Crystallization and sintering characteristics of chemically precipitated hydroxyapatite nanopowder

被引:67
作者
Sung, YM [1 ]
Lee, JC [1 ]
Yang, JW [1 ]
机构
[1] Daejin Univ, Funct Nanostructured Mat Lab, Dept Mat Sci & Engn, Pochunkoon 487711, Kyunggi Do, South Korea
关键词
biomaterials; crystallization; sintering; nanomaterials;
D O I
10.1016/j.jcrysgro.2003.10.001
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
Hydroxyapatite (HAp) nanopowder was synthesized using a modified chemical precipitation route. Dried HAp gel powder was almost in amorphous state with very low crystallinity as prepared, showing fine a particle size of similar to 50-100 nm. Due to the enhanced surface area HAp nanopowder showed high sintered density at 1000degreesC. The Ca/P ratio in powder preparation was varied and the amount of each HAp and beta-TCP phase was analyzed using a quantitative X-ray diffraction. The powder with a Ca/P ratio of 1.70 showed the formation of the lowest beta-TCP content, while that of 1.75 showed the formation of a CaO phase as well as beta-TCP. By using a modified chemical route and varying chemical compositions sintering and beta-TCP phase formation behavior of HAp powder could be successfully controlled for artificial hard tissue applications. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:467 / 472
页数:6
相关论文
共 21 条