Effect of Bonding Strength on Electromigration Failure in Cu-Cu Bumps

被引:15
作者
Shie, Kai-Cheng [1 ,2 ]
Hsu, Po-Ning [1 ,2 ]
Li, Yu-Jin [1 ,2 ]
Tu, K. N. [1 ,2 ,3 ,4 ]
Chen, Chih [1 ,2 ]
机构
[1] Natl Yang Ming Chiao Tung Univ, Dept Mat Sci & Engn, Hsinchu 30010, Taiwan
[2] Natl Chiao Tung Univ, Dept Mat Sci & Engn, Hsinchu 30010, Taiwan
[3] Natl Yang Ming Chiao Tung Univ, Int Coll Semicond Technol, Hsinchu 30010, Taiwan
[4] Natl Chiao Tung Univ, Int Coll Semicond Technol, Hsinchu 30010, Taiwan
关键词
electromigration; Cu-Cu direct bonding; three-dimensional integrated circuits (3D ICs); RELIABILITY CHALLENGES; SOLDER; MICROBUMPS; GROWTH; JOINTS;
D O I
10.3390/ma14216394
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In microelectronic packaging technology for three-dimensional integrated circuits (3D ICs), Cu-to-Cu direct bonding appears to be the solution to solve the problems of Joule heating and electromigration (EM) in solder microbumps under 10 mu m in diameter. However, EM will occur in Cu-Cu bumps when the current density is over 106 A/cm2. The surface, grain boundary, and the interface between the Cu and TiW adhesion layer are the three major diffusion paths in EM tests, and which one may lead to early failure is of interest. This study showed that bonding strength affects the outcome. First, if the bonding strength is not strong enough to sustain the thermal mismatch of materials during EM tests, the bonding interface will fracture and lead to an open circuit of early failure. Second, if the bonding strength can sustain the bonding structure, voids will form at the passivation contact area between the Cu-Cu bump and redistribution layer (RDL) due to current crowding. When the void grows along the passivation interface and separates the Cu-Cu bump and RDL, an open circuit can occur, especially when the current density and temperature are severe. Third, under excellent bonding, when the voids at the contact area between the Cu-Cu bump and RDL do not merge together, the EM lifetime can be more than 5000 h.
引用
收藏
页数:16
相关论文
共 53 条
[1]  
Beyne E, 2017, INT EL DEVICES MEET
[2]   STRESS GENERATION BY ELECTROMIGRATION [J].
BLECH, IA ;
HERRING, C .
APPLIED PHYSICS LETTERS, 1976, 29 (03) :131-133
[3]   ELECTROMIGRATION IN THIN ALUMINUM FILMS ON TITANIUM NITRIDE [J].
BLECH, IA .
JOURNAL OF APPLIED PHYSICS, 1976, 47 (04) :1203-1208
[4]   Effect of anisotropic grain growth on improving the bonding strength of <111>-oriented nanotwinned copper films [J].
Chang, Shih-Yang ;
Chu, Yi-Cheng ;
Tu, K. N. ;
Chen, Chih .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 804
[5]  
Chen C, 2015, MRS BULL, V40, P257, DOI 10.1557/mrs.2015.29
[6]   Effect of deposition temperature on mechanical properties of nanotwinned Cu fabricated by rotary electroplating [J].
Cheng, Hsiang-Yuan ;
Dinh-Phuc Tran ;
Tu, K. N. ;
Chen, Chih .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 811
[7]   Electrical and Reliability Investigation of Cu-to-Cu Bonding With Silver Passivation Layer in 3-D Integration [J].
Chou, Tzu-Chieh ;
Huang, Shin-Yi ;
Chen, Pin-Jun ;
Hu, Han-Wen ;
Liu, Demin ;
Chang, Chih-Wei ;
Ni, Tzu-Hsuan ;
Chen, Chao-Jung ;
Lin, Yu-Min ;
Chang, Tao-Chih ;
Chen, Kuan-Neng .
IEEE TRANSACTIONS ON COMPONENTS PACKAGING AND MANUFACTURING TECHNOLOGY, 2021, 11 (01) :36-42
[8]   Electromigration drift and threshold in Cu thin-film interconnects [J].
Frankovic, R ;
Bernstein, GH .
IEEE TRANSACTIONS ON ELECTRON DEVICES, 1996, 43 (12) :2233-2239
[9]   An introduction to Cu electromigration [J].
Hau-Riege, CS .
MICROELECTRONICS RELIABILITY, 2004, 44 (02) :195-205
[10]   Electromigration lifetime and critical void volume [J].
He, J ;
Suo, Z ;
Marieb, TN ;
Maiz, JA .
APPLIED PHYSICS LETTERS, 2004, 85 (20) :4639-4641