Improvement of stretch formability of Mg-3Al-1Zn alloy sheet by high temperature rolling at finishing pass

被引:145
作者
Huang, Xinsheng [1 ]
Suzuki, Kazutaka [1 ]
Chino, Yasumasa [1 ]
Mabuchi, Mamoru [2 ]
机构
[1] Natl Inst Adv Ind Sci & Technol, Mat Res Inst Sustainable Dev, Nagoya, Aichi 4638560, Japan
[2] Kyoto Univ, Grad Sch Energy Sci, Kyoto 6068501, Japan
关键词
Magnesium alloy; Microstructure; Texture; Stretch formability; Mechanical property; MAGNESIUM ALLOY; ROOM-TEMPERATURE; STATIC RECRYSTALLIZATION; PRESS FORMABILITY; AZ31; MICROSTRUCTURE; TEXTURE; COMBINATION; EVOLUTION; BEHAVIOR;
D O I
10.1016/j.jallcom.2011.04.132
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effects of increasing rolling temperature from 723K to 828K at the last rolling pass on microstructure, texture, mechanical properties and stretch formability of a Mg-3Al-1Zn magnesium alloy previously rolled at 723K were investigated. In the as-rolled condition, the basal texture strengthens slightly with increasing the rolling temperature whereas it weakens more remarkably after static recrystallization during annealing for the sheets rolled at higher temperatures. Only by increasing the rolling temperature from 723K to 798 K, the Erichsen value is significantly increased from 4.5 to 8.6 due to the weakened texture for the annealed sheets. Further increasing the last rolling temperature does not appear to further improve the stretch formability. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:7579 / 7584
页数:6
相关论文
共 27 条
[1]   Comparative study of the deformation behavior of hexagonal magnesium-lithium alloys and a conventional magnesium AZ31 alloy [J].
Al-Samman, T. .
ACTA MATERIALIA, 2009, 57 (07) :2229-2242
[2]  
Avedesian M.M., 1999, Magnesium and Magnesium Alloys, P258
[3]   Drawability of AZ31 magnesium alloy sheet produced by equal channel angular rolling at room temperature [J].
Cheng, Yong Qi ;
Chen, Zhen Hua ;
Xia, Wei Jun .
MATERIALS CHARACTERIZATION, 2007, 58 (07) :617-622
[4]   Mechanical properties and press formability at room temperature of AZ31 Mg alloy processed by single roller drive rolling [J].
Chino, Y ;
Mabuchi, M ;
Kishihara, R ;
Hosokawa, H ;
Yamada, Y ;
Wen, C ;
Shinojima, K ;
Iwasaki, H .
MATERIALS TRANSACTIONS, 2002, 43 (10) :2554-2560
[5]   Microstructure and press formability of a cross-rolled magnesium alloy sheet [J].
Chino, Yasumasa ;
Sassa, Kensuke ;
Kamiya, Akira ;
Mabuchi, Mamoru .
MATERIALS LETTERS, 2007, 61 (07) :1504-1506
[6]   Texture and stretch formability of a rolled Mg-Zn alloy containing dilute content of Y [J].
Chino, Yasumasa ;
Sassa, Kensuke ;
Mabuchi, Mamoru .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 513-14 :394-400
[7]   Enhanced stretch formability of Mg-Al-Zn alloy sheets rolled at high temperature (723 K) [J].
Chino, Yasumasa ;
Mabuchi, Mamoru .
SCRIPTA MATERIALIA, 2009, 60 (06) :447-450
[8]   Texture and Stretch Formability of Mg-1.5 mass % Zn-0.2 mass % Ce Alloy Rolled at Different Rolling Temperatures [J].
Chino, Yasumasa ;
Sassa, Kensuke ;
Mabuchi, Mamoru .
MATERIALS TRANSACTIONS, 2008, 49 (12) :2916-2918
[9]   DEFORMATION TWINNING [J].
CHRISTIAN, JW ;
MAHAJAN, S .
PROGRESS IN MATERIALS SCIENCE, 1995, 39 (1-2) :1-157
[10]  
*GEN STAND COMM JA, 2000, AL HDB GEN STAND COM, P103