RHEOLOGICAL BEHAVIOUR OF THERMOPLASTIC POLY(ESTER-SILOXANE)S

被引:3
作者
Antic, Vesna V. [1 ]
Pergal, Marija V. [2 ]
Antic, Malisa P. [1 ]
Djonlagic, Jasna [3 ]
机构
[1] Univ Belgrade, Fac Agr, Belgrade, Serbia
[2] Univ Belgrade, Inst Chem Technol & Met, Ctr Chem, Belgrade, Serbia
[3] Univ Belgrade, Fac Technol & Met, Belgrade 11000, Serbia
关键词
Poly(ester-siloxane)s; Rheology; Complex dynamic viscosity; Storage and loss shear modulus; Microphase separation transition temperature; POLY(BUTYLENE TEREPHTHALATE); DISORDER TRANSITION; COPOLYMERS; POLYURETHANE; SILOXANE; ORDER;
D O I
10.2298/HEMIND101015067A
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Two series of thermoplastic elastomers (TPES), based on poly(dimethylsiloxane) (PDMS) as the soft segment and poly(butylene terephthalate) (PBT) as the hard segment, were analyzed by dynamic mechanical spectroscopy. In the first TPES series the lengths of both hard and soft segments were varied while the mass ratio of the hard to soft segments was nearly constant (about 60 mass%). In the second series, the mass ratio of hard and soft segments was varied in the range from 60/40 to 40/60, with a constant length of soft PDMS segments. The influence of the structure and composition of TPESs on the rheological properties, such as complex dynamic viscosity, eta*, the storage, G', and loss, G '', shear modulus as well as the microphase separation transition temperature, T-MST, was examined. The obtained results showed that the storage modulus of the TPESs increased in a rubbery plateau region with increase in degree of crystallinity. The rheological measurements of TPESs also showed that a microphase reorganization occurred during the melting process. The microphase separation transition temperatures were in the range from 220 to 234 degrees C. In the isotropic molten state, the complex dynamic viscosity increased with increasing both the content and lenght of hard PBT segments.
引用
收藏
页码:537 / 545
页数:9
相关论文
共 40 条
  • [31] Veenstra H, 1998, J POLYM SCI POL PHYS, V36, P1795, DOI 10.1002/(SICI)1099-0488(199808)36:11<1795::AID-POLB1>3.0.CO
  • [32] 2-Q
  • [33] Synthesis and characterization of poly(ester ether siloane)s
    Vuckovic, Mariia V.
    Antic, Vesna V.
    Dojcinovic, Bijana P.
    Govedarica, Milutin N.
    Djonlagic, Jasna
    [J]. POLYMER INTERNATIONAL, 2006, 55 (11) : 1304 - 1314
  • [34] Synthesis and Characterization of Copolymers Based on Poly(butylene terephthalate) and Ethylene Oxide-Poly(dimethylsiloxane)-Ethylene Oxide
    Vuckovic, Marija V.
    Antic, Vesna V.
    Govedarica, Milutin N.
    Djonlagic, Jasna
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2010, 115 (06) : 3205 - 3216
  • [35] Synthesis and characterization of organosiloxane modified segmented polyether polyurethanes
    Wang, LF
    Ji, Q
    Glass, TE
    Ward, TC
    McGrath, JE
    Muggli, M
    Burns, G
    Sorathia, U
    [J]. POLYMER, 2000, 41 (13) : 5083 - 5093
  • [36] YAMAMOTO N, 1990, Patent No. 4894427
  • [37] YILGOR I, 1988, ADV POLYM SCI, V86, P1
  • [38] Contribution of soft segment entanglement on the tensile properties of silicone-urea copolymers with low hard segment contents
    Yilgor, Iskender
    Eynur, Tugba
    Yilgor, Emel
    Wilkes, Garth L.
    [J]. POLYMER, 2009, 50 (19) : 4432 - 4437
  • [39] YOUNG DJ, 1992, Patent No. 5132392
  • [40] Characterization of polydimethylsiloxane-polyurethanes synthesized by graft or block copolymerizations
    Zong, Jianping
    Zhang, Qingsi
    Sun, Haifeng
    Yu, Yitao
    Wang, Shijie
    Liu, Yunhui
    [J]. POLYMER BULLETIN, 2010, 65 (05) : 477 - 493