Sulfuration corrosion failure analysis of Inconel 600 alloy heater sleeve in high-temperature flue gas

被引:12
|
作者
Wei, Chen [1 ]
Wang, Zejun [1 ]
Chen, Jianguo [1 ,2 ]
机构
[1] Tianjin Special Equipment Inspect Inst, Tianjin 300192, Peoples R China
[2] China Elect Technol Grp Corp, Res Inst 18, Tianjin 300384, Peoples R China
关键词
Inconel; 600; alloy; Sulfuration corrosion; High-temperature flue gas; Microstructure; 650; DEGREES-C; FIRESIDE CORROSION; BEHAVIOR; SUPERALLOY;
D O I
10.1016/j.engfailanal.2022.106111
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The sulfuration corrosion behavior of Inconel 600 alloy in high-temperature flue gas was investigated. The element distribution around corrosion layer, corrosion morphology and the phase composition of the corrosion layer were analyzed by scanning electron microscope (SEM) and X-ray diffractometer (XRD), respectively. The results indicate that the alloy is susceptible to be corroded in high-temperature sulfur-containing atmosphere. The corrosion mechanism is that, on the one hand, sulfur (S) could penetrate the Cr2O3 oxide layer, diffuse into the matrix along the grain boundary, combine with chromium (Cr) to form Cr sulfide and weaken the intergranular bonding strength. On the other hand, sulfur (S) in the flue gas and nickel (Ni) in the alloy matrix form Ni3S2 with low melting point, which is continuously generated and melted during service, and eventually results in the constant occurrence of sulfuration corrosion.
引用
收藏
页数:7
相关论文
共 50 条
  • [41] Evaluating the efficiency of grain boundary serrations in attenuating high-temperature hot corrosion degradation in Alloy 617
    Bhuyan, P.
    Pradhan, S. K.
    Mitra, R.
    Mandel, S.
    CORROSION SCIENCE, 2019, 149 : 164 - 177
  • [42] A correlation between anodic film properties and stress corrosion cracking Behavior of alloy 600 and alloy 690 in high-temperature caustic solutions
    Hur, DH
    CORROSION, 2003, 59 (03) : 203 - 206
  • [43] Effect of post-deposition heat treatments on high-temperature wear and corrosion behavior of Inconel 625
    Kocaman, Engin
    Gurol, Ugur
    Gunen, Ali
    Cam, Gurel
    MATERIALS TODAY COMMUNICATIONS, 2025, 42
  • [44] Surface mechanical rolling treatment-introduced gradient nanostructured Inconel 625 alloy with enhanced high-temperature wear resistance
    Wang, Yanjiang
    Jia, Zhi
    Ji, Jinjin
    Cheng, Qianqian
    Chan, Luenchow
    Lu, Xianzheng
    Lai, Chiping
    Liu, Dexue
    TRIBOLOGY INTERNATIONAL, 2025, 201
  • [45] Research on Microstructure Stability of Ti600 High-Temperature Titanium Alloy at 600 °C
    Xin Shewei
    Hong Quan
    Lu Yafeng
    Guo Ping
    Qi Yunlian
    Zeng Liying
    RARE METAL MATERIALS AND ENGINEERING, 2010, 39 (11) : 1918 - 1922
  • [46] Research on Surface Stability of Ti600 High-Temperature Titanium Alloy at 600 °C
    Xin Shewei
    Hong Quan
    Lu Yafeng
    Xi Zhengping
    Guo Ping
    Qi Yunlian
    Zeng Liying
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 (08) : 1422 - 1425
  • [47] High-Temperature Creep and Microstructure Evolution of Alloy 800H Weldments with Inconel 625 and Haynes 230 Filler Materials
    Li, Wenjing
    Xiao, Lin
    Walters, Lori
    Dong, Qingshan
    Ienzi, Maurizio
    Sloan, Robyn
    APPLIED SCIENCES-BASEL, 2024, 14 (04):
  • [48] Attainment of favorable microstructure for residual stress reduction through high-temperature heat treatment on additive manufactured inconel 718 alloy
    Kumar, Vijayakumar Praveen
    Jebaraj, Alfred Vinoth
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2022, 121 (7-8) : 4455 - 4472
  • [49] Crevice corrosion behavior of Alloy 690 in high-temperature water
    Ning, Fangqiang
    Wu, Xinqiang
    Tan, Jibo
    JOURNAL OF NUCLEAR MATERIALS, 2019, 515 : 326 - 337
  • [50] Intergranular stress corrosion cracking initiation and growth in mill-annealed alloy 600 tubing in high-temperature caustic
    Brisson, BW
    Ballinger, RG
    McIlree, AR
    CORROSION, 1998, 54 (07) : 504 - 514