High pressure performance of thin Pd-23%Ag/stainless steel composite membranes in water gas shift gas mixtures; influence of dilution, mass transfer and surface effects on the hydrogen flux

被引:177
作者
Peters, T. A. [1 ]
Stange, M. [1 ]
Klette, H. [1 ]
Bredesen, R. [1 ]
机构
[1] SINTEF Mat & Chem, N-0314 Oslo, Norway
关键词
palladium membrane; hydrogen flux; water gas shift; concentration polarisation; CO adsorption;
D O I
10.1016/j.memsci.2007.08.056
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The hydrogen permeation and stability of tubular palladium alloy (Pd-23%Ag) composite membranes have been investigated at elevated temperatures and pressures. In our analysis we differentiate between dilution of hydrogen by other gas components, hydrogen depletion along the membrane length, concentration polarization adjacent to the membrane surface, and effects due to surface adsorption, on the hydrogen flux. A maximum H-2 flux of 1223 mL cm(-2) min(-1) or 8.4 mol m(-2) s(-1) was obtained at 400 degrees C and 26bar hydrogen feed pressure, corresponding to a permeance of 6.4 x 10(-3) mol m(-2) s(-1) Pa-0.5. A good linear relationship was found between hydrogen flux and pressure as predicted for rate controlling bulk diffusion. In a mixture of 50% H-2 + 50% N-2 a maximum H-2 flux of 230 mL cm(-2) min(-1) and separation factor of 1400 were achieved at 26 bar. The large reduction in hydrogen flux is mainly caused by the build-up of a hydrogen-depleted concentration polarization layer adjacent to the membrane due to insufficient mass transport in the gas phase. Substituting N-2 with CO2 results in further reduction of flux, but not as large as for CO where adsorption prevail as the dominating flow controlling factor. In WGS conditions (57.5% H-2, 18.7% CO2, 3.8% CO, 1.2% CH4 and 18.7% steam), a H-2 permeance of 1.1 x 10(-3) mol m(-2) s(-1) Pa-0.5 was found at 400 degrees C and 26 bar feed pressure. Operating the membrane for 500 h under various conditions (WGS and H-2 + N-2 mixtures) at 26 bars indicated no membrane failure, but a small decrease in flux. A peculiar flux inhibiting effect of long term exposure to high concentration of N-2 was observed. The membrane surface was deformed and expanded after operation, mainly following the topography of the macroporous support. (C) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:119 / 127
页数:9
相关论文
共 24 条
  • [1] Hydrogen permeation through surface modified Pd and PdAg membranes
    Amandusson, H
    Ekedahl, LG
    Dannetun, H
    [J]. JOURNAL OF MEMBRANE SCIENCE, 2001, 193 (01) : 35 - 47
  • [2] The effect of CO and O2 on hydrogen permeation through a palladium membrane
    Amandusson, H
    Ekedahl, LG
    Dannetun, H
    [J]. APPLIED SURFACE SCIENCE, 2000, 153 (04) : 259 - 267
  • [3] Experimental and simulation of both Pd and Pd/Ag for a water gas shift membrane reactor
    Basile, A
    Chiappetta, G
    Tosti, S
    Violante, V
    [J]. SEPARATION AND PURIFICATION TECHNOLOGY, 2001, 25 (1-3) : 549 - 571
  • [4] Bredesen R., 2000, US Patent, Patent No. [6,086,729, 6086729]
  • [5] BREDESEN R, 2004, T MAT RES SOC JPN, V29, P3233
  • [6] Brüning H, 1933, Z PHYS CHEM A-CHEM T, V163, P409
  • [7] Influence of steam and carbon dioxide on the hydrogen flux through thin Pd/Ag and Pd membranes
    Gielens, F. C.
    Knibbeler, R. J. J.
    Duysinx, P. F. J.
    Tong, H. D.
    Vorstman, M. A. G.
    Keurentjes, J. T. F.
    [J]. JOURNAL OF MEMBRANE SCIENCE, 2006, 279 (1-2) : 176 - 185
  • [8] Effects of surface activity, defects and mass transfer on hydrogen permeance and n-value in composite palladium-porous stainless steel membranes
    Guazzone, Federico
    Engwall, Erik Edwin
    Ma, Yi Hua
    [J]. CATALYSIS TODAY, 2006, 118 (1-2) : 24 - 31
  • [9] The effect of external mass transfer, competitive adsorption and coking on hydrogen permeation through thin Pd/Ag membranes
    Hou, K
    Hughes, R
    [J]. JOURNAL OF MEMBRANE SCIENCE, 2002, 206 (1-2) : 119 - 130
  • [10] Compatibility of hydrogen transfer via Pd-membranes with the rates of heterogeneously catalysed steam reforming
    Kleinert, A
    Grubert, G
    Pan, XL
    Hamel, C
    Seidel-Morgenstern, A
    Caro, J
    [J]. CATALYSIS TODAY, 2005, 104 (2-4) : 267 - 273