Recent Advances in Hydrophobic and Icephobic Surface Treatments of Concrete

被引:79
作者
Di Mundo, Rosa [1 ]
Labianca, Claudia [1 ]
Carbone, Giuseppe [2 ]
Notarnicola, Michele [1 ]
机构
[1] Polytech Univ Bari, Dept Civil Environm Land Bldg Engn & Chem DICATEC, Via E Orabona 4, I-70125 Bari, Italy
[2] Polytech Univ Bari, Dept Mech Math & Management DMMM, Via E Orabona 4, I-70125 Bari, Italy
关键词
concrete; cement composite; surface treatment; coating; impregnation; pore blockage; hydrophobic; anti-icing; chloride penetration; corrosion resistance; REINFORCED-CONCRETE; CARBONATE PRECIPITATION; CHLORIDE PERMEABILITY; WATER-ABSORPTION; SOLID-SURFACES; REDUCING WATER; CORROSION; COATINGS; PERFORMANCE; RESISTANCE;
D O I
10.3390/coatings10050449
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this review, we present a survey on hydrophobic surface treatments of concrete, important protection tools against deterioration and corrosion phenomena. In the frame of a standardized distinction in coatings, pore blockage, and impregnation methods, we highlight the huge variety of compounds and formulations utilized, and the different performances reached in terms of water contact angle, water absorption, chloride penetration, and, rarely reported, anti-icing/icephobic action. Our view covers the spectrum of the surface treatments, but also makes a comparison with hydrophobic bulk modifications of concrete, procedures often utilized as well; further, novel proposals of more sustainable routes are presented. We note that coating and impregnation, preferably when based on polyurethane and silane/siloxane, respectively, appear more effective against water ingress. The achieved wetting character is hydrophobic or, at most, overhydrophobic. Superhydrophobic coatings for concrete have been obtained by embedding nano-powders in hydrophobic emulsions, allowing to add a nanotexture to the preexisting complex roughness of the material. Concrete treated with this type of coating has also recently shown a pronounced icephobic character, a parameter that goes beyond the freeze-thaw characterization usually conducted on cement-based materials.
引用
收藏
页数:36
相关论文
共 100 条
[1]   Development of hydrophobic concrete by adding dual-crystalline admixture at mixing stage [J].
Al-Kheetan, Mazen J. ;
Rahman, Mujib M. ;
Chamberlain, Denis A. .
STRUCTURAL CONCRETE, 2018, 19 (05) :1504-1511
[2]   Effectiveness of surface coatings in improving concrete durability [J].
Almusallam, AA ;
Khan, FM ;
Dulaijan, SU ;
Al-Amoudi, OSB .
CEMENT & CONCRETE COMPOSITES, 2003, 25 (4-5) :473-481
[3]  
Amleh L, 1999, ACI STRUCT J, V96, P415
[4]   QUANTITATIVE MEASUREMENTS OF CORROSION RATE OF REINFORCING STEELS EMBEDDED IN CONCRETE USING POLARIZATION RESISTANCE MEASUREMENTS [J].
ANDRADE, C ;
GONZALEZ, JA .
WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1978, 29 (08) :515-519
[5]  
[Anonymous], 2010, G102 ASTM
[6]   Superhydrophobic Coatings on Asphalt Concrete Surfaces Toward Smart Solutions for Winter Pavement Maintenance [J].
Arabzadeh, Ali ;
Ceylan, Halil ;
Kim, Sunghwan ;
Gopalakrishnan, Kasthurirangan ;
Sassani, Alireza .
TRANSPORTATION RESEARCH RECORD, 2016, (2551) :10-17
[7]  
ASTM International, 2009, 87609 ASTM INT
[8]   Purity of the sacred lotus, or escape from contamination in biological surfaces [J].
Barthlott, W ;
Neinhuis, C .
PLANTA, 1997, 202 (01) :1-8
[9]   Freeze-thaw resistance of concretes treated with pore liners [J].
Basheer, L. ;
Cleland, D. J. .
CONSTRUCTION AND BUILDING MATERIALS, 2006, 20 (10) :990-998
[10]   Corrosion protection investigation of reinforcement by inorganic coating in the presence of alkanolamine-based inhibitor [J].
Batis, G ;
Pantazopoulou, P ;
Routoulas, A .
CEMENT & CONCRETE COMPOSITES, 2003, 25 (03) :371-377