Initiation of stress corrosion cracking and hydrogen-induced cracking in oil and gas line-pipe

被引:5
|
作者
Shehata, Mahmoud T. [1 ]
Elboujdaini, Mimoun [1 ]
Revie, R. Winston [1 ]
机构
[1] Nat Resources Canada, CANMET Mat Technol Lab, 568 Booth St, Ottawa, ON K1A OG1, Canada
来源
SAFETY, RELIABILITY AND RISKS ASSOCIATED WITH WATER, OIL AND GAS PIPELINES | 2008年
关键词
stress corrosion cracking; hydrogen-induced cracking; environmentally assisted cracking; oil and gas line-pipe steels;
D O I
10.1007/978-1-4020-6526-2_7
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Environmentally assisted cracks in line-pipe steels are initiated either as a result of stresses in combination with environmental effects, as in stress corrosion cracking (SCC), or as a result of trapped hydrogen in the steel, as in hydrogen-induced cracking (HIC). To understand better the mechanism of the crack initiation process, key metallurgical and environmental elements that can affect the cracking phenomena were investigated and are reviewed in this paper. The complexity of both cracking phenomena results from the dependence of SCC and HIC on multiple metallurgical, mechanical, and environmental parameters that may all influence both crack initiation and propagation; e.g., composition, microstructure, and nonmetallic inclusions in the steel, applied stress, water chemistry in the field, and ionic concentrations in the groundwater near the pipe surface to name a few for SCC. In addition, for HIC phenomena, one can add the concentration of hydrogen sulfide (H2S) in the fluids transported in the pipe as well as concentration Of CO2, pH, etc. In this paper, cracking of line-pipe steels is analyzed critically, with particular attention to the crack initiation process. The paper is divided into two parts: The first part covers SCC and the second covers HIC.
引用
收藏
页码:115 / +
页数:3
相关论文
共 50 条
  • [31] Studies on inhibition of hydrogen-induced cracking of linepipe steels
    Elboujdaîni, M
    Sastri, VS
    Perumareddi, JR
    CORROSION, 2006, 62 (01) : 29 - 34
  • [32] Hydrogen-induced cracking by nanovoids in 310 stainless steel
    黄一中
    陈奇志
    王燕斌
    褚武扬
    Science in China(Series E:Technological Sciences), 1998, (04) : 372 - 382
  • [33] Mechanism of hydrogen-induced intergranular cracking of tubular steels
    乔利杰
    褚武扬
    于广华
    程以环
    Science in China(Series E:Technological Sciences), 1996, (05) : 543 - 550
  • [34] Hydrogen-induced cracking by nanovoids in 310 stainless steel
    Yizhong Huang
    Qizhi Chen
    Yanbin Wang
    Wuyang Chu
    Science in China Series E: Technological Sciences, 1998, 41 : 372 - 382
  • [35] Mechanism of hydrogen-induced intergranular cracking of tubular steels
    Qiao, LJ
    Chu, WY
    Yu, GH
    Cheng, YH
    SCIENCE IN CHINA SERIES E-TECHNOLOGICAL SCIENCES, 1996, 39 (05): : 543 - 550
  • [36] Effect of microstructure on hydrogen-induced cracking of linepipe steels
    Koh, S. U.
    Jung, H. G.
    Kang, K. B.
    Park, G. T.
    Kim, K. Y.
    CORROSION, 2008, 64 (07) : 574 - 585
  • [37] Sulphide stress corrosion cracking of multiple welding repairs of girth welds in line pipe
    Vega, O. E.
    Villagomez, A.
    Hallen, J. M.
    Contreras, A.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2009, 44 (04) : 289 - 296
  • [38] Stress corrosion cracking of a buried flow line
    Bolzoni, F
    Cabrini, M
    Hoxha, G
    Pedeferri, P
    CORROSION IN REFINERY PETROCHEMICAL AND POWER GENERATION PLANTS, PROCEEDINGS, 2000, : 75 - 81
  • [39] Effect of hydrogen-induced plasticity on the stress corrosion cracking of X70 pipeline steel in simulated soil environments
    Liu, Z. Y.
    Wang, X. Z.
    Du, C. W.
    Li, J. K.
    Li, X. G.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 658 : 348 - 354
  • [40] Modelling Hydrogen Induced Stress Corrosion Cracking in Austenitic Stainless Steel
    Ogosi, E., I
    Asim, U. B.
    Siddiq, M. A.
    Kartal, M. E.
    JOURNAL OF MECHANICS, 2020, 36 (02) : 213 - 222