Microstructure Evolution Mechanism of Ultra-Thin Dual Phase Magnesium-Lithium Alloy during Asymmetric Warm Rolling

被引:6
作者
An, Shuang [1 ]
Shang, Deli [2 ]
Chen, Ming [1 ]
Ma, Cong [1 ]
Lu, Yanqing [3 ]
Hu, Xiaodong [3 ]
机构
[1] Univ Sci & Technol Liaoning, Sch Mech Engn & Automat, Anshan 114000, Peoples R China
[2] State Key Lab Met Mat Marine Equipment & Applicat, Anshan 114000, Peoples R China
[3] Univ Sci & Technol Liaoning, Sch Met & Mat, Anshan 114000, Peoples R China
关键词
dual phase LZ91 Mg-Li alloy; asymmetric warm rolling; FEM; VPSC; EBSD; texture evolution; TEXTURE EVOLUTION; MG; COLD; BEHAVIOR; DEFORMATION; PLASTICITY; ANISOTROPY; STRESS; MODEL;
D O I
10.3390/ma15145026
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Magnesium-lithium alloy is the lightest metal alloy material so far, and the ultra-thin plate is also one of the main trends in the future development of Mg-Li alloy. In order to explore how to prepare LZ91 ultra-thin Mg-Li alloy, this topic adopts the combination of the finite element method (FEM) and visco-plastic self-consistent (VPSC) calculation, electron back-scattered diffraction (EBSD) and tensile experiment, and uses the asymmetric warm rolling process to realize the processing of ultra-thin LZ91 Mg-Li alloy plate with a thickness of 0.25 mm. The experimental results show that the maximum basal texture strengths of 1 mm initial plate and 0.25 mm ultra-thin rolled plate are 36.02 mud and 29.19 mud, respectively. The asymmetric warm rolling process not only reduces the basal texture strength but also significantly refines the grains. The tensile strength and yield strength of 0.25 mm ultra-thin rolled plate along the rolling direction reached 206.8 MPa and 138.4 MPa, respectively. This has a positive effect on the mechanical properties of subsequent materials. VPSC results show that the base slip is the main factor in Mg-Li alloy asymmetric warm rolling, and a large number of tensile twinning are initiated due to the coordinated deformation of the body-centered cubic (BCC) phase, which is beneficial to improve the plastic deformation capacity of Mg-Li alloy.
引用
收藏
页数:15
相关论文
共 39 条
[1]   A Taylor model based description of the proof stress of magnesium AZ31 during hot working [J].
Barnett, MR .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2003, 34A (09) :1799-1806
[2]   Incipient plasticity and deformation mechanisms in single-crystal Mg during spherical nanoindentation [J].
Catoor, D. ;
Gao, Y. F. ;
Geng, J. ;
Prasad, M. J. N. V. ;
Herbert, E. G. ;
Kumar, K. S. ;
Pharr, G. M. ;
George, E. P. .
ACTA MATERIALIA, 2013, 61 (08) :2953-2965
[3]   Modeling strain rate sensitivity and high temperature deformation of Mg-3Al-1Zn alloy [J].
Chapuis, Adrien ;
Liu, Qing .
JOURNAL OF MAGNESIUM AND ALLOYS, 2019, 7 (03) :433-443
[4]   Effects of cold and warm cross-rolling on microstructure and texture evolution of AZ31B magnesium alloy sheet [J].
Choquechambi Catorceno, Litzy Lina ;
Gomes de Abreu, Hamilton Ferreira ;
Padilha, Angelo Fernando .
JOURNAL OF MAGNESIUM AND ALLOYS, 2018, 6 (02) :121-133
[5]   Thermodynamic studies and the phase diagram of the Li-Mg system [J].
Gasior, W ;
Moser, Z ;
Zakulski, W ;
Schwitzgebel, G .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (09) :2419-2428
[6]   Slip behavior and its effect on rolling texture development in a dual-phase Mg-Li alloy [J].
Guo, Fei ;
Liu, Lei ;
Ma, Yanlong ;
Jiang, Luyao ;
Zhang, Yuhe ;
Zhang, Dingfei ;
Pan, Fusheng .
JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 813
[7]  
He J.J, 2018, THESIS CHONGQING U C
[8]   Statistical optimization of stress level in Mg-Li-Al alloys upon hot compression testing [J].
Islam, Rezawana ;
Haghshenas, Meysam .
JOURNAL OF MAGNESIUM AND ALLOYS, 2019, 7 (02) :203-217
[9]   Implementation of VPSC polycrystal model into rigid plastic finite element method and its application to Erichsen test of Mg alloy [J].
Kang, Gyeong Pil ;
Lee, Kyounghoon ;
Kim, Yong Hwan ;
Park, Sang Jun ;
Shin, Kwang Seon .
METALS AND MATERIALS INTERNATIONAL, 2017, 23 (05) :930-939
[10]   Microstructure and texture evolution during hot rolling of Mg-9Li-7Al-1Sn alloy for aerospace application [J].
Kumar, Vinod ;
Balasubramaniam, R. ;
Shekhar, Rajiv ;
Balani, Kantesh .
TEXTURES OF MATERIALS, PTS 1 AND 2, 2012, 702-703 :85-88