murr, L. E. ;
Martinez, E. ;
Shindo, P. W. ;
Hernandez, J. ;
Collins, S. ;
Medina, F. .
ACTA MATERIALIA, 2012, 60 (05) :2229-2239
[2]   Role of silicon in accelerating the nucleation of Al3(Sc,Zr) precipitates in dilute Al-Sc-Zr alloys [J].
Booth-Morrison, C. ;
Mao, Z. ;
Diaz, M. ;
Dunand, D. C. ;
Wolverton, C. ;
Seidman, D. N. .
ACTA MATERIALIA, 2012, 60 (12) :4740-4752
[3]   Coarsening resistance at 400 °C of precipitation-strengthened Al-Zr-Sc-Er alloys [J].
Booth-Morrison, Christopher ;
Dunand, David C. ;
Seidman, David N. .
ACTA MATERIALIA, 2011, 59 (18) :7029-7042
[4]   In situ nanoindentation study on plasticity and work hardening in aluminium with incoherent twin boundaries [J].
Bufford, D. ;
Liu, Y. ;
Wang, J. ;
Wang, H. ;
Zhang, X. .
NATURE COMMUNICATIONS, 2014, 5
[5]   Aging Behavior of High-Strength Al Alloy 2618 Produced by Selective Laser Melting [J].
Casati, Riccardo ;
Lemke, Jannis Nicolas ;
Alarcon, Adrianni Zanatta ;
Vedani, Maurizio .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2017, 48A (02) :575-579
[6]   Deformation twinning in nanocrystalline aluminum [J].
Chen, MW ;
Ma, E ;
Hemker, KJ ;
Sheng, HW ;
Wang, YM ;
Cheng, XM .
SCIENCE, 2003, 300 (5623) :1275-1277
[7]   Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting [J].
Croteau, Joseph R. ;
Griffiths, Seth ;
Rossell, Marta D. ;
Leinenbach, Christian ;
Kenel, Christoph ;
Jansen, Vincent ;
Seidman, David N. ;
Dunand, David C. ;
Vo, Nhon Q. .
ACTA MATERIALIA, 2018, 153 :35-44
[8]   Microstructure and mechanical properties of a precipitation-strengthened Al-Zr-Sc-Er-Si alloy with a very small Sc content [J].
De Luca, Anthony ;
Dunand, David C. ;
Seidman, David N. .
ACTA MATERIALIA, 2018, 144 :80-91
[9]   Characterization of interfacial microstructures in 3003 aluminum alloy blocks fabricated by ultrasonic additive manufacturing [J].
Dehoff, R. R. ;
Babu, S. S. .
ACTA MATERIALIA, 2010, 58 (13) :4305-4315
[10]   THEORETICAL PREDICTION AND DIRECT OBSERVATION OF THE 9R STRUCTURE IN AG [J].
ERNST, F ;
FINNIS, MW ;
HOFMANN, D ;
MUSCHIK, T ;
SCHONBERGER, U ;
WOLF, U ;
METHFESSEL, M .
PHYSICAL REVIEW LETTERS, 1992, 69 (04) :620-623