Interfacial enhancement and mechanical properties of CF/Al composites with improved interfacial structure induced by Al-Ni-Mg ternary reaction

被引:16
|
作者
Liu, Jiaming [1 ]
Zhang, Yubo [1 ,2 ]
Wang, Wei [1 ]
Yang, Xi [1 ]
Liu, Shichao [3 ]
Zhang, Junjia [4 ]
Guo, Zhongkai [1 ]
Wang, Tongmin [1 ,2 ]
Li, Tingju [1 ,2 ]
机构
[1] Dalian Univ Technol, Sch Mat Sci & Engn, Key Lab Solidificat Control & Digital Preparat Te, Dalian 116024, Peoples R China
[2] Dalian Univ Technol, Ningbo Inst, Ningbo 315016, Peoples R China
[3] Soochow Univ, Sch Iron & Steel, Suzhou 215006, Peoples R China
[4] Northeastern Univ, Sch Mat Sci & Engn, Key Lab Lightweight Struct Mat Liaoning Prov, Shenyang 110819, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2022年 / 831卷
基金
中国国家自然科学基金;
关键词
Carbon fiber reinforced Al-Matrix composites; Interfacial structure enhancement; Infiltration behavior; Failure behavior; ALUMINUM-MATRIX COMPOSITES; CARBON-FIBER; FABRICATION; NANOCOMPOSITES; WETTABILITY; STRENGTH; FRICTION; FRACTURE; MODULUS;
D O I
10.1016/j.msea.2021.142040
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In the present study, an Al-Ni-Mg ternary reaction was used to provide an improved interfacial structure of carbon fiber reinforced Al-matrix (CF/Al) composites fabricated by a rapid process in open space. Driven by ternary reaction, better infiltration behavior of Al matrix can be obtained. With increasing Mg element addition, the ternary reaction was enhanced with the formation of Al-Ni-Mg IMCs with gradually larger size. When the value is 2.5 wt%, the relative density increases from 96.3% to 97.1%, and the crack density is reduced by 88.5% compared with those of Al-matrix composites due to the elimination of micro-defects. At the same time, the formation of IMCs with optimal size and distribution was obtained, which indicates the suitably Al/Ni interfacial state and provides effective load transfer and significant enhancement of the mechanical properties. The ultimate tensile strength (UTS) of the composites with Al-2.5 Mg matrix is 108 MPa, which is 18.7% higher than that of the corresponding matrix, and the improvement of UTS is the largest compared with that of the composites with 1.25 wt%, 3.75 wt%, and 5 wt% Mg element addition.
引用
收藏
页数:10
相关论文
共 50 条
  • [21] Effect of Interfacial Interlocking Composite Zn Interlayer on Interfacial Microstructure and Mechanical Properties of Thick Plate Al/Mg FSW Joint
    Sun Jifeng
    Ke Liming
    Xu Yang
    Xing Li
    RARE METAL MATERIALS AND ENGINEERING, 2023, 52 (11) : 3900 - 3908
  • [22] Effects of Cu, Si and Mg additions on the interfacial properties and mechanical properties of Be/Al composites: First-principles calculations and experimental studies
    Kuang, Zeyang
    Han, Zhichao
    Wang, Chengjin
    Xia, Yixiao
    Sun, Yutong
    Ju, Boyu
    Yang, Wenshu
    Sun, Dongli
    Chen, Guoqin
    Wu, Gaohui
    SURFACES AND INTERFACES, 2024, 46
  • [23] Effect of diamond surface chemistry and structure on the interfacial microstructure and properties of Al/diamond composites
    Che, Zifan
    Li, Jianwei
    Wang, Luhua
    Qi, Yingxu
    Zhang, Yang
    Zhang, Hailong
    Wang, Xitao
    Wang, Jinguo
    Kim, Moon J.
    RSC ADVANCES, 2016, 6 (71): : 67252 - 67259
  • [24] Effect of oxidization of 3D-SiC preforms on the interfacial structure and mechanical properties of co-continuous SiC/Al composites
    Zhu, Jingbo
    Wang, Yangwei
    Bao, Chonggao
    Lu, Bingheng
    CERAMICS INTERNATIONAL, 2021, 47 (10) : 14635 - 14646
  • [25] Magnetic pulse welding of Al to Mg alloys: structural-mechanical properties of the interfacial layer
    Stern, A.
    Aizenshtein, M.
    MATERIALS SCIENCE AND TECHNOLOGY, 2011, 27 (12) : 1809 - 1813
  • [26] Influence of matrix property and interfacial reaction on the mechanical performance and fracture mechanism of TiC reinforced Al matrix lamellar composites
    Guo, Rui-Fen
    Wang, Ya
    Shen, Ping
    Shaga, Alateng
    Ma, Yun-Hai
    Jiang, Qi-Chuan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 775 (775):
  • [27] Effect of Cu/Ni coating on the interface and mechanical properties of Cf/2024Al composites
    Zhou, Xuan
    Gao, Yimin
    Wang, Yiran
    DIAMOND AND RELATED MATERIALS, 2023, 140
  • [28] Effect of thermal cycling on the mechanical properties of Cf/Al composites
    Li Daguang
    Chen Guoqin
    Jiang Longtao
    Xiu Ziyang
    Zhang Yunhe
    Wu Gaohui
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 586 : 330 - 337
  • [29] Effects of heat-treatment on the interfacial reaction and tensile properties of Al2O3 coated-Al18B4O33w/Al-Mg matrix composites
    Yu, Yucheng
    Tang, Shawei
    Hu, Jin
    MATERIALS & DESIGN, 2016, 90 : 416 - 423
  • [30] Effects of ceramic lamellae compactness and interfacial reaction on the mechanical properties of nacre-inspired Al/Al2O3-ZrO2 composites
    Guo, Rui-Fen
    Guo, Ning
    Shen, Ping
    Yang, Li-Kai
    Jiang, Qi-Chuan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 718 : 326 - 334